Please wait a minute...
金属学报  2010, Vol. 46 Issue (2): 161-166    DOI: 10.3724/SP.J.1037.2009.00432
  论文 本期目录 | 过刊浏览 |
基于过冷奥氏体动态相变的热轧TRIP钢组织控制 II. 动态相变后冷却速率
尹云洋1;3;杨王玥1;李龙飞2;孙祖庆2;王西涛2
1. 北京科技大学材料科学与工程学院; 北京 100083
2. 北京科技大学新金属材料国家重点实验室; 北京 100083
3. 武汉钢铁(集团)公司研究院; 武汉 430080
MICROSTRUCTURE CONTROL OF HOT ROLLED TRIP STEEL BASED ON DYNAMIC TRANSFORMATION OF UNDERCOOLED AUSTENITE
II. Cooling Rate After Dynamic Transformation of Undercooled Austenite
YIN Yunyang 1;3; YANG Wangyue 1; LI Longfei 2; SUN Zuqing 2; WANG Xitao 2
1. School of Materials Science and Engineering; University of Science & Technology Beijing; Beijing 100083
2. State Key Laboratory for Advanced Metals and Materials; University of Science & Technology Beijing; Beijing 100083
3. Research and Development Center; Wuhan Iron and Steel (Group) Corp.; Wuhan 430080
引用本文:

尹云洋 杨王玥 李龙飞 孙祖庆 王西涛. 基于过冷奥氏体动态相变的热轧TRIP钢组织控制 II. 动态相变后冷却速率[J]. 金属学报, 2010, 46(2): 161-166.
, , , , . MICROSTRUCTURE CONTROL OF HOT ROLLED TRIP STEEL BASED ON DYNAMIC TRANSFORMATION OF UNDERCOOLED AUSTENITE
II. Cooling Rate After Dynamic Transformation of Undercooled Austenite[J]. Acta Metall Sin, 2010, 46(2): 161-166.

全文: PDF(1850 KB)  
摘要: 

利用OM, SEM和TEM等研究了动态相变后的冷却速率对基于动态相变的热轧TRIP钢组织控制影响.结果表明, 动态相变后的冷却过程中, 亚稳的未相变奥氏体会继续以形核为主的方式发生铁素体相变. 随着冷却速率的降低, 铁素体体积分数增多, 铁素体晶粒内的位错回复较为充分,但铁素体晶粒尺寸变化不大. 控制一定的冷却速率(30℃/s), 可使实验钢组织中铁素体体积分数及位错密度适中, 残余奥氏体体积分数较高, 具有较好的强度及塑性.

关键词 : 热轧TRIP钢,  过冷奥氏体动态相变 (DTUA),  冷却速率,  显微组织,  力学性能    
Abstract:

TRIP–aided steels are ideal for lightweight automotive applications due to their high strength and ductility. Thermomechanical processing simulations were performed by hot compression on a Gleeble–1500 machine, in order to develop a comprehensive understanding of the effect of cooling rate after dynamic transformation of undercooled austenite (DTUA) on the microstructure evolution and mechanical properties of 0.2C–1.5Mn–0.5Si–1.0Al (mass faction, %) transformation–induced plasticity (TRIP) steel. The results show that the metastable austenite would be transformed to ferrite mainly by means of nucleation during cooling after DTUA. Decreasing the cooling rate after DTUA, the vlume fraction of ferrite increase, the static recovery of dislocations in ferrite produced during dynamic transformation could fully take place, thus the density of dislocations in ferrite decreased through by rearranging and merging, but the grain size of ferrite changes little. At the cooling rate of 30℃/s, the investigated steel has a moderate volume fraction of ferrite and dislocation density in ferrite and a higher volume fraction of retained austenite, resulting in the steel having a higher strength and plasticity.

Key words: hot rolled TRIP steel    dynamic transformation of undercooled austenite (DTUA)    cooling rate    microstructure    mechanical property
收稿日期: 2009-06-29     
基金资助:

国家高技术研究发展计划资助项目2007AA03Z501和高等学校博士学科点专项科研基金项目200800081014资助

作者简介: 尹云洋, 男, 1976年生, 博士生

[1] Zackay V F, Parker E R, Fahr D, Bush R. Trans ASM, 1967; 60: 252
[2] Traint S, Pichler A, Hauzenberger K, Stiaszny P, Werner E. Steel Res, 2002; 73: 259
[3] Van der Zwaag S, Zhao L, Suzelotte O, Sietsma J. ISIJ Int, 2002; 42: 1565
[4] Sakuma Y, Matsumura O, Takechi H. Metall Trans, 1991; 22A: 489
[5] Koh H, Lee S, Park S, Choi S J, Kwon S J, Kim N J. Scr Mater, 1998; 38: 763
[6] Ryu H B, Speer J G, Wise J P. Metall Mater Trans, 2002; 33A: 2811
[7] Girault E, Mertens A, Jacques P, Houbaert Y, Verlinden B, ven Humbeeck J. Scr Mater, 2001; 44: 885
[8] Krizan D, de Cooman B C, Antonissen J. In: Baker M A ed., Int Conf on Advanced High Strength Sheet for Automotive Applications Proceedings, Winter Park, Colorado, 2004: 205
[9] Yin Y Y, Yang W Y, Li L F, Sun Z Q, Wang X T. Acta Metall Sin, 2008; 44: 1299
(尹云洋, 杨王玥,李龙飞, 孙祖庆, 王西涛. 金属学报, 2008; 44: 1299)
[10] Yin Y Y, Yang W Y, Li L F, Sun Z Q, Wang X T. Acta Metall Sin, 2008; 44: 686
(尹云洋, 杨王玥,李龙飞, 孙祖庆, 王西涛. 金属学报, 2008; 44: 686)
[11] Yin Y Y, Yang W Y, Li L F, Sun Z Q, Wang X T. Acta Metall Sin, 2010; 46: 155
(尹云洋, 杨王玥,李龙飞, 孙祖庆, 王西涛. 金属学报, 2010; 46: 155)
[12] Yang W Y, Qi J J, Zun Z Q, Yang P. Acta Metall Sin,2004; 40: 135
(杨王玥,齐俊杰, 孙祖庆, 杨平. 金属学报, 2004; 40: 135)
[13] Dong H, Sun X J. Curr Opin Solid State & Mater Sci, 2005; 9: 269
[14] Matsumura O, Sakuma Y, Takechi H. Trans ISIJ, 1987; 27: 570
[15] Hanlon D N, Sietma J, Van der Zwaag S. ISIJ Int, 2001; 41: 1028
[16] Liu Z Y, Yang Z G, Li Z D, Zhang C, Sheng G. Acta Metall Sin, 2008; 44: 703
(刘志远, 杨志刚, 李昭东, 张 弛, 盛广. 金属学报, 2008; 44: 703)
[17] Yu Y N. Fundamentals of Materials Science. Beijing: Higher Education Press, 2006: 720
(余永宁. 材料科学基础. 北京: 高等教育出版社, 2006: 720)
[18] Kim S K, Shin H C, Chung J H, Chang Y W. Inst Met Mater, 1998; 36: 151

[1] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[6] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[7] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[9] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[10] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[11] 王法, 江河, 董建新. 高合金化GH4151合金复杂析出相演变行为[J]. 金属学报, 2023, 59(6): 787-796.
[12] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[13] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[14] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[15] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.