| Ta-7.5%W合金箔材冷轧过程中的位错结构演变 |
| 陈畅, 汪明朴, 王珊, 贾延琳, 左波, 夏福中 |
| (中南大学材料科学与工程学院, 长沙 410083) |
|
| EVOLUTION OF DISLOCATION MICROSTRUCTURES IN Ta–7.5%W ALLOY FOILS DURING COLD–ROLLING |
| CHEN Chang, WANG Mingpu, WANG Shan, JIA Yanlin, ZUO Bo, XIA Fuzhong |
| School of Material Science and Engineering, Central South University, Changsha 410083 |
引用本文:
陈畅 汪明朴 王珊 贾延琳 左波 夏福中. Ta-7.5%W合金箔材冷轧过程中的位错结构演变[J]. 金属学报, 2011, 47(8): 984-989.
,
,
,
,
,
.
EVOLUTION OF DISLOCATION MICROSTRUCTURES IN Ta–7.5%W ALLOY FOILS DURING COLD–ROLLING[J]. Acta Metall Sin, 2011, 47(8): 984-989.
| [1] Shen K, Duggan B J. Acta Mater, 2007; 55: 1137[2] Chen Q Z, Quadira M Z, Duggana B J. Philos Mag, 2006;86: 3633[3] Li Z J, Winther G, Hansen N. Acta Mater, 2006; 54: 401[4] Park Y B, Lee D N, Gottstein G. Acta Mater, 1998; 46: 3371[5] Jonas J J. J Mater Process Technol, 2001; 117: 293[6] Hansen N. Mater Sci Technol, 1990; 6: 1039[7] Hutchinson B. Mater Sci Forum, 2007; 558–559: 13[8] Li B L, Godfrey A, Meng Q C, Liu Q, Hansen N. Acta Mater, 2004; 52: 1069[9] Kuhlmann–Wilsdorf D. Acta Mater, 1999; 47: 1697[10] Nasser S N, Kapoo R. Int J Plasticity, 2001; 17: 1351[11] Nemat–Nasser S, Isaacs J B. Acta Mater, 1997; 45: 907[12] Tse Y Y, Duggan B J. Metall Mater Trans, 2006; 37A: 1055[13] Duesbery M S. Acta Metall, 1983, 31: 1747[14] Duesbery M S, Vitek V. Acta Mater, 1998; 46: 1481[15] Hansen N, Huang X, Winther G. Mater Sci Eng, 2008; A494: 61[16] Chang J P, Cai W, Bulatov V V. Comput Mater Sci, 2002; 23: 111[17] Hirth J P, Lothe J. Theory of Dislocations, 2nd Ed. New York: John Wiley & Sons Inc., 1960: 63[18] Kuhlmann–Wilsdorf D. Prog Mater Sci, 2009; 54: 707[19] Chen Q Z, Duggan B J. Metall Mater Trans, 2004; 35A: 3423[20] Quadir M Z, Duggan B J. Acta Mater, 2006; 54: 4337[21] Hull D, Bacon D J. Introduction to Dislocations, 4th Ed.Oxford: A division of Reed Educational and Professional Publishing Ltd., 2001: 14 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|