| 强磁场对低活化钢中析出行为和力学性能的影响 |
| 夏志新,张弛,杨志刚 |
| 清华大学材料科学与工程系 先进材料教育部重点实验室, 北京 100084 |
|
| EFFECT OF HIGH MAGNETIC FIELD ON PRECIPITATION BEHAVIORS AND MECHANICAL PROPERTIES IN REDUCED ACTIVATION STEELS |
| XIA Zhixin, ZHANG Chi, YANG Zhigang |
Key Laboratory of Advanced Materials of Ministry of Education, Department of Materials Science and Engineering,
Tsinghua University, Beijing 100084 |
引用本文:
夏志新 张弛 杨志刚. 强磁场对低活化钢中析出行为和力学性能的影响[J]. 金属学报, 2011, 47(6): 713-719.
,
,
.
EFFECT OF HIGH MAGNETIC FIELD ON PRECIPITATION BEHAVIORS AND MECHANICAL PROPERTIES IN REDUCED ACTIVATION STEELS[J]. Acta Metall Sin, 2011, 47(6): 713-719.
| [1] Baluc N, Gelles D S, Jitsukawa S, Kimura A, Klueh R L, Odette G R, Schaaf B van der, Yu J N. J Nucl Mater, 2007; 367: 33[2] Hao X J, Ohtsuka H, Rango P D, Wada H. Mater Trans, 2003; 44: 211[3] Choi J K, Ohtsuka H, Xu Y, Choo W Y. Scr Mater, 2000; 43: 221[4] Kohno Y, Konishi Y, Konishi H, Shibata K, Wada H. Mater Sci Eng, 1999; A273: 21[5] Zhou Z N, Wu K M. Scr Mater, 2009; 61: 670[6] Zhang Y D, Zhao X, Bozzolo N, He C S, Zhuo L, Esling C. ISIJ Int, 2005; 45: 913[7] Xia Z X, Zhang C, Yang Z G, Wang P H, Chen J M, Xu Z Y, Li X W, Liu S. Mater Sci Eng, 2010; A528: 657[8] Xia Z X, Zhang C, Lan H, Liu Z Q, Yang Z G. Mater Lett, 2011; 65: 937[9] Zhang Y D, Gey N, He C S, Zhao X, Esling C. Acta Mater, 2004; 52: 3467[10] Hsu T Y. Theory of Phase Transformation. Beijing: Science Press of China, 1988: 35(徐祖耀. 相变原理. 北京: 科学出版社, 1988: 35)[11] Jile D. Introduction to Magnetism and Magnetic Materials, London: Chapman & Hall, 1991: 254[12] Langer J S, Schwartz A. Phys Rev, 1980; 21A: 948[13] Xia Z X, Zhang C, Yang Z G. J Mater Sci, 2011; 46: 3151[14] Fujii H, Tsurekawa S. Phys Rev, 2011; 83B: 054412[15] Zhang C, Enomoto M, Yamashita T, Sano N. Metall Mater Trans, 2004; 35A: 1264[16] Cahn J W, Hilliard J E. J Chem Phys, 1959; 31: 688[17] Yang Z G, Enomoto M. Mater Sci Eng, 2002; A332: 184[18] Johnson C A. Surf Sci, 1965; 3: 429[19] Schneider A, Inden G. Acta Mater, 2005; 53: 519[20] Yong Q L, Zheng L. Acta Metall Sin, 1984; 20: A9(雍岐龙, 郑鲁. 金属学报, 1984; 20: A9)[21] Ashby M F. Acta Metall, 1966; 14: 679[22] Kelly A, Nicholson R B. Prog Mater Sci, 1963; 10: 151[23] James L Maloney, Warren M Garrison Jr. Acta Mater, 2005; 53: 533 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|