| 跨尺度协同增强铝基复合材料研究进展 |
欧阳求保, 苏楠, 王瑞安, 刘侃, 张荻( ) |
| 上海交通大学 材料科学与工程学院 金属基复合材料全国重点实验室 上海 200240 |
|
| Research Progress on Cross-Scale Synergistically Reinforced Aluminum Matrix Composites |
OUYANG Qiubao, SU Nan, WANG Ruian, LIU Kan, ZHANG Di( ) |
| National Key Laboratory of Metal Matrix Composites, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China |
引用本文:
欧阳求保, 苏楠, 王瑞安, 刘侃, 张荻. 跨尺度协同增强铝基复合材料研究进展[J]. 金属学报, 2026, 62(5): 733-742.
Qiubao OUYANG,
Nan SU,
Ruian WANG,
Kan LIU,
Di ZHANG.
Research Progress on Cross-Scale Synergistically Reinforced Aluminum Matrix Composites[J]. Acta Metall Sin, 2026, 62(5): 733-742.
| [1] |
Wang X S, Wang X Z, Liu K, et al. Effect of the CNTs into SiCp-Al interfacial micro-zones on ageing precipitation behavior, microstructure and mechanical properties of SiCp(CNT)/Al-Zn-Mg-Cu composites [J]. Composites, 2023, 259B: 110708
|
| [2] |
Li S S, Su Y S, Zhu X H, et al. Enhanced mechanical behavior and fabrication of silicon carbide particles covered by in-situ carbon nanotube reinforced 6061 aluminum matrix composites [J]. Mater. Des., 2016, 107: 130
doi: 10.1016/j.matdes.2016.06.021
|
| [3] |
Guan L C R, Cao H, Su Y, et al. Enhanced strength-ductility synergy of SiC particles reinforced aluminum matrix composite via dual configuration design of reinforcement and matrix [J]. Mater. Des., 2024, 245: 113186
doi: 10.1016/j.matdes.2024.113186
|
| [4] |
Ma Z Y, Xiao B L, Zhang J F, et al. Overview of research and development for aluminum matrix composites driven by aerospace equipment demand [J]. Acta Metall. Sin., 2023, 59: 457
doi: 10.11900/0412.1961.2022.00605
|
| [4] |
马宗义, 肖伯律, 张峻凡 等. 航天装备牵引下的铝基复合材料研究进展与展望 [J]. 金属学报, 2023, 59: 457
doi: 10.11900/0412.1961.2022.00605
|
| [5] |
Wu Z Y, Shao H F, Cai C C, et al. Tensile and fracture behaviors of stitched twill carbon fabric structure reinforced aluminum matrix composites at elevated temperature [J]. Acta Metall. Sin., 2025, 61: 1387
doi: 10.11900/0412.1961.2023.00469
|
| [5] |
吴志勇, 邵徽凡, 蔡长春 等. 斜纹碳布缝合织物结构增强铝基复合材料的高温拉伸及断裂行为 [J]. 金属学报, 2025, 61: 1387
doi: 10.11900/0412.1961.2023.00469
|
| [6] |
Cai Y P, Su Y S, Liu K, et al. Effect of Sc microalloying on fabrication, microstructure and mechanical properties of SiCp/Al-Cu-Mg-Sc composites via powder metallurgy [J]. Mater. Sci. Eng., 2023, A877: 145152
|
| [7] |
Hua A D, Su Y S, Cai Y P, et al. Fabrication, microstructure characterization and mechanical properties of B4C microparticles and SiC nanowires hybrid reinforced aluminum matrix composites [J]. Mater. Charact., 2022, 193: 112243
doi: 10.1016/j.matchar.2022.112243
|
| [8] |
Zhang Z M, Fan G L, Tan Z Q, et al. Towards the strength-ductility synergy of Al2O3/Al composite through the design of roughened interface [J]. Composites, 2021, 224B: 109251
|
| [9] |
Liu K, Su Y S, Wang X Z, et al. Achieving simultaneous enhancement of strength and ductility in Al matrix composites by employing the synergetic strengthening effect of micro- and nano-SiCps [J]. Composites, 2023, 248B: 110350
|
| [10] |
Wang X S, Su Y S, Qiu C H, et al. Mechanical behavior and interfacial micro-zones of SiCp(CNT) hybrid reinforced aluminum matrix composites [J]. Mater. Charact., 2022, 189: 111982
doi: 10.1016/j.matchar.2022.111982
|
| [11] |
Ma Y, Chen H, Zhang M X, et al. Break through the strength-ductility trade-off dilemma in aluminum matrix composites via precipitation-assisted interface tailoring [J]. Acta Mater., 2023, 242: 118470
doi: 10.1016/j.actamat.2022.118470
|
| [12] |
