| 高能球磨法制备的碳纳米管增强铝基复合材料的微观组织和力学性能 |
| 许世娇, 肖伯律, 刘振宇, 王文广, 马宗义 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| MICROSTRUCTURES AND MECHANICAL PROPERTIES OF CNT/Al COMPOSITES FABRICATED BY HIGH ENERGY BALL-MILLING METHOD |
| XU Shijiao, XIAO Bolu, LIU Zhenyu, WANG Wenguang, MA Zongyi |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
许世娇 肖伯律 刘振宇 王文广 马宗义. 高能球磨法制备的碳纳米管增强铝基复合材料的微观组织和力学性能[J]. 金属学报, 2012, 48(7): 882-888.
,
,
,
,
.
MICROSTRUCTURES AND MECHANICAL PROPERTIES OF CNT/Al COMPOSITES FABRICATED BY HIGH ENERGY BALL-MILLING METHOD[J]. Acta Metall Sin, 2012, 48(7): 882-888.
| [1] Pan F S, Zhang D F. Aluminum Alloy and Its Application. Beijing: Chemical Industry Press, 2006: 414(潘复生, 张丁非. 铝合金及应用. 北京: 化学工业出版社, 2006: 414)[2] Iijima S. Nature, 1991; 354: 56[3] Wong E W, Sheehan P E, Lieber C M. Science, 1997; 277: 1971[4] Treacy M M J, Ebbesen T W, Gibson J M. Nature, 1996; 381: 678[5] Baughman R H, Zakhidov A A, de Heer W A. Science, 2002; 297: 787[6] Breuer O, Sundararaj U. Polym Compos, 2004; 25: 630[7] Zhong R, Cong H T, Hou P. Carbon, 2003; 41: 848[8] Jiang L, Fan G L, Li Z Q, Kai X Z, Zhang D, Chen Z X, Humphries S, Heness G, Yeung W Y. Carbon, 2011; 49: 1965[9] Esawi A, Morsi K. Composites, 2007; 38A: 646[10] Esawi A, Morsi K, Sayed A, Tacher M, Lanka S. Compos Sci Technol, 2010; 70: 2237[11] Kim K T, Eckert J, Menzel S B, Gemming T, Hong S H. Appl Phys Lett, 2008; 92: 121901[12] Choi H J, Shin J Y, Min B H, Park J, Bae D H. J Mater Res, 2009; 24: 2610[13] Liu Z Y, Wang Q Z, Xiao B L, Ma Z Y, Liu Y. Mater Sci Eng, 2010; A527: 5582[14] Casiraghi C, Ferrari A C, Robertson J. Phys Rev, 2005; 72B: 085401[15] McGuire K, Gothard N, Gai P L, Dresselhaus M S, Sumanasekera G, Rao A M. Carbon, 2005; 43: 219[16] Delhaes P, Couzi M, Trinqucoste M, Dentzer J, Hamidou H, Vix–Guterl C. Carbon, 2006; 44: 964[17] Dominique P, Raynald G, Robin A L D. Composites, 2009; 40A: 1482[18] Ci L J, Ryu Z Y, Jin–Phillipp N Y, Ruhle M. Acta Mater, 2006; 54: 5367[19] Esawi A M K, Morsi K, Sayed A, Taher M, Lanka S. Composites, 2011; 42A: 234[20] Deng C F, Zhang X X, Wang D Z. Mater Lett, 2007; 61: 904[21] George R, Kashyap K T, Rahul R, Yamdagni S. Scr Mater, 2005; 53: 1159[22] Kaneko S, Murakami K, Sakai T. Mater Sci Eng, 2009; A500: 8[23] Liu Z Y, Xiao B L, Wang W G, Ma Z Y. Carbon, 2012; 50: 1843[24] Wilcox B A, Clauer A H. Acta Metall, 1972; 20: 743[25] Choi H J, Kwon G B, Lee G Y, Bae D H. Scr Mater, 2008; 59: 360 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|