| La和Hf对CoNiCrAl合金涂层高温氧化行为的影响 |
| 宋鹏1,2,陆建生1,张德丰1,吕建国3,李德江4 |
1. 昆明理工大学材料科学与工程学院, 昆明 650093
2. Forschungszentrum Juelich, IEK-2, Juelich 52425, Germany
3. 昆明理工大学应用技术学院, 昆明 650093
4. 上海交通大学材料科学与工程学院, 上海 200240 |
|
| EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS |
| SONG Peng 1,2, LU Jiansheng 1, ZHANG Defeng 1, L¨U Jianguo 3, LI Dejiang 4 |
1. Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
2. Forschungszentrum Juelich, IEK–2, Juelich 52425, Germany
3. Faculty of Applied Technology, Kunming University of Science and Technology, Kunming 650093
4. School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240 |
引用本文:
宋鹏 陆建生 张德丰 吕建国 李德江. La和Hf对CoNiCrAl合金涂层高温氧化行为的影响[J]. 金属学报, 2011, 47(6): 655-662.
,
,
,
,
.
EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS[J]. Acta Metall Sin, 2011, 47(6): 655-662.
| [1] Padture N P, Gell M, Jordan E H. Science, 2002; 296: 280[2] Clarke D R, Levi C G. Annu Rev Mater Res, 2003; 33: 383[3] Evans A G, Mumm D R, Hutchinson J W, Meier G H, Pettit F S. Prog Mater Sci, 2001; 46: 505[4] Wu R T, Reed R C. Acta Mater, 2008; 56: 313[5] Nijdama T J, Sloof W G. Acta Mater, 2007; 55: 5980[6] Naumenko D, Kochubey V, Niewolak L, Dymiati A, Mayer J, Singheiser L, Quadakkers W J. J Mater Sci, 2008; 43: 4550[7] Haynes J A, Pint B A, More K L, Zhang Y, Wright I G. Oxid Met, 2002; 58: 513[8] Pint B A. J Am Ceram Soc, 2003; 86: 686[9] Hamadi S, Bacos M P, Poulain M, Seyeux A, Maurice V, Marcus P. Surf Coat Technol, 2009; 204: 756[10] Kuenzly J D, Douglass D L. Oxid Met, 1974; 8: 139[11] Pint B A. Oxid Met, 1996; 45: 1[12] Carling K M, Carter E A. Acta Mater, 2007; 55: 2791[13] Evans E. Int Mater Rev, 1995; 40: 1[14] Wessel E, Kochubey V, Naumenko D, Niewolak L, Singheiser L, Quadakkers W J. Scr Mater, 2004; 51: 987[15] Young D J, Naumenko D, Niewolak L,Wessel E, Singheiser L, Quadakkers W J. Mater Corros, 2010; 61: 1[16] Hou P Y. J Mater Sci, 2009; 44: 1711[17] Soboyejo W O, Mensah P, Diwan R, Crowe J, Akwaboa S. Mater Sci Eng, 2011; A528: 2223[18] Toscano J P. PhD Thesis, RWTH–Aachen University, Germany, 2008[19] Quadakkers W J, Elschner A, Holzbrecher H, Schmidt K, Speier W, Nickel H. Microchim Acta, 1992; 107: 197[20] Quadakkers W J, Naumenko D, Wessel E, Kochubey V, Singheiser L. Oxid Met, 2004; 61: 17[21] Hou P Y, Izumi T, Gleeson B. Oxid Met, 2009; 752: 109[22] Patterson T, Leon A, Jayaraj B, Liu J, Sohn Y H. Surf Coat Technol, 2008; 203: 437[23] Basu S N, Halloran J W. Oxid Met, 1987; 27: 143[24] Puetz P, Huang X, Lima R S, Yang Q, Zhao L. Surf Coat Technol, 2010; 205: 647[25] Subanovic M. PhD Thesis, RWTH–Aachen University, Germany, 2009 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|