| 相场法模拟两相多孔组织烧结 |
| 刘明治1,张瑞杰1,方伟1,章书周1,曲选辉1,2 |
1. 北京科技大学新材料技术研究院, 北京 100083
2. 北京科技大学新金属材料国家重点实验室, 北京 100083 |
|
| PHASE FIELD SIMULATION OF SINTERING PROCESS IN BIPHASIC POROUS MATERIAL |
| LIU Mingzhi 1, ZHANG Ruijie 1, FANG Wei 1, ZHANG Shuzhou 1, QU Xuanhui 1,2 |
1. Institute of Advanced Materials and Technologies, University of Science and Technology Beijing, Beijing 100083
2. State Key Laboratory for Advanced Metal and Materials, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
刘明治 张瑞杰 方伟 章书周 曲选辉. 相场法模拟两相多孔组织烧结[J]. 金属学报, 2012, 48(10): 1207-1214.
| [1] German R M. Sintering Theory and Practice. New York: Wiley, 1996: 1[2] Coble R L. J Appl Phys, 1961; 32: 787[3] Coble R L. J Appl Phys, 1961; 32: 793[4] Deborah C B, John D G, Seong J P. Mater Trans, 2006; 37: 715[5] Wang Y U. Acta Mater, 2006; 54: 953[6] Chen L Q, Fan D. J Am Ceram Soc, 1996; 79: 1163[7] Jing X N, Zhao J H, He L H. J Mater Sci Eng, 2003; 21: 170(景晓宁, 赵建华, 何陵辉. 材料科学与工程学报, 2003; 21: 170)[8] Krill C E III, Chen L Q. Acta Mater, 2002; 50: 3057[9] Kazaryan A, Patton B R, Dregia S A, Wang Y. Phys Rev, 2001; 50B: 499[10] Kazaryan A, Wang Y, Dregia S A, Patton B R. Acta Mater, 2002; 50: 2491[11] Kazaryan A, Wang Y, Dregia S A, Patton B R. Phys Rev, 2000; 61B: 14275[12] Kazaryan A, Wang Y, Dregia S A, Patton B R. Phys Rev, 2001; 63B: 4102[13] Suwa Y, Saito Y, Onodera H. Scr Mater, 2006; 55: 407[14] Lange F F, Eur J. J Am Ceram Soc, 2008; 28: 1509[15] Fan D, Chen S P, Chen L Q, Voorhees P W. Acta Mater, 2002; 50: 1895[16] Wang Y Z, Banerjee D, Su J C, Khachaturyan A G. Acta Mater, 1998; 46: 2985[17] Tiaden J, Nestler B, Diepers H J, Steinbach I. Physica, 1998; 115D: 73[18] Zhu J Z, Liu Z K, Vaithyanathan V, Chen L Q. Scr Mater, 2002; 46: 401[19] Zhang W, Jin YW, Khachaturyan A G. Acta Mater, 2007; 55: 565[20] Kazaryan A, Wang Y, Patton B R. Scr Metall, 1999; 41: 487[21] Fan D, Chen L Q. Acta Mater, 1997; 45: 611[22] Wang Y Z, Liu Y H. J Am Ceram Soc, 2000; 83: 2219[23] Fan D. PhD Thesis, The Pennsylvania State University, 1996[24] Cahn J W, Hilliard J E. J Chem Phys, 1958; 28: 258[25] Allen S M, Cahn J W. Acta Metall, 1978; 27: 1085[26] Kazushige S K. J Cryst Growth, 2002; 237: 144[27] Kumar V, Fang Z Z, Fife P C. Mater Sci Eng, 2010; A528: 254[28] Cahn J W, Allen S M. Acta Metall, 1962; 10: 789 |
|