| 室温等径转角挤压对18Ni(C-250)马氏体时效钢微观组织和拉伸性能的影响 |
| 杨沐鑫1,2,杨钢2,刘正东2,王昌2,胡超2,黄崇湘3 |
1. 昆明理工大学材料科学与工程学院, 昆明 650093
2. 钢铁研究总院结构材料研究所, 北京 100081
3. 四川大学建筑与环境学院, 成都 610065 |
|
| EFFECT OF EQUAL–CHANNEL ANGULAR PRESSING ON THE MICROSTRUCTURES AND TENSILE PROPERTIES OF 18Ni(C–250) MARAGING STEEL |
| YANG Muxin 1,2, YANG Gang 2, LIU Zhengdong 2, WANG Chang 2, HU Chao 2, HUANG Chongxiang 3 |
1. Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
2. Institute for Structural Materials, Central Iron and Steel Research Institute, Beijing 100081
3. College of Architecture and Environment, Sichuan University, Chengdu 610065 |
引用本文:
杨沐鑫 杨钢 刘正东 王昌 胡超 黄崇湘. 室温等径转角挤压对18Ni(C-250)马氏体时效钢微观组织和拉伸性能的影响[J]. 金属学报, 2012, 48(2): 164-169.
,
,
,
,
,
.
EFFECT OF EQUAL–CHANNEL ANGULAR PRESSING ON THE MICROSTRUCTURES AND TENSILE PROPERTIES OF 18Ni(C–250) MARAGING STEEL[J]. Acta Metall Sin, 2012, 48(2): 164-169.
| [1] ASM Handbook Committee. ASM Handbook. Volume 1, 10th Ed., Ohio: ASM International, 1990: 739[2] Li X D. PhD Thesis, Harbin Institute of Technology, 1993(李晓东. 哈尔滨工业大学博士学位论文, 1993)[3] Sha W, Guo Z. Maraging Steels: Modelling of Microstructure, Properties and Applications. Oxford: Woodhead Publishing, 2009: 3[4] Roberson J A, Adair A M. Trans TMS–AIME, 1969; 245: 1937[5] Baker A J, Swann P R. Trans ASM, 1964; 57: 1008[6] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881[7] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X. Acta Mater, 2006; 54: 655[8] Huang C X, Yang G, Wang C, Zhang Z F, Wu S D. Metall Mater Trans, 2011; 42A: 2061[9] Yang G, Huang C X, Wang C, Zhang L Y, Hu C, Zhang Z F, Wu S D. Mater Sci Eng, 2009; A515: 199[10] Huang C X, Yang G, Gao Y L, Wu S D, Zhang Z F. Mater Sci Eng, 2008; A485: 643[11] He Y, Yang K, Kong F Y, Qu W S, Su G Y. Acta Metall Sin, 2002; 38: 278(何毅, 杨柯, 孔凡亚, 曲文生, 苏国跃. 金属学报, 2002; 38: 278)[12] Yang G, Yin F. Mater Sci Forum, 2010; 667–669: 879[13] Mobarake M I, Nili–Ahmadabadia M, Poorganji B, Fatehi A, Shirazi H, Furuhara T, Parsaa H, Nejad S H. Mater Sci Eng, 2008; A491: 172[14] Yang M X, Yang G, Liu Z D, Wang C, Huang C X. Mater Sci Forum, 2010; 667–669: 421[15] Iwahashi Y, Wang J, Horita Z, Nemoto M, Langdon T G. Scr Mater, 1996; 35: 143[16] Marder J M, Marder A R. Trans ASM, 1969; 62: 1[17] Tsai C K, Chu C, He C Z, Shen H W, Luo L K, Song W S, Yu W L. Acta Metall Sin, 1977; 13: 289(蔡其巩, 朱静, 何崇智, 申辉旺, 罗力更, 宋为顺, 于维乐. 金属学报, 1977; 13: 289)[18] Ye H Q, Zou S B. Acta Metall Sin, 1979; 15: 69(叶恒强, 邹三本. 金属学报, 1979; 15: 69)[19] Tsai C K, Zhu Q, He C Z. Acta Phys Sin, 1974; 23: 178(蔡其巩, 朱静, 何崇智. 物理学报, 1974; 23: 178)[20] Tewari R, Mazumder S, Batra I S, Dey G K, Banerjee S. Acta Mater, 2000; 48: 1187[21] Yin Z D, Li X D, Li H B, Lai Z H. Acta Metall Sin, 1995; 31: 7(尹钟大, 李晓东, 李海滨, 来忠红. 金属学报, 1995; 31: 7)[22] Yong Q L, MaMT. Micro–alloyed Steel—Physics and Mechanics Metallurgy. Beijing: Metallurgy Industry Press, 1989: 315(雍岐龙, 马鸣图. 微合金钢-物理和力学冶金. 北京: 冶金工业出版社, 1989: 315)[23] Martin J W, Doherty R D. Translated by Li X L. Stability of Microstructure in Metallic Systems. Beijing: Science Press, 1984: 55(Martin J W, Doherty R D. 李新立 译. 金属系中显微结构的稳定性. 北京: 科学出版社, 1984: 55)[24] He Y, Liu K, Yang K. Acta Metall Sin, 2003; 39: 381(何毅, 刘 凯, 杨柯. 金属学报, 2003; 39: 381) |
|