| Mn,B复合合金化对Ni_3Al室温塑性的影响 |
| 杨文英;吕反修;章守华 |
| 北京科技大学材料系;副教授;北京(100083);北京科技大学;北京科技大学 |
|
| AN ATTEMPT TO IMPROVE AMBIENT DUCTILITY OF Ni_3Al BY COMPLEX ALLOYING WITH Mn AND B |
| YANG Wenying;LU Fanxiu;ZHANG Shouhua University of Science and Techhology Beijing |
引用本文:
杨文英;吕反修;章守华. Mn,B复合合金化对Ni_3Al室温塑性的影响[J]. 金属学报, 1993, 29(1): 39-42.
,
,
.
AN ATTEMPT TO IMPROVE AMBIENT DUCTILITY OF Ni_3Al BY COMPLEX ALLOYING WITH Mn AND B[J]. Acta Metall Sin, 1993, 29(1): 39-42.
1 Baker I, Ichishita F S, Shulson E M. In: Kear B H, Giessen B C eds., Rapidly Solidified Metastable Materials. Amsterdam: North-Holland, 1984: 395 2 青木清,和泉修.日本金属学会志,1979;43:358 3 Inoue A, Masumotc T, Tomioko H, Yano N. Int J Rapid Solidi, 1984/1985; 1: 15 4 Liu C T, White C L, Horton J A. Acta Metall, 1985; 33: 213 5 杨文英,吕反修,章守华.金属学报,1990;26:A385 6 杨文英.北京科技大学博士学位论文,1988S |
|