| 基于团簇模型的高强度马氏体沉淀硬化不锈钢成分设计 |
| 王清1,2,查钱锋1,2,刘恩雪1,2,董闯1,2,王学军3,谭朝鑫3,冀春俊4 |
1. 大连理工大学三束材料改性教育部重点实验室, 大连 116024
2. 大连理工大学材料科学与工程学院, 大连 116024
3. 沈阳鼓风机集团股份有限公司, 沈阳 110869
4. 大连理工大学能源与动力学院, 大连 116024 |
|
| COMPOSITION DESIGN OF HIGH–STRENGTH MARTENSITIC PRECIPITATION HARDENING STAINLESS STEELS BASED ON A CLUSTER MODEL |
| WANG Qing 1,2, ZHA Qianfeng 1,2, LIU Enxue 1,2, DONG Chuang 1,2, WANG Xuejun 3,TAN Chaoxin 3, JI Chunjun 4 |
1. Key Laboratory of Materials Modification of Ministry of Education, Dalian University of Technology, Dalian 116024
2. School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024
3. Shenyang Blower Works Group Corporation, Shenyang 110869
4. School of Energy and Power Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
王清 查钱锋 刘恩雪 董闯 王学军 谭朝鑫 冀春俊. 基于团簇模型的高强度马氏体沉淀硬化不锈钢成分设计[J]. 金属学报, 2012, 48(10): 1201-1206.
WANG Qing ZHA Qianfeng LIU Enxue DONG Chuang Xuejun TAN Chaoxin JI Chunjun.
COMPOSITION DESIGN OF HIGH–STRENGTH MARTENSITIC PRECIPITATION HARDENING STAINLESS STEELS BASED ON A CLUSTER MODEL[J]. Acta Metall Sin, 2012, 48(10): 1201-1206.
| [1] Zhao X C, Song W S, Yang Z Y, Liang J X, Li W H. High Strength and Super–high Strength Stainless Steels. Beijing: Metallurgical Industry Press, 2008: 244(赵先存, 宋为顺, 杨志勇, 梁剑雄, 李文辉. 高强度超高强度不锈钢. 北京: 冶金工业出版社, 2008: 244)[2] Floreen S. Met Rev, 1968; 13: 115[3] Decker R F, Floreen S. Proc Conf on Maraging Steels–Recent Developments and Applications, Warrendale, PA:TMS–AIME, 1988: 1[4] Garrison W M. JOM, 1990; 42: 20[5] Zhou Q Q, Zhai Y C. Acta Metall Sin, 2009; 45: 1249(周倩青, 翟玉春. 金属学报, 2009; 45: 1249)[6] Qiao G Y, Xiao F R, Tan C X. Spec Steel, 1998; 19: 18(乔桂英, 肖福仁, 谭朝鑫. 特殊钢, 1998; 19: 18)[7] Hsiao C N, Chiou C S, Yang J R. Mater Chem Phys, 2002;74: 134[8] Wang J, Zou H, Li C, Yeng Y H, Qiu S Y, Shen B L. Nucl Eng Des, 2006; 236: 2531[9] Sen D, Patra A K, Mazumder S, Mittra J, Dey G K, De P K. Mater Sci Eng, 2005; A397: 370[10] Schaeffler A L. Met Prog, 1949; 56: 680[11] Delong W T, Ostrom G, Szumachowski E. Weld J, 1956; 35: s521[12] Olson G B. Science, 1997; 277: 1237[13] Xu W, Rivera–Diaz–del–Castillo P E J, Yan W, Yang K, San Martin S, Kestens L A I, van der Zwaag S. Acta Mater, 2010; 58: 4067[14] Dong C, Wang Q, Qiang J B, Wang Y M, Jiang N, Han G, Li Y H, Wu J, Xia J H. J Phys, 2007; 40D: 273[15] Wang Q, Dong C, Qiang J B, Wang Y M. Mater Sci Eng, 2007; A18: 449[16] Zhang J, Wang Q, Wang Y M, Li C Y, Wen L S, Dong C. J Mater Res, 2010; 25: 328[17] Ma R T, Hao C P, Wang Q, Ren M F, Wang Y M, Dong C. Acta Metall Sin, 2010; 46: 1034(马仁涛, 郝传璞, 王清, 任明法, 王英敏, 董闯. 金属学报, 2010; 46: 1034)[18] Li B Z, Wang Q, Wang Y M, Li C Y, Qiang J B, Ji C J, Dong C. Metall Mater Trans, 2012; 43A: 544[19] Takeuchi A, Inoue A. Mater Trans JIM, 2005; 46: 2817[20] Raynor G V, Rivlin V G. Phase Equilibria in Iron Ternary Alloys. London: Inst Metals, 1988: 316[21] Abdelshehid M, Mahmodieh K, Mori K, Chen L, Stoyanov P, Davlantes D, Foyos J, Ogren J, Clark Jr R, Es–Said O S. Eng Failure Anal, 2007; 14: 626[22] Dong H, Esfandiari M, Li X Y. Surf Coat Technol, 2008; 202: 2969[23] Greer A L. Science, 1995; 267: 1947[24] Shiflet G. Science, 2003; 300: 443[25] Lo K H, Shek C H, Lai J K L. Mater Sci Eng, 2009; R65: 39[26] H¨attestrand M, Nilsson J O, Stiller K, Liu P, Andersson M. Acta Mater, 2004; 52: 1023 |
|