| 搅拌摩擦加工超细晶及纳米结构Cu-Al合金的微观组织和力学性能研究* |
薛鹏, 肖伯律, 马宗义( ) |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR PROCESSED ULTRAFINE-GRAINED AND NANOSTRUCTURED Cu-Al ALLOYS |
XUE Peng, XIAO Bolü, MA Zongyi( ) |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
薛鹏, 肖伯律, 马宗义. 搅拌摩擦加工超细晶及纳米结构Cu-Al合金的微观组织和力学性能研究*[J]. 金属学报, 2014, 50(2): 245-251.
Peng XUE,
Bolü XIAO,
Zongyi MA.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF FRICTION STIR PROCESSED ULTRAFINE-GRAINED AND NANOSTRUCTURED Cu-Al ALLOYS[J]. Acta Metall Sin, 2014, 50(2): 245-251.
| [1] |
Valiev R. Nat Mater, 2004; 3: 511
|
| [2] |
Zhu Y T, Liao X Z. Nat Mater, 2004; 3: 351
|
| [3] |
Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771
|
| [4] |
Mughrabi H, Höppel H W. Int J Fatigue, 2010; 32: 1413
|
| [5] |
Goto M, Han S Z, Euh K, Kang J H, Kim S S. Acta Mater, 2010; 58: 6249
|
| [6] |
An X H. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, 2012
|
| [6] |
(安祥海. 中国科学院金属研究所博士学位论文, 沈阳, 2012)
|
| [7] |
Mishra R S, Mahoney M W, McFadden S X, Mara N A, Mukherjee A K. Scr Mater, 1999; 42: 163
|
| [8] |
Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
|
| [9] |
Ma Z Y. Metall Mater Trans, 2008; 39A: 642
|
| [10] |
Xue P, Xiao B L, Ma Z Y. Mater Sci Eng, 2012; A532: 106
|
| [11] |
Su J Q, Nelson T W, Sterling C J. Scr Mater, 2005; 52: 135
|
| [12] |
Xue P, Xiao B L, Ma Z Y. Scr Mater, 2013; 68: 751
|
| [13] |
Chang C I, Du X H, Huang J C. Scr Mater, 2007; 57: 209
|
| [14] |
Xue P, Xiao B L, Wang W G, Zhang Q, Wang D, Wang Q Z, Ma Z Y. Mater Sci Eng, 2013; A575: 30
|
| [15] |
Xue P, Xiao B L, Ma Z Y. J Mater Sci Technol, 2013; 29: 1111
|
| [16] |
An X H, Lin Q Y, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2011; 64: 954
|
| [17] |
Qu S, An X H, Yang H J, Huang C X, Yang G, Zang Q S, Wang Z G, Wu S D, Zhang Z F. Acta Mater, 2009; 57: 1586
|
| [18] |
Zhang P, An X H, Zhang Z J, Wu S D, Li S X, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 67: 871
|
| [19] |
Murr L E. Interfacial Phenomena in Metals and Alloys. Massachusetts: Addison-Wesley Publishing Company, 1975: 142
|
| [20] |
Zhang Y, Tao N R, Lu K. Acta Mater, 2011; 59: 6048
|
| [21] |
Torre F D, Lapovok R, Sandlin J, Thomson P F, Davies C H J, Pereloma E V. Acta Mater, 2004; 52: 4819
|
| [22] |
Meyers M A,Chawla K K. Mechanical Behavior of Materials. 2nd Ed., Cambridge: Cambridge University Press, 2009: 337
|
| [23] |
McNelley T R, Swaminathan S, Su J Q. Scr Mater, 2008; 58: 349
|
| [24] |
Jata K V, Semiatin S L. Scr Mater, 2000; 43: 743
|
| [25] |
Su J Q, Nelson T W, Sterling C J. J Mater Res, 2003; 18: 1757
|
| [26] |
Feng A H, Ma Z Y. Acta Mater, 2009; 57: 4248
|
| [27] |
An X H, Wu S D, Zhang Z F, Figueiredo R B, Gao N, Langdon T G. Scr Mater, 2012; 66: 227
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|