| 7075-T6铝合金搅拌摩擦焊焊缝表面带状纹理的组织与性能 |
| 康举1), 栾国红1), 付瑞东2) |
1) 北京航空制造工程研究所中国搅拌摩擦焊中心, 北京 100024
2) 燕山大学材料科学与工程学院, 秦皇岛 066004 |
|
| MICROSTRUCTURES AND MECHANICAL PROPERTIES OF BANDED TEXTURES OF FRICTION STIR WELDED 7075-T6 ALUMINUM ALLOY |
| KANG Ju1), LUAN Guohong1), FU Ruidong2) |
1) Beijing Aeronautical Manufacturing Technology Research Institute, China Friction Stir Welding Center, Beijing 100024
2) Yanshan University, College of Materials Science and Engineering, Qinhuangdao 066004 |
引用本文:
康举 栾国红 付瑞东. 7075-T6铝合金搅拌摩擦焊焊缝表面带状纹理的组织与性能[J]. 金属学报, 2011, 47(2): 224-230.
,
,
.
MICROSTRUCTURES AND MECHANICAL PROPERTIES OF BANDED TEXTURES OF FRICTION STIR WELDED 7075-T6 ALUMINUM ALLOY[J]. Acta Metall Sin, 2011, 47(2): 224-230.
| [1] Matrukanitz R P. ASM Handbook–Welding, Brazing and Soldering. Ohio, Geauga: ASM Int, 1990: 528[2] Thomas W M, Nicholas E D, Needham J C, Murch M G, Templesmith P, Dawes C J. Int Pat, PCT/GB92/02203, 1991[3] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1[4] Cavaliere P, Cerri E, Squillace A. J Mater Sci, 2005; 40: 3669[5] Lumsden J B, Mahoney M W, Pollock G. Corrosion, 1999; 55: 1127[6] Kang J, Fu R D, Luan G H, Dong C L, He M. Corros Sci, 2010; 52: 620[7] Chai P, Luan GH, Guo D L, Li J. Trans China Weld Inst, 2005; 26: 79(柴 鹏, 栾国红, 郭德伦, 李 菊. 焊接学报, 2005; 26: 79)[8] Li Y, Murr L E, Mclure J C. Scr Mater, 1999; 40: 1041[9] Lu S X, Yan J C, Li W G, Yang S Q. Acta Metall Sin (Engl Lett), 2005; 18: 552[10] Rhodnev C G, Mahonev M V, Bingel W H. Scr Mater, 1997; 37: 69[11] Krishnan K N. Mater Sci Eng, 2002; A327: 246[12] Liu H J, Chen Y C, Feng J C. Scr Mater, 2006; 55: 231[13] Attallah M M, Salem H G. Mater Sci Eng, 2005; A391: 51[14] Dawes C J. Sheet Metal Ind–Weld Join, 1995; 72: 22[15] Cui G R, Ma Z Y, Li S X. Scr Mater, 2008; 58: 1082[16] Wang D Y, Feng J C. Trans China Weld Inst, 2003; 24: 42(王大勇, 冯吉才. 焊接学报, 2003; 24: 42)[17] Chen Z W, Cui S. Scr Mater, 2008; 58: 417[18] Yan J H, Sutton M A, Reynolds A P. Sci Technol Weld Joining, 2007; 12: 72[19] Jin H, Saimoto S, Ball M, Threadgill P L. Mater Sci Technol, 2001; 17: 1605[20] Schneider J A, Nunes A C. Metall Mater Trans, 2004; 35B: 777[21] Yang B S, Yan J H, Michael S A, Reynolds P A. Mater Sci Eng, 2004; A364: 55[22] Zhu R Z. Metal Corrosion Science. Beijing: China Metallurgical Industry Press, 1989: 97–131(朱日彰. 金属腐蚀学. 北京: 冶金工业出版社, 1989: 97-131)[23] Cao G, Kou S. Weld J, 2005; 1: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|