| Q&P工艺处理低碳CrNi3Si2MoV钢中马氏体的研究 |
| 王存宇,时捷,曹文全,惠卫军,王毛球,董瀚 |
| 钢铁研究总院结构材料研究所, 北京 100081 |
|
| STUDY ON THE MARTENSITE IN LOW CARBON CrNi3Si2MoV STEEL TREATED BY Q&P PROCESS |
| WANG Cunyu, SHI Jie, CAO Wenquan, HUI Weijun, WANG Maoqiu, DONG Han |
| Institute for Structural Materials, Central Iron & Steel Research Institute, Beijing 100081 |
引用本文:
王存宇 时捷 曹文全 惠卫军 王毛球 董瀚. Q&P工艺处理低碳CrNi3Si2MoV钢中马氏体的研究[J]. 金属学报, 2011, 47(6): 720-726.
,
,
,
,
,
.
STUDY ON THE MARTENSITE IN LOW CARBON CrNi3Si2MoV STEEL TREATED BY Q&P PROCESS[J]. Acta Metall Sin, 2011, 47(6): 720-726.
| [1] Edmonds D V, He K Rizzo F C, Cooman B C De, Matlock D K, Speer J G. Mater Sci Eng, 2006; A438–440: 25[2] Hsu T Y. Heat Treat, 2007; 22: 1(徐祖耀. 热处理, 2007, 22: 1)[3] Rizzo F, Martins A R, Speer J G. Mater Sci Forum, 2007;539–543: 4476[4] Zhong N, Wang X D, Huang B X, Rong Y H, Wang L. In: Lee H C ed., The 3rd International Coference on Advanced Structural Steels, Gyeongju: The Korean Institute of Metals and Materials, 2006: 885[5] DeCooman B C, Speer J G. In: Lee H C eds, The 3rd International Cnferece on Advanced Structural Steels, Gyeongju: The Korean Institute of Metals and Materials, 2006: 798[6] Wang C Y, Shi J, Cao W Q, Dong H. Trans Mater Heat Treat, 2010; 31(6): 83(王存宇, 时捷, 曹文全, 董瀚. 材料热处理学报, 2010; 31(6): 83)[7] Wang C Y. PhD Thesis. Central Iron & Steel Research Institute, Beijing, 2010(王存宇. 钢铁研究总院博士学位论文, 北京, 2010)[8] Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426–432: 1089[9] Gerdeman F L H, Speer J G, Matlock D K. In: Margaret A B ed., Materials Science and Technology Conference Proceedings, New Orleans: Association for Iron and Steel Technology, 2004: 439[10] MaM T,Wu B R. Dual Phase Steel–Physical and Mechanical Metallurgy, Beijing: Metallurgical Industry Press,2009: 117(马鸣图, 吴宝榕. 双相钢--物理和力学冶金. 北京: 冶金工业出版社, 2009: 117)[11] Hsu T Y. Martensitic Transformation and Martensite. 2nd Ed, Beijing: Science Press, 1999: 228(徐祖耀. 马氏体相变与马氏体. 第二版. 北京: 科学出版社, 1999: 228)[12] Yu D G. Fe–base Martensitic Aging–Tempering Transformation Theory and the Strength and Toughness. Shanghai: Shanghai Jiaotong University Press, 2008: 194(俞德刚. 铁基马氏体时效--回火转变理论及其强韧性. 上海: 上海交通大学出版社, 2008: 194)[13] Wang C Y, Shi J, CaoWQ, Dong H. Mater Sci Eng, 2010; A527: 3442[14] Cox T B, Low J R. Metall Trans, 1974; 5: 1457[15] Quentin Furnemont. PhD Thesis, Universit´e catholique de Louvain, 2003[16] Pascal Jacques. PhD Thesis, Universit´e catholique de Louvain, 1998[17] Marder A R, Krauss G. Trans ASM, 1969; 62: 957[18] Krauss G, Marder A R. Metall Trans, 1971; 2: 2343[19] Marder J M, Marder A R. Trans ASM, 1969; 62: 1[20] Su D D, Li J J. High–Temperature Metallography of Steel In situ Observation of Phase Transformation, Tianjin:Tianjin university Press, 2007: 144(苏德达, 李家俊. 钢的高温金相学--钢的相变过程原位观察. 天津: 天津大学出版社, 2007: 144)[21] Morito S, Saito H, Ogawa T, Furuhara T, Maki T. ISIJ Int, 2005; 45: 91[22] Erdogan M. J Mater Sci, 2002; 37: 3623[23] Hasegawa K, Kawamura K, Urabe T. ISIJ Int, 2004; 44: 603[24] Pychmintsev I Y, Savrai R A, DeCooman B C. In: Decooman B C ed. Conference on TRIP–Aided High Strength Ferrous Alloys, Ghent: Mainz in Aachen, 2002: 79[25] Hu G X. Metallography. Shanghai: Shanghai Scientific & Technical Publishers, 1980: 260(胡庚祥, 金属学. 上海: 上海科学技术出版社, 1980: 260)[26] Tvergaard V. Adv Appl Mech, 1990; 27: 83[27] McMeeking R M. J Mech Phys Solids, 1977; 25: 357[28] Xia L, Shih C F. J Mech Phys Solids, 1996; 44: 603[29] Xia L, Shih C F. J Mech Phys Solids, 1995; 43: 233 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|