| 纳米SiC颗粒增强NiTi形状记忆复合材料制备及其力学性能和阻尼行为 |
| 江鸿杰, 柯常波, 曹姗姗, 马骁, 张新平 |
| 华南理工大学材料科学与工程学院, 广州 510640 |
|
| PREPARATION OF NANO-SIZED SiC REINFORCED NiTi SHAPE MEMORY COMPOSITES AND THEIR MECHANICAL PROPERTIES AND DAMPING BEHAVIOR |
| JIANG Hongjie, KE Changbo, CAO Shanshan, MA Xiao, ZHANG Xinping |
| School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640 |
引用本文:
江鸿杰 柯常波 曹姗姗 马骁 张新平. 纳米SiC颗粒增强NiTi形状记忆复合材料制备及其力学性能和阻尼行为[J]. 金属学报, 2011, 47(9): 1105-1111.
,
,
,
,
.
PREPARATION OF NANO-SIZED SiC REINFORCED NiTi SHAPE MEMORY COMPOSITES AND THEIR MECHANICAL PROPERTIES AND DAMPING BEHAVIOR[J]. Acta Metall Sin, 2011, 47(9): 1105-1111.
| [1] Miyazaki S, Otsuka K. Trans ISIJ, 1989; 29: 353[2] Graesser E J, Cozzarelli F A. J EngMech, 1991; 117: 2590[3] Aiken I D, Nims K D, Whittaker A S, James M K, Eeri M. Earthq Spectra, 1993; 9: 335[4] Van Humbeeck J. J Alloys Compd, 2003; 355: 58[5] Li D S, Zhang Y P, Xiong Z P, Zhang X P. Acta Metall Sin, 2008; 44: 995(李大圣, 张宇鹏, 熊志鹏, 张新平. 金属学报, 2008; 44: 995)[6] Li B Y, Rong L J. J Mater Res, 1998; 13: 2847[7] Yuan B, Chung C Y, Zhang X P, Zeng M Q, Zhu M. Smart Mater Struct, 2005; 14: S201[8] Zhang Y P, Li D S, Zhang X P. Scr Mater, 2007; 57: 1020[9] Yang Y, Lan J, Li X C. Mater Sci Eng, 2004; A386: 284[10] Li D S, Zhang X P, Xiong Z P, Mai Y W. J Alloys Compd, 2010; 490: 15[11] Maruyama B, Hunt W. JOM, 1999; 11: 59[12] Contreras A, Angeles–Ch´avez C, Flores O, Perez R. Mater Charact, 2007; 58: 685[13] Zhang Y P, Yuan B, Zeng M Q, Chung C Y, Zhang X P. J Mater Process Technol, 2007; 439: 192[14] Kuang Y H, Ngai T, H G, Li Y Y. J Alloys Compd, 2009; 209: 4607[15] Gale W F, Totemeier T C. Smithell Metals Reference Book. Netherlands: Elsevier, 2004: 9[16] Ke C B, Ma X, Zhang X P. Acta Metall Sin, 2011; 47: 129(柯常波, 马骁, 张新平. 金属学报, 2011; 47: 129)[17] Rao G B, Wang J Q, Han E H, Ke W. Acta Metall Sin, 2002; 38: 575(饶光斌, 王俭秋, 韩恩厚, 柯 伟. 金属学报, 2002; 38: 575)[18] Zhang X P, Liu H Y, Yuan B, Zhang Y P. Mater Sci Eng, 2008; A481: 170[19] Li D S. PhD Thesis, South China University of Technology, Guangzhou, 2009(李大圣. 华南理工大学博士论文, 广州, 2009)[20] Zhao J S. The Basis of Dislocation Theory. Beijing: National Defense Industry Press, 1989: 148(赵敬世. 位错理论基础. 北京: 国防工业出版社, 1989: 148)[21] Lin H C, Wu S K, Yeh M T. Metall Mater Trans, 1993; 24A: 2189[22] Nishiyama K, Yamanaka M, Omori M, Umekawa S. Mater Sci Lett, 1990; 9: 526[23] Gao M X, Oliveira F J, Pan Y, Yang L, Baptista J L, Vieira J M. Intermetallics, 2005; 13: 406[24] Wang H M, Wang C M, Cai L X. Surf Coat Technol, 2003; 168; 202[25] Cai W, Lu X L, Zhao L C. Mater Sci Eng, 2005; A394: 78 |
|