| 部分非晶态Fe_(33)Zr_(67)合金条带的表观晶化动力学 |
| 孙年祥;刘学东;李淑苓;丁炳哲;卢柯 |
| 中国科学院金属研究所快速凝固非平衡合金国家重点实验室 |
|
| APPARENT CRYSTALLIZATION KINETICS OF PARTIALLY AMORPHOUS Fe_(33)Zr_(67), ALLOYS |
| SUN Nianxiang; (Institute of Metal Research; Chinese Academy of Sciences Shenyang 110015) LIU Xuedong; LI Shuling; DING Bingzhe; LU Ke(Institute of Metal Research; Chinese A cademy of Sciences; Shenyang 110015) |
引用本文:
孙年祥;刘学东;李淑苓;丁炳哲;卢柯. 部分非晶态Fe_(33)Zr_(67)合金条带的表观晶化动力学[J]. 金属学报, 1995, 31(17): 206-211.
,
,
,
,
.
APPARENT CRYSTALLIZATION KINETICS OF PARTIALLY AMORPHOUS Fe_(33)Zr_(67), ALLOYS[J]. Acta Metall Sin, 1995, 31(17): 206-211.
| 1ChristainJW.TheTheoryofTransformationinMetalsandAlloys,lsted.,Oxford:PergamonPress,19652HolzerJC.KeltonKF.ActaMetallMaler.1991;39:18333KissingerHE.AnalChem,1957;29:17024CalkaA.RadlinskiAP.MaterResSocSympProc,1987;80:2035RanganathanS.JMaterSci,1981;16:24016SpassovT.KosterU.JMaterSci1993;28:2789 |
|