| Fe-P与Fe-P-Ce合金中的晶界磷偏聚及其对脆性的影响 |
| 张东彬;吴承建;杨让 |
| 北京科技大学材料科学与工程系;讲师北京(100083);北京科技大学;北京科技大学 |
|
| GRAIN BOUNDARY SEGREGATION OF P IN Fe-P AND Fe-P-Ce ALLOYS AND EFFECT ON THEIR BRITTLENESS |
| ZHANG Dongbin;WU Chengjian;YANG Rang University of Sciencs and Technology Beijing |
引用本文:
张东彬;吴承建;杨让. Fe-P与Fe-P-Ce合金中的晶界磷偏聚及其对脆性的影响[J]. 金属学报, 1991, 27(2): 33-36.
,
,
.
GRAIN BOUNDARY SEGREGATION OF P IN Fe-P AND Fe-P-Ce ALLOYS AND EFFECT ON THEIR BRITTLENESS[J]. Acta Metall Sin, 1991, 27(2): 33-36.
1 Grabke H J. ISIJ Int, 1989; 29: 529 2 Ohtani H, Feng H C, McMahon C J Jr. Metall Trans, 1976; 7A: 1123 3 Wagner C D, Riggs W M, Davis L E, Moulder J F, Muilenberg G E, Handbook of X-Ray Photoelectron Spectroscopy, Perkin-Elmer Corp, Eden Prairie, 1979 4 Guttmann M, McLean D. In: Johnson W C, Blakely J M eds., Interfacial Segregation, Metals Park, Ohio: ASM, 1979: 261 5 张东彬,吴承建.金属学报,1988;24:A100 6 安彦兼次,铃木茂,木村宏.铁钢,1983;69:625 7 Losch W. Acta Metall, 1979; 27: 1885 8 Zhang Dongbin, Wu Chengjian, Yang Rang. Mater Sci Eng, 1991; A131:93 9 Briant C L, Messmer R P. Acta Metall, 1984; 32: 2043 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|