| 恒位移下BaTiO3单晶在空气中亚临界裂纹扩展与畴变 |
| 赵显武1;褚武扬2;乔利杰2 |
1.北京大学力学与空天技术系; 北京 100871
2.北京科技大学腐蚀与防护中心; 北京 100083 |
|
| SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION |
| ZHAO Xianwu 1;CHU Wuyang 2;QIAO Lijie2 |
1.Department of Mechanics and Aerospace Engineering; Peking University; Beijing 100871
2.Corrosion and Protection Center; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
赵显武 褚武扬 乔利杰. 恒位移下BaTiO3单晶在空气中亚临界裂纹扩展与畴变[J]. 金属学报, 2010, 46(2): 167-171.
,
,
.
SUB–CRITICAL CRACK GROWTH IN AIR AND DOMAIN SWITCHING FOR BaTiO3 SINGLE CRYSTAL UNDER CONSTANT DEFLECTION[J]. Acta Metall Sin, 2010, 46(2): 167-171.
| [1] Zhao X W, Chu W Y, Su Y J, Li J X, Gao K W, Qiao L J. Acta Metall Sin, 2006; 42: 13
(赵显武, 褚武扬, 宿彦京, 李金许, 高克玮, 乔利杰. 金属学报, 2006; 42: 13)
[2] Hao T H, Gong X, Suo Z. J Mech Phys Solids, 1996; 44: 23
[3] Jiang B, Bai Y, Chu W Y, Su Y J, Qiao L J. Appl Phys Lett, 2008; 93: 152905
[4] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102
[5] Yang W, Fang F, Tao M. Int J Solids Struct, 2001; 38: 2203
[6] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207
[7] Fang F, Yang W. Mater Lett, 2002; 57: 198
[8] Kreher W S. J Mech Phys Solids, 2002; 50: 1029
[9] Fang D N, Jiang Y J, Li S, Sun C T. Acta Mater, 2007; 55: 5758
[10] Jiang Y J, Fang D N, Li F X. Appl Phys Lett, 2007; 90: 222907
[11] Wang R M, Chu W Y, Su Y J, Li J X, Qiao L J. Mater Sci Eng, 2006; B135: 141
[12] Fang F, Yang W, Zhang F C. J Am Ceram Soc, 2005; 88:2491
[13] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583
[14] Su Y J, Wang Y, Chu W Y, Gao K W, Qiao L J. Acta Mater, 2004; 52: 3713
[15] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811
[16] Wang Y, Chu W Y, Su Y J, Qiao L J. Mater Sci Eng, 2002; B95: 263
[17] Micjhalske T A, Freiman S W. J Am Ceram Soc, 1983; 66: 284 |
|