金属学报  2011, Vol. 47 Issue (6): 655-662    DOI: 10.3724/SP.J.1037.2010.00713
  论文 本期目录 | 过刊浏览 |
La和Hf对CoNiCrAl合金涂层高温氧化行为的影响
宋鹏1,2,陆建生1,张德丰1,吕建国3,李德江4
1. 昆明理工大学材料科学与工程学院, 昆明 650093
2. Forschungszentrum Juelich, IEK-2, Juelich 52425, Germany
3. 昆明理工大学应用技术学院, 昆明 650093
4. 上海交通大学材料科学与工程学院, 上海 200240
EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS
SONG Peng 1,2, LU Jiansheng 1, ZHANG Defeng 1, L¨U Jianguo 3, LI Dejiang 4
1. Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093
2. Forschungszentrum Juelich, IEK–2, Juelich 52425, Germany
3. Faculty of Applied Technology, Kunming University of Science and Technology, Kunming 650093
4. School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
引用本文:

宋鹏 陆建生 张德丰 吕建国 李德江. La和Hf对CoNiCrAl合金涂层高温氧化行为的影响[J]. 金属学报, 2011, 47(6): 655-662.
, , , , . EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS[J]. Acta Metall Sin, 2011, 47(6): 655-662.

全文: PDF(4924 KB)  
摘要: 对单一添加及同时添加La和Hf的CoNiCrAl合金进行真空高温氧化处理, 研究单一添加与同时添加La和Hf对合金表面氧化物生长机制和黏结性能的影响. 结果表明: 表面抛光的合金在1100℃氧化时, 同时添加La和Hf使CoNiCrAl合金在其表面形成了连续均匀的Al2O3, 并且具有较好的黏结性能.通过18O追踪原子氧化发现CoNiCrAlLa, CoNiCrAlHf和CoNiCrAlLaHf合金的Al2O3生长均为O2-内扩散为主的生长机制,同时伴随少量的金属离子外扩散. 单一添加La和Hf, 形成的Al2O3表面富集Cr,Co和Ni等, 且随Al2O3深度增加而逐渐降低, 这些元素促使Al2O3表面形成Ni(Co)Al2O4, 从而降低Al2O3的黏结性能. 同时添加La和Hf,没有改变O2-内扩散为主的生长机制, 但Hf能够阻碍La在氧化物/合金界面的富集,减少Ni(Co)Al2O4形成, 同时合金表面局部内氧化的钉扎效应提高了Al2O3的黏结性能.
关键词 : CoNiCrAl合金,  La,  Hf,  高温氧化,  生长机制    
Abstract:CoNiCrAl alloys are widely used as bond coats for thermal barrier coating (TBC) at high operating temperature for energy conversion systems, especially turbine. However, the effect of reactive element (RE) on the oxidation behavior of CoNiCrAl alloys is still not uniform, thereby limiting the usage of the alloys. To study the effect of co–doped RE, the polished cast CoNiCrAlLa, CoNiCrAlHf and CoNiCrAlLaHf alloys were oxidized at 1100 ℃ in vacuum. Growth kinetics and adherence of oxide scales formed on above alloys were studied through comparing mass dynamics curves and tracer oxidation of the alloys. SEM, TG and XRD as well as secondary neutrals mass spectrometry (SNMS) were employed to study the microstructure and growth mechanism of the oxide layers. The results showed that a protective Al2O3 scale formed on the surface of CoNiCrAlLaHf alloy, and the Al2O3 scale showed a good adherence due to a pinning effect of the internal oxidation and less Ni(Co)Al2O4 formation. The Hf could suppress La enrichment at the oxide/alloy interface for the co–doped alloy. Oxygen inwards–diffusion along the oxide, which mainly controlled oxide scale growth, was observed when these three alloys oxidized in the atmospheres including tracer 18O. Enrichment of Cr, Co and Ni occurred at the outer part of oxide scale, and then decreased to a low level within the oxide layer. These Cr, Co and Ni enrichments could promote the Ni(Co)Al2O4 formation at the top of oxide scale for the single–doped alloys, which was detrimental to Al2O3 adherence properties.
Key words: CoNiCrAl alloy    La    Hf    high temperature oxidation    growth mechanism
收稿日期: 2010-12-31     
作者简介: 宋鹏, 男, 1979年生, 博士
[1] Padture N P, Gell M, Jordan E H. Science, 2002; 296: 280

[2] Clarke D R, Levi C G. Annu Rev Mater Res, 2003; 33: 383

[3] Evans A G, Mumm D R, Hutchinson J W, Meier G H, Pettit F S. Prog Mater Sci, 2001; 46: 505

[4] Wu R T, Reed R C. Acta Mater, 2008; 56: 313

[5] Nijdama T J, Sloof W G. Acta Mater, 2007; 55: 5980

[6] Naumenko D, Kochubey V, Niewolak L, Dymiati A, Mayer J, Singheiser L, Quadakkers W J. J Mater Sci, 2008; 43: 4550

[7] Haynes J A, Pint B A, More K L, Zhang Y, Wright I G. Oxid Met, 2002; 58: 513

[8] Pint B A. J Am Ceram Soc, 2003; 86: 686

[9] Hamadi S, Bacos M P, Poulain M, Seyeux A, Maurice V, Marcus P. Surf Coat Technol, 2009; 204: 756

