Please wait a minute...
金属学报  2012, Vol. 48 Issue (2): 164-169    DOI: 10.3724/SP.J.1037.2011.00420
  论文 本期目录 | 过刊浏览 |
室温等径转角挤压对18Ni(C-250)马氏体时效钢微观组织和拉伸性能的影响
杨沐鑫1,2,杨钢2,刘正东2,王昌2,胡超2,黄崇湘3
1. 昆明理工大学材料科学与工程学院, 昆明 650093
2. 钢铁研究总院结构材料研究所, 北京 100081
3. 四川大学建筑与环境学院, 成都 610065
EFFECT OF EQUAL–CHANNEL ANGULAR PRESSING ON THE MICROSTRUCTURES AND TENSILE PROPERTIES OF 18Ni(C–250) MARAGING STEEL
YANG Muxin 1,2, YANG Gang 2, LIU Zhengdong 2, WANG Chang 2, HU Chao 2, HUANG Chongxiang 3
1. Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
2. Institute for Structural Materials, Central Iron and Steel Research Institute, Beijing 100081
3. College of Architecture and Environment, Sichuan University, Chengdu 610065
引用本文:

杨沐鑫 杨钢 刘正东 王昌 胡超 黄崇湘. 室温等径转角挤压对18Ni(C-250)马氏体时效钢微观组织和拉伸性能的影响[J]. 金属学报, 2012, 48(2): 164-169.
, , , , , . EFFECT OF EQUAL–CHANNEL ANGULAR PRESSING ON THE MICROSTRUCTURES AND TENSILE PROPERTIES OF 18Ni(C–250) MARAGING STEEL[J]. Acta Metall Sin, 2012, 48(2): 164-169.

全文: PDF(1043 KB)  
摘要: 采用等径转角挤压(ECAP)工艺在室温下对18Ni (C-250)马氏体时效钢进行单道次冷变形.对比固溶处理试样480 ℃时效曲线、固溶+ECAP处理试样的460和480 ℃时效曲线发现,一道次ECAP变形及随后的时效处理能够使马氏体时效钢的峰值时效时间明显缩短,峰值强度提高约100 MPa. 结构分析表明, ECAP态实验钢的马氏体板条宽度为100-200 nm, 随后的时效过程对马氏体板条宽度影响不大, 而ECAP工艺对棒状δ-Ni3Mo相析出尺寸有显著影响. 统计结果表明, 经4 h时效处理后, 固溶+480 ℃时效态、固溶+ECAP+480 ℃, 460 ℃时效态的δ-Ni3Mo宽度(直径)分别为4.92,12.33和3.54 nm. 此外, ECAP工艺还促使18Ni马氏体钢中δ-Ni3Mo相在时效后期加速分解, 使强度迅速衰减.
关键词 : 马氏体时效钢,  等径转角挤压(ECAP),  力学性能,  时效强化    
Abstract:An 18Ni (C–250) maraging steel was successfully processed by equal–channel angular pressing (ECAP) for a single pass at room temperature. After ECAP deformation, the peak aging time was cut obviously and the peak strength of the steel was enhanced about 100 MPa. Microstructural observations showed that the martensite laths of 18Ni maraging steel were elongated to more narrow bands with a width of 100—200 nm after ECAP deformation, and the width of martensite lath was not affected by the subsequent aging treatment. ECAP deformation has significant influence on the size of rod–shaped δ–Ni3Mo precipitates. It was observed that the widths (diameters) of precipitates in specimens under treatments of solution+480℃, 4 h, solution+ECAP+480℃, 4 h and solution+ECAP+460 ℃, 4 h are 4.92, 12.33 and 3.54 nm, respectively. Additionally, a decomposition of the δ–Ni3Mo precipitates was accelerated after the peak aging time, resulting in a decrease in the strength.
Key words: maraging steel    equal–channel angular pressing (ECAP)    mechanical property    aging hardening
收稿日期: 2011-07-07     
ZTFLH: 

TG142.1

 
基金资助:

国家自然科学基金资助项目 50971045

作者简介: 杨沐鑫, 男, 1982年生, 博士生
[1] ASM Handbook Committee. ASM Handbook. Volume 1, 10th Ed., Ohio: ASM International, 1990: 739

