| Ce在铁基溶液中分别与Cu,P,Ti相互作用规律的研究 |
| 王跃奎;杜挺 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院16室;高级工程师;北京(100081) |
|
| INTERACTION OF Ce AGAINST Cu, P OR Ti IN Fe-BASE SOLUTION |
| WANG Yuekui;DU Ting Central Iron and Steel Rasearch Institute; Ministry of Metallurgical Industry; Beijing professor;Department No.16;Central Iron and Steel Research Institute; Ministry of Metallurgical Industry;Beijing 100081 |
引用本文:
王跃奎;杜挺. Ce在铁基溶液中分别与Cu,P,Ti相互作用规律的研究[J]. 金属学报, 1990, 26(3): 150-152.
,
.
INTERACTION OF Ce AGAINST Cu, P OR Ti IN Fe-BASE SOLUTION[J]. Acta Metall Sin, 1990, 26(3): 150-152.
1 周谦莉,杜挺.金属学报,1989;25:B11 2 Gschneidner K K Jr., Verkade M E. Selected Cerium Phase Diagrams, IS-RIC-7, Ames, Iowa: Iowa State University, 1974: 17 3 乐可襄,杜挺,李继宗,沈汝美.金属学报,1987;23:A99 4 Wu Yieming, Wang Longmei, Du Ting. J Less Common Met, 1985; 110: 187 5 Sigworth G K, Elliott J F. Met Sci, 1974: 8: 298 6 韩其勇.北京钢铁学院学报,1986;3:115 7 王常珍,王福珍,杜英敏,张小平.金属学报,1980;16:83 8 韩其勇,项长祥,董元篪,杨斯馥.钢铁,1984;19(7) :9 9 周谦莉,杜挺.钢铁研究总院学报,1988;8:55 10 唱鹤鸣,杜挺,余景生.钢铁研究总院学报,1988;8:93 11 唱鹤鸣,杜挺,余景生.金属学报,1989;25:B140K |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|