| Ti-Ni-Si纳米合金的制备和特性 |
| 平德海;谢天生;金志雄;李斗星;叶恒强 |
| 中国科学院金属研究所固体原子像开放研究实验室 |
|
| PREPARATION AND PROPERTIES OF NANOCRYSTALLINE Ti_(70)Ni_(20)Si_(10) ALLOY |
| PING Dehai; (Laborutory of Atornic Imaging of Solids; Inslitute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) XIE Miansheng; JIN Zhixiong; LI Douxing; YE HenKqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Cthinese Academy of Sciences; Shenyang 110015) |
引用本文:
平德海;谢天生;金志雄;李斗星;叶恒强. Ti-Ni-Si纳米合金的制备和特性[J]. 金属学报, 1995, 31(17): 200-205.
,
,
,
,
.
PREPARATION AND PROPERTIES OF NANOCRYSTALLINE Ti_(70)Ni_(20)Si_(10) ALLOY[J]. Acta Metall Sin, 1995, 31(17): 200-205.
| 1BirringerR,GleiterH,KleinHP,MarquardtP.PhysLett,1984;A102:3652GleiterH.ProgMaterSci,1989;33:2233LuK,WangJT,WeiWD.JApplPhys,1991;69:5224NicolausMM,SinningH-R,HaessnerF.MaterSciEng,1992;A150:1015YshizawaY,OgumaS,YamauchiK.JApplPhys,1988;64:60646HerzerG.IEEETransMaRn,1989;25:33277LiuXD,WangJT,PingDH,LiDX.JApplPhys,1993;74:45018PingDH,LiDX,YeHQ,LiuXD,HuZQ.MaterSciEngA,1995;inpress9SiegelRW.MaterResSocBull,1990;15:6010吴希俊.力学进展,1991;21:6311UerrU,JingJ,GonserU,GleiterH.SolidStateCommun,1990;76:19712SchaeferHE,WurschumR,BirringerR,GleiterH.JLess-CommonMet,1988;140:16113SiegelRW.NanostrMaler,1993;3:114SuryanarayanaC.IntMaterRev,1995;inpress15BuchwitzM,Adlwarth-DieballR,RyderPL.ActaMetallMater,1993;41:188516NiehTG,WadsworthJ.ScrMetallMater,1991;25:95517El-Sherik,ErbU,PaumboG,AustKT.ScrMetallMater,1992;27:18518SuryanarayanaC,MukhopadhyayD,PatankarSN,FroesFH.JMaterRes,1992;7:2114Z |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|