[2] Li X D. PhD Thesis, Harbin Institute of Technology, 1993

(李晓东. 哈尔滨工业大学博士学位论文, 1993)

[3] Sha W, Guo Z. Maraging Steels: Modelling of Microstructure, Properties and Applications. Oxford: Woodhead Publishing, 2009: 3

[4] Roberson J A, Adair A M. Trans TMS–AIME, 1969; 245: 1937

[5] Baker A J, Swann P R. Trans ASM, 1964; 57: 1008

[6] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881

[7] Huang C X, Wang K, Wu S D, Zhang Z F, Li G Y, Li S X. Acta Mater, 2006; 54: 655

[8] Huang C X, Yang G, Wang C, Zhang Z F, Wu S D. Metall Mater Trans, 2011; 42A: 2061

[9] Yang G, Huang C X, Wang C, Zhang L Y, Hu C, Zhang Z F, Wu S D. Mater Sci Eng, 2009; A515: 199

[10] Huang C X, Yang G, Gao Y L, Wu S D, Zhang Z F. Mater Sci Eng, 2008; A485: 643

[11] He Y, Yang K, Kong F Y, Qu W S, Su G Y. Acta Metall Sin, 2002; 38: 278

(何毅, 杨柯, 孔凡亚, 曲文生, 苏国跃. 金属学报, 2002; 38: 278)

[12] Yang G, Yin F. Mater Sci Forum, 2010; 667–669: 879

[13] Mobarake M I, Nili–Ahmadabadia M, Poorganji B, Fatehi A, Shirazi H, Furuhara T, Parsaa H, Nejad S H. Mater Sci Eng, 2008; A491: 172

[14] Yang M X, Yang G, Liu Z D, Wang C, Huang C X. Mater Sci Forum, 2010; 667–669: 421

[15] Iwahashi Y, Wang J, Horita Z, Nemoto M, Langdon T G. Scr Mater, 1996; 35: 143

[16] Marder J M, Marder A R. Trans ASM, 1969; 62: 1

[17] Tsai C K, Chu C, He C Z, Shen H W, Luo L K, Song W S, Yu W L. Acta Metall Sin, 1977; 13: 289

(蔡其巩, 朱静, 何崇智, 申辉旺, 罗力更, 宋为顺, 于维乐. 金属学报, 1977; 13: 289)

[18] Ye H Q, Zou S B. Acta Metall Sin, 1979; 15: 69

(叶恒强, 邹三本. 金属学报, 1979; 15: 69)

[19] Tsai C K, Zhu Q, He C Z. Acta Phys Sin, 1974; 23: 178

(蔡其巩, 朱静, 何崇智. 物理学报, 1974; 23: 178)

[20] Tewari R, Mazumder S, Batra I S, Dey G K, Banerjee S. Acta Mater, 2000; 48: 1187

[21] Yin Z D, Li X D, Li H B, Lai Z H. Acta Metall Sin, 1995; 31: 7

(尹钟大, 李晓东, 李海滨, 来忠红. 金属学报, 1995; 31: 7)

[22] Yong Q L, MaMT. Micro–alloyed Steel—Physics and Mechanics Metallurgy. Beijing: Metallurgy Industry Press, 1989: 315

(雍岐龙, 马鸣图. 微合金钢-物理和力学冶金. 北京: 冶金工业出版社, 1989: 315)

[23] Martin J W, Doherty R D. Translated by Li X L. Stability of Microstructure in Metallic Systems. Beijing: Science Press, 1984: 55

(Martin J W, Doherty R D. 李新立 译. 金属系中显微结构的稳定性. 北京: 科学出版社, 1984: 55)

[24] He Y, Liu K, Yang K. Acta Metall Sin, 2003; 39: 381

(何毅, 刘 凯, 杨柯. 金属学报, 2003; 39: 381)
[1] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[6] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[9] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[10] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[11] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[12] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[13] 李述军, 侯文韬, 郝玉琳, 杨锐. 3D打印医用钛合金多孔材料力学性能研究进展[J]. 金属学报, 2023, 59(4): 478-488.
[14] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.
[15] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.