| 淬火温度对TC16钛合金显微组织及变形行为的影响 |
| 张志强,董利民,杨洋,关少轩,刘羽寅,杨锐 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| INFLUENCES OF QUENCHING TEMPERATURE ON THE MICROSTRUCTURE AND DEFORMATION BEHAVIORS OF TC16 TITANIUM ALLOY |
| ZHANG Zhiqiang, DONG Limin, YANG Yang, GUAN Shaoxuan, LIU Yuyin, YANG Rui |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
张志强 董利民 杨洋 关少轩 刘羽寅 杨锐. 淬火温度对TC16钛合金显微组织及变形行为的影响[J]. 金属学报, 2011, 47(10): 1257-1262.
,
,
,
,
,
.
INFLUENCES OF QUENCHING TEMPERATURE ON THE MICROSTRUCTURE AND DEFORMATION BEHAVIORS OF TC16 TITANIUM ALLOY[J]. Acta Metall Sin, 2011, 47(10): 1257-1262.
| [1] Zhang Q L, Wang Q R, Li X W. Mater Eng, 2007; 284: 11(张庆玲, 王庆如, 李兴无. 材料工程, 2007; 284: 11)[2] Ma Q Q, Zheng W W, Li X W. Mater Eng, 2009; 308: 19(马琴琴, 郑为为, 李兴无. 材料工程, 2009; 308: 19)[3] Li X W, Lu M X, Sha A X, Zhang L. Mater Sci Eng, 2008; A490: 193[4] Wu C Z, Li X W. Rare Met Mater Eng, 2008; 37(suppl.3): 580(吴崇周, 李兴无. 稀有金属材料与工程, 2008; 37(增3): 580)[5] Sha A X, Li X W, Li H E, Wang Q R. Chin J Nonferrous Met, 2010; 20: 943(沙爱学, 李兴无, 李红恩, 王清瑞. 中国有色金属学报, 2010; 20: 943)[6] Li X W, Sha A X, Chu J P, Zhang L, Lu M X. Mater Eng, 2007; 292: 3(李兴无, 沙爱学, 储俊鹏, 张雷, 路民旭. 材料工程, 2007; 292: 3)[7] Li X W, Su S M, Lu M X, Sha A X, Chu J P. J Aeronaut Mater, 2008; 28(3): 82(李兴无, 苏生明, 路民旭, 沙爱学, 储俊鹏. 航 空材料学报, 2008; 28(3): 82)[8] Sass S L. J Less–Common Met, 1972; 28: 157[9] Jones N G, Dashwood R J, Jackson M, Dye D. Acta Mater, 2009; 57: 3830[10] Boyer R, Welsch G, Collings E W. Materials Properties Handbook: Titanium Alloy. OH, Materials Park: ASM International, 1994: 41[11] Luetjering G, Williams J C. Titanium. Heidelberg: Springer, 2003: 30[12] Borisova E A et al, translated by Chen S Q. Metallography of Titanium Alloys. Beijing: National Defence Inductry Press, 1986: 327(鲍利索娃 E A 等著, 陈石卿 译. 钛合金金相学. 北京: 国防工业出版社, 1986: 327)[13] Duerig T W, Albrecht J, Richter D, Fishcher P. Acta Mater, 1982; 30: 2161[14] Duerig T W, Terlinde G T, Williams J C. Metall Trans, 1980; 11A: 1987[15] Grosdidier T, Philippe M J. Mater Sci Eng, 2000; A291: 218 |
|