[10] Kuenzly J D, Douglass D L. Oxid Met, 1974; 8: 139

[11] Pint B A. Oxid Met, 1996; 45: 1

[12] Carling K M, Carter E A. Acta Mater, 2007; 55: 2791

[13] Evans E. Int Mater Rev, 1995; 40: 1

[14] Wessel E, Kochubey V, Naumenko D, Niewolak L, Singheiser L, Quadakkers W J. Scr Mater, 2004; 51: 987

[15] Young D J, Naumenko D, Niewolak L,Wessel E, Singheiser L, Quadakkers W J. Mater Corros, 2010; 61: 1

[16] Hou P Y. J Mater Sci, 2009; 44: 1711

[17] Soboyejo W O, Mensah P, Diwan R, Crowe J, Akwaboa S. Mater Sci Eng, 2011; A528: 2223

[18] Toscano J P. PhD Thesis, RWTH–Aachen University, Germany, 2008

[19] Quadakkers W J, Elschner A, Holzbrecher H, Schmidt K, Speier W, Nickel H. Microchim Acta, 1992; 107: 197

[20] Quadakkers W J, Naumenko D, Wessel E, Kochubey V, Singheiser L. Oxid Met, 2004; 61: 17

[21] Hou P Y, Izumi T, Gleeson B. Oxid Met, 2009; 752: 109

[22] Patterson T, Leon A, Jayaraj B, Liu J, Sohn Y H. Surf Coat Technol, 2008; 203: 437

[23] Basu S N, Halloran J W. Oxid Met, 1987; 27: 143

[24] Puetz P, Huang X, Lima R S, Yang Q, Zhao L. Surf Coat Technol, 2010; 205: 647

[25] Subanovic M. PhD Thesis, RWTH–Aachen University, Germany, 2009
[1] 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江. 镁合金抗高温氧化机理研究进展[J]. 金属学报, 2023, 59(3): 371-386.
[2] 徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生. 微量Al、Ti对Inconel 690合金高温氧化行为的影响[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] 张丽丽, 吉宗威, 赵九洲, 何杰, 江鸿翔. 亚共晶Al-Si合金中微量元素La变质共晶Si的关键影响因素[J]. 金属学报, 2023, 59(11): 1541-1546.
[4] 丛鸿达, 王金龙, 王成, 宁珅, 高若恒, 杜瑶, 陈明辉, 朱圣龙, 王福会. 新型无机硅酸盐复合涂层制备及其在高温水蒸气环境的氧化行为[J]. 金属学报, 2022, 58(8): 1083-1092.
[5] 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会. 制备工艺对FGH4097高温合金微观组织与性能的影响[J]. 金属学报, 2022, 58(8): 992-1002.
[6] 温冬辉, 姜贝贝, 王清, 李相伟, 张鹏, 张书彦. MoNb改性FeCrAl不锈钢高温组织演变和力学性能[J]. 金属学报, 2022, 58(7): 883-894.
[7] 陈建军, 丁雨田, 王琨, 闫康, 马元俊, 王兴茂, 周胜名. Laves相对 GH3625合金管材热挤压过程中爆裂行为的影响[J]. 金属学报, 2021, 57(5): 641-650.
[8] 杨亮, 吕皓天, 万春磊, 巩前明, 陈浩, 张弛, 杨志刚. 综述:活性元素作用机理——氧化物“钉扎”模型[J]. 金属学报, 2021, 57(2): 182-190.
[9] 郑秋菊, 叶中飞, 江鸿翔, 卢明, 张丽丽, 赵九洲. 微合金化元素La对亚共晶Al-Si合金凝固组织与力学性能的影响[J]. 金属学报, 2021, 57(1): 103-110.
[10] 吴贇, 刘雅辉, 康茂东, 高海燕, 王俊, 孙宝德. K4169合金循环加载过程中的微观组织演变[J]. 金属学报, 2020, 56(9): 1185-1194.
[11] 杜瑜宾, 胡小锋, 张守清, 宋元元, 姜海昌, 戎利建. 含1.4%Cu的HSLA钢的组织和力学性能[J]. 金属学报, 2020, 56(10): 1343-1354.
[12] 赵明雨,甄会娟,董志宏,杨秀英,彭晓. 新型耐磨耐高温氧化NiCrAlSiC复合涂层的制备及性能研究[J]. 金属学报, 2019, 55(7): 902-910.
[13] 高博, 王磊, 宋秀, 刘杨, 杨舒宇, 千叶晶彦. 预氧化对Co-Al-W基高温合金高温氧化和热腐蚀行为的影响[J]. 金属学报, 2019, 55(10): 1273-1281.
[14] 王帅鹏, 罗文华, 李赣, 李海波, 张广丰. La含量对Ce-La合金氢化动力学的影响[J]. 金属学报, 2018, 54(8): 1187-1192.
[15] 白银, 刘正东, 谢建新, 包汉生, 陈正宗. 预氧化处理对G115钢高温蒸气氧化行为的影响[J]. 金属学报, 2018, 54(6): 895-904.