| 打底层对铝合金表面GLC镀层组织和摩擦学特性的影响 |
| 时惠英,龙艳妮,蒋百灵,陈迪春 |
| 西安理工大学材料科学与工程学院, 西安 710048 |
|
| EFFECT OF SUBLAYER ON THE STRUCTURES AND TRIBOLOGICAL PROPERTIES OF GLC COATING ON Al–BASED ALLOY |
| SHI Huiying, LONG Yanni, JIANG Bailing, CHEN Dichun |
| School of Materials Science and Engineering, Xi’an University of Technology, Xi’an 710048 |
引用本文:
时惠英 龙艳妮 蒋百灵 陈迪春. 打底层对铝合金表面GLC镀层组织和摩擦学特性的影响[J]. 金属学报, 2012, 48(8): 983-988.
,
,
,
.
EFFECT OF SUBLAYER ON THE STRUCTURES AND TRIBOLOGICAL PROPERTIES OF GLC COATING ON Al–BASED ALLOY[J]. Acta Metall Sin, 2012, 48(8): 983-988.
| [1] Wei T, Yan F, Tian J. J Alloys Compd, 2005; 389: 169[2] Sun X, Jiang Z, Xin S, Yao Z. Thin Solid Films, 2005; 471: 194[3] Akarca S S, Altenhof W J, Alpas A T. Tribol Int, 2007; 40: 735[4] Wu J J. Foundry Technol, 2002; 23: 273(吴浚郊. 铸造技术, 2002; 23: 273)[5] Xue W B, Shi X L, Hua M, Li Y L. Appl Surf Sci, 2007; 253: 6118[6] Donnet C, Erdemir A. Surf Coat Technol, 2004; 180: 76[7] Xu B S, Zhu S H, Liu S S. Materials Surface Engineering. Harbin: Harbin Institute of Technology Press, 2005: 1(徐滨士, 朱绍华, 刘世参. 材料表面工程. 哈尔滨 : 哈尔滨工业大学出版社, 2005: 1)[8] Zhou F, Wang Y, Ding H Y, Wang M L, Yu M, Dai Z D. Surf Coat Technol, 2008; 202: 3808[9] Zhu M H, Cai Z B, Lin X Z, Ren P D, Tan J, Zhou Z R. Wear, 2007; 263: 472[10] Ding H Y, Dai Z D, Skuiry S C, Hui D. Tribol Int, 2010; 43: 868[11] Li H X, Rudnev V S, Zheng X H, Yarovay T P, Song R G. J Alloys Compd, 2008; 462: 99[12] Nie X,Wilson A, Leyland A, Matthews A. Surf Coat Technol, 2000; 121: 506[13] Dobrzanski L A, Polok M, Panjan P, Bugliosi S, Adamiak M. J Mater Process Technol, 2004; 155–156: 1995[14] Baragetti S, Gerosa R, Rivolta B, Silva G, Tordini F. Procedia Eng, 2011; 10: 3375[15] Dobrza’nski L A, Polok M, Adamiak M. J Mater Process Technol, 2005; 164–165: 843[16] Hua M, Ma H Y, Li J, Mok C K. Surf Coat Technol, 2006; 200: 3612[17] Xia C B, Wang D J. Surface Engineering of Aviation Maintenance. Xinyang: Air Force flight School Press, 1997: 206(夏成宝, 汪定江. 航空维修表面工程. 信阳: 空军一航院出版社, 1997: 206)[18] Wang Y X, Wang L P, Xue Q J. Appl Surf Sci, 2011; 257: 10246[19] Wang Y X, Wang L P, Wang S C, Zhang G A, Wood R J K, Xue Q J. Tribol Lett, 2010; 40: 301[20] Teer D G. Wear, 2001; 251: 1068[21] Renevier N M, Hamphire J, Fox V C, Allen T, Teer D G. Surf Coat Technol, 2001; 142: 67[22] Zhao L, Fu Y H, Liu D Y, Zhu X D, He J W. Chin J Inorg Mater, 2005; 20: 181(赵蕾, 付永辉, 刘登益, 朱晓东, 何家文. 无机材料学报, 2005; 20: 181)[23] Chen D C, Jiang B L, Shi H Y, Long Y N. Vacuum, 2012; 86: 1576[24] Shi H Y, Zhang B, Jiang B L, Zhang Y H, Chen Z S. Trans Mater Heat Treat, 2009; 30: 136[25] Ichimur H, Ishii Y. Surf Coat Technol, 2003; 165: 1 |
|