| 添加Cu对M5合金在500℃过热蒸汽中耐腐蚀性能的影响 |
| 李士炉1), 姚美意1), 张欣1), 耿建桥1), 彭剑超2), 周邦新1) |
1) 上海大学材料研究所, 上海 200072
2) 上海大学微结构重点实验室, 上海 200444 |
|
| EFFECT OF ADDING Cu ON THE CORROSION RESISTANCE OF M5 ALLOY IN SUPERHEATED STEAM AT 500℃ |
| LI Shilu1), YAO Meiyi1), ZHANG Xin1), GENG Jianqiao1), PENG Jianchao2), ZHOU Bangxin1) |
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Key Laboratory for Advanced Micro-Analysis, Shanghai University, Shanghai 200444 |
引用本文:
李士炉 姚美意 张欣 耿建桥 彭剑超 周邦新. 添加Cu对M5合金在500℃过热蒸汽中耐腐蚀性能的影响[J]. 金属学报, 2011, 47(2): 163-168.
,
,
,
,
,
.
EFFECT OF ADDING Cu ON THE CORROSION RESISTANCE OF M5 ALLOY IN SUPERHEATED STEAM AT 500℃[J]. Acta Metall Sin, 2011, 47(2): 163-168.
| [1] Park J Y, Choi B K, Yoo S J, Jeong Y H. J Nucl Mater, 2006; 359: 59[2] Park J Y, Yoo S J, Choi B K, Jeong Y H. J Alloys Compd, 2007; 437: 274[3] Hong H S, Moon J S, Kim S J, Lee K S. J Nucl Mater, 2001; 297: 113[4] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1[5] Kim J M, Jeong Y H. J Nucl Mater, 1999; 275: 74[6] Charquet D, Hahn R, Ortlieb E, Gros J P, Wadier J F. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1988: 405[7] Anada H, Takeda K. In: Sabol G P, Bradley E R eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 35[8] Wadman B, Lai Z, Andr´en H O, Nystr¨om A L, Rudling P, Pettersson H. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: 10th International Symposium, ASTM STP 1245, Ann Arbor: ASTM International, 1994: 579[9] Jeong Y H, Lee K O, Kim H G. J Nucl Mater, 2002; 302: 9[10] Kim H G, Jeong Y H, Kim T H. J Nucl Mater, 2004; 326: 125[11] Jeong Y H, Kim H G, Kim D J. J Nucl Mater, 2003; 323: 72[12] Abe T, Shimono M, Ode M, Onodera H. Acta Mater, 2006; 54: 909[13] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260(杨文斗. 反应堆材料学. 第二版. 北京: 原子能出版社, 2006: 260)[14] Zhou B X, Li Q, Yao M Y, Liu W Q. Nucl Power Eng, 2005; 26: 364(周邦新, 李 强, 姚美意, 刘文庆. 核动力工程, 2005; 26: 364)[15] Zhou B X, Li Q, LiuWQ, YaoMY, Chu Y L. Rare Metal Mat Eng, 2006; 35: 1009(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)[16] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Intl, 2008; 5: 360 |
|