| 敏化温度对SAF2304双相不锈钢耐局部腐蚀性能的影响 |
| 郭丽芳1,李旭晏1,孙涛1,徐菊良1,李劲1,2,蒋益明1 |
1. 复旦大学材料科学系, 上海 200433
2. 中国科学金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 |
|
| THE INFLUENCE OF SENSITIVE TEMPERATURE ON THE LOCALIZED CORROSION RESISTANCE OF DUPLEX STAINLESS STEEL SAF2304 |
| GUO Lifang 1, LI Xuyan 1, SUN Tao 1, XU Juliang 1, LI Jin 1,2, JIANG Yiming 1 |
1. Department of Materials Science, Fudan University, Shanghai 200433
2. State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
郭丽芳 李旭晏 孙涛 徐菊良 李劲 蒋益明. 敏化温度对SAF2304双相不锈钢耐局部腐蚀性能的影响[J]. 金属学报, 2012, 48(12): 1503-1509.
GUO Lifang LI Xuyan SUN Tao XU Juliang LI Jin JIANG Yiming.
THE INFLUENCE OF SENSITIVE TEMPERATURE ON THE LOCALIZED CORROSION RESISTANCE OF DUPLEX STAINLESS STEEL SAF2304[J]. Acta Metall Sin, 2012, 48(12): 1503-1509.
| [1] Solomon H D, Devine T M. In: Lula R A ed., Proc Conf on Duplex Stainless Steels, Metals Park, Ohio: American Society for Metals, 1983: 693[2] Olsson J O, Groth H L. Desalination, 1994; 97: 67[3] Olsson J, Snis M. Desalination, 2007; 205: 104[4] Zhang Z Y, Han D, Jiang Y M, Shi C, Li J. Nucl Eng Des, 2012; 243: 56[5] Straffelini G, Baldo S, Calliari I. Metall Mater Trans, 2009; 40A: 2616[6] Garzon C M, Ramirez A J. Acta Mater, 2006; 54: 3321[7] Kobayashi D Y, Wolynec S. Mater Res, 1999; 2: 239[8] Duprez L, De Cooman B, Akdut N. Steel Res, 2000; 71: 417[9] Chen T H, Weng K L, Yang J R. Mater Sci Eng, 2002; A338: 259[10] Wilms M E, Gadgil V J, Krougman J M, Ijsseling F P. Corros Sci, 1994; 36: 871[11] Lopez N, Cid M, Puiggali M. Corros Sci, 1999; 41: 1615[12] Nilsson J O. Mater Sci Technol, 1992; 8: 685[13] King A, Johnson G, Engelberg D. Science, 2008; 321: 382[14] Bohni H. Langmuir, 1987; 3: 924[15] Bastos I N, Tavares S S, Dalard F, Nogueira R P. Scr Mater, 2007; 57: 913[16] Buhler H E, Gerlach L, Greven O, Bleck W. Corros Sci, 2003; 45: 2325[17] Lopez N, Cid M, Puiggali M, Azkarate I, Pelayo A. Mater Sci Eng, 1997; A229: 123[18] Jin W S, Lang Y P, Rong F, Sun L J. J Chin Soc Corros Prot, 2007; 27: 54(金维松, 郎宇平, 荣凡, 孙力军. 中国腐蚀与防护学报, 2007; 27: 54)[19] Deng B, Jiang Y M, Gong J, Zhong C, Gao J, Li J. Electrochim Acta, 2008; 53: 5220[20] Ovarfort R. Corros Sci, 1989; 29: 987[21] Brigham R J, Tozer E W. Corrosion, 1973; 29: 33[22] Moayed M H, Newman R C. Corros Sci, 2006; 48: 1004[23] Garfias–Mesias L F, Sykes J M. Corros Sci, 1999; 41: 959[24] Li S S. Corros Sci Technol Prot, 2000; 12: 288(李神速. 腐蚀科学与防护技术, 2000; 12: 288)[25] Schwind M, Kallqvist J, Nilsson J O. Acta Mater, 2000; 48: 2473[26] Fargas G, Anglada M, Mateo A. J Mater Process Technol, 2009; 209: 1770[27] Gao J, Jiang Y, Deng B, Ge Z, Li J. Electrochim Acta, 2010; 55: 4837[28] Ebrahimi N, Momeni M, Moayed M H, Davoodi A. Corros Sci, 2011; 53: 637[29] Deng B, Jiang Y, Xu J, Sun T, Gao J, Zhang L, Zhang W, Li J. Corros Sci, 2010; 52: 969 |
|