| C_F/Al复合材料界面质量控制研究 |
| 王玉庆;唐凤军;郑久红;周本濂 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院国际材料物理中心 |
|
| BETTERMENT ON INTERFACE OF C_F/Al COMPOSITES |
| WANG Yuqing; TANG Fengjun; ZHENG Jiuhong(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015); ZHOU Benlian(Institute of Metal Research; International Centre for Materials Phisics; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 94-03-11;in revised form 94-06-01) |
引用本文:
王玉庆;唐凤军;郑久红;周本濂. C_F/Al复合材料界面质量控制研究[J]. 金属学报, 1995, 31(14): 86-90.
,
,
,
.
BETTERMENT ON INTERFACE OF C_F/Al COMPOSITES[J]. Acta Metall Sin, 1995, 31(14): 86-90.
| 1CoorCR,YunDI,HuntJrWH.inFishmanSGed.,CastReinforcedMetalComposites,ASM,1988:1952ZhangGD,ZhangWD.ProceedofICCM//Ⅷ,USA,Hawsaii,1991:19H3张国定.航空学报,1991;12:B5704WangYuping,ZhouBenlian,WangZouming,ShiChangxu,JMaterSciTechnol,1993;97:75 王玉庆,郑久红,周本濂.金属学报,1994;30:B1946 王玉庆,王作明,刘 敏,周本濂,师昌绪.复合材料学报,1992;9:137 RocherJP,QuenissetJM,NaslainR.JMaterSciLetter,1985;4:1527 |
|