| 0.02%Nb空冷仿晶界型铁素体/粒状贝氏体复相钢的相变及强韧性 |
| 冯春;方鸿生;白秉哲;郑燕康 |
| 清华大学材料科学与工程系先进材料教育部重点实验室; 北京 100084 |
|
| PHASE TRANSFORMATION AND STRENGTH–TOUGHNESS OF A FGBA/BG DIPHASE STEEL CONTAINING 0.02%Nb |
| FENG Chun; FANG Hongsheng; BAI Bingzhe; ZHENG Yankang |
| Key Laboratory of Advanced Materials of Ministry of Education; Department of Material Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
冯春 方鸿生 白秉哲 郑燕康. 0.02%Nb空冷仿晶界型铁素体/粒状贝氏体复相钢的相变及强韧性[J]. 金属学报, 2010, 46(4): 473-478.
,
,
,
.
PHASE TRANSFORMATION AND STRENGTH–TOUGHNESS OF A FGBA/BG DIPHASE STEEL CONTAINING 0.02%Nb[J]. Acta Metall Sin, 2010, 46(4): 473-478.
| [1]Thompson SW, Colvin D J, Krauss G. Metall Trans, 1990; 21A: 1493
[2]Park K T, Kim Y S, Lee J G. Mater Sci Eng, 2000; A293: 165
[3]Adachi Y, Tomida T, Hinotani S. Tetsu Hagan´e 1999, 85,620
[4](足立吉隆, 富田俊郎, 日野谷重晴. 铁と钢, 1999; 85: 620)
[5]Hickson M R, Gibbs R K, Hondgson P D. ISIJ Int 1999, 39,1176
[6]Han B Q, Yue S. J Mater Process Technol 2003, 136,100
[7]Fang H S, Feng C, Zheng Y K, Bai B Z. J Iron Steel Res Int, 2008; 15: 1
[8]Xu P G, Fang H S, Bai B Z. J Iron Steel Res Int, 2002; 9: 33
[9]Xu P G, Fang H S, Bai B Z. Acta Metall Sin, 2002; 38: 255
[10](徐平光, 方鸿生, 白秉哲. 金属学报, 2002; 38: 255)
[11]Wang J P, Yang Z G, Bai B Z, Fang H S. Mater Sci Eng, 2004; A369: 112
[12]Li L, Ding H, Du L X. Acta Metall Sin, 2006; 42: 1227
[13](李龙, 丁桦, 杜林秀. 金属学报, 2006; 42: 1227)
[14]Lee Y K. In: Hong J M eds., Proc of the 2nd Symposium on Development of Advanced Steels. Shenyang: Northeastern University Press, 2004: 29
[15]Abad R, Fernandez A I, Lqpez B. ISIJ Int 2001, 41,1373
[16]Petrov R, Kestens L, Houbaert Y. Mater Charact 2004, 53,51
[17]Deng T Y, Xu Y B, Yuan X Q. Acta Metall Sin, 2007; 43: 1091
[18](邓天勇, 许云波, 袁向前. 金属学报, 2007; 43: 1091)
[19]Yuan X Q, Liu Z Y, Jiao S H. ISIJ Int 2006, 46,579
[20]Sato K, Suehiro M. Tetsu Hagan´e 1991, 77,675
[21](佐藤一昭, 末广正芳. 铁と钢, 1991; 77: 675)
[22]Zrník J, Kvackaj T. Mater Sci Eng, 2001; A319: 321
[23]Fang H S, Wang J J. Acta Metall Sin, 1994; 30: 491
[24](方鸿生, 王家军. 金属学报, 1994; 30: 491)
[25]Aaronson H I. Decomposition of Austenite by Diffusional Processes. New York: Interscience Press, 1962: 387
[26]Weiss I, Jonas J J. Metall Trans, 1979; 10A: 831
[27]Hansen S S, Vandersande J B, Cohen M. Metall Tran, 1980; 11A: 387
[28]Jonas J J, Akben M G. Met Forum, 1981; 4: 92
[29]Coladas R, Masounave J. In: Bailon J P eds., Proc of Int Conf on The Hot Deformation of Austenite. New York: the Metallurgical Society of AIME, 1977: 341
[30]Yamamoto S, Ouchi C. In: Osuka T eds.Proc of Int Conf on Thermomechanical Processing of Microalloyed Austenite. New York: The etallurgical Society of AIME, 1982:613
[31]Medina S F. Scr Metall ater 1995, 32,43
[32]Irvine K J, Pickerin F B, Gladman T. J Iron Steel Inst, 1967; 205: 161
[33]Fang H S, Wang J J, Yang Z G. Bainite Transformation. Beijing: Science Press, 1999: 13
[34](方鸿生, 王家军, 杨志刚. 贝氏体相变. 北京: 科学出版社, 1999: 13)
[35]Fang H S, Bai B Z, Zheng X H. Acta Metall Sin, 1986; 22: 283
[36](方鸿生, 白秉哲, 郑秀华. 金属学报, 1986; 22: 283)
[37]Xu F Y. PhD Thesis, Tsinghua University, Beijing, 2009
[38](许峰云. 清华大学博士论文, 北京, 2009) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|