Yi C L, Chen X M, Gou F L, et al. Direct measurements of the mechanical strength of carbon nanotube-aluminum interfaces [J]. Carbon, 2017, 125: 93
doi: 10.1016/j.carbon.2017.09.020
|
| [13] |
Zhou T, Lei M, Xu J. Recent progress in the development and properties of aluminum matrix composites reinforced with graphene: A review [J]. Mater. Today Sustain., 2024, 25: 100674
|
| [14] |
Zhang X, Li S F, Pan B, et al. A novel strengthening effect of in-situ nano Al2O3w on CNTs reinforced aluminum matrix nanocomposites and the matched strengthening mechanisms [J]. J. Alloys Compd., 2018, 764: 279
doi: 10.1016/j.jallcom.2018.06.006
|
| [15] |
He H Y, Fan G L, Saba F, et al. Enhanced distribution and mechanical properties of high content nanoparticles reinforced metal matrix composite prepared by flake dispersion [J]. Composites, 2023, 252B: 110514
|
| [16] |
Bakshi S R, Lahiri D, Agarwal A. Carbon nanotube reinforced metal matrix composites—A review [J]. Int. Mater. Rev., 2010, 55: 41
doi: 10.1179/095066009X12572530170543
|
| [17] |
Jiang L, Li Z Q, Fan G L, et al. Strong and ductile carbon nanotube/aluminum bulk nanolaminated composites with two-dimensional alignment of carbon nanotubes [J]. Scr. Mater., 2012, 66: 331
doi: 10.1016/j.scriptamat.2011.11.023
|
| [18] |
Li S S, Su Y S, Ouyang Q B, et al. In-situ carbon nanotube-covered silicon carbide particle reinforced aluminum matrix composites fabricated by powder metallurgy [J]. Mater. Lett., 2016, 167: 118
doi: 10.1016/j.matlet.2015.12.155
|
| [19] |
Li S S, Su Y S, Jin H L, et al. Effects of carbon nanotube content on morphology of SiCp(CNT) hybrid reinforcement and tensile mechanical properties of SiCp(CNT)/Al composites [J]. J. Mater. Res., 2017, 32: 1239
doi: 10.1557/jmr.2017.12
|
| [20] |
Liu K, Cui Q F, Shi L, et al. Tuning lamella spacings for simultaneous strength-ductility improvements in heterogeneous lamella SiCp/2024Al composites [J]. Mater. Des., 2025, 249: 113510
doi: 10.1016/j.matdes.2024.113510
|
| [21] |
Cao L, Chen B, Jia Z D, et al. Research progress and aerospace applications of aluminum matrix composite [J]. Foundry Technol., 2023, 44: 685
|
| [21] |
曹 遴, 陈 彪, 贾振东 等. 铝基复合材料研究进展及其航空航天应用 [J]. 铸造技术, 2023, 44: 685
|
| [22] |
Li P Y. Research progress in high-performance aluminum matrix composites [J]. J. Mater. Eng, 2023, 51(4): 67
doi: 10.11868/j.issn.1001-4381.2021.000255
|
| [22] |
李沛勇. 高性能铝基复合材料研究进展 [J]. 材料工程, 2023, 51(4): 67
doi: 10.11868/j.issn.1001-4381.2021.000255
|
| [23] |
Ye X P, Li Y L, Weng J D, et al. Research status on strengthening mechanism of particle-reinforced metal matrix composites [J]. J. Mater. Eng., 2018, 46(12): 28
|
| [23] |
叶想平, 李英雷, 翁继东 等. 颗粒增强金属基复合材料的强化机理研究现状 [J]. 材料工程, 2018, 46(12): 28
doi: 10.11868/j.issn.1001-4381.2016.001214
|
| [24] |
Ma G N, Zhu S Z, Wang D, et al. Aging behaviors and mechanical properties of SiC/Al-Zn-Mg-Cu Composites [J]. Acta Metall. Sin., 2023, 59: 1655
|
| [24] |
马国楠, 朱士泽, 王 东 等. SiC颗粒增强Al-Zn-Mg-Cu复合材料的时效行为和力学性能 [J]. 金属学报, 2023, 59: 1655
doi: 10.11900/0412.1961.2021.00473
|
| [25] |
Sun T T, Wang H Z, Wu Y, et al. Effect of in situ 2%TiB2 particles on microstructure and mechanical properties of 2024Al additive manufacturing alloy [J]. Acta Metall. Sin., 2023, 59: 169
|
| [25] |
孙腾腾, 王洪泽, 吴 一 等. 原位自生2%TiB2颗粒对2024Al增材制造合金组织和力学性能的影响 [J]. 金属学报, 2023, 59: 169
doi: 10.11900/0412.1961.2022.00410
|
| [26] |
Nie J F, Wu Y L, Xie K W, et al. Microstructure and thermal stability of heterostructured Al-AlN nanocomposite [J]. Acta Metall. Sin., 2022, 58: 1497
doi: 10.11900/0412.1961.2022.00305
|
| [26] |
聂金凤, 伍玉立, 谢可伟 等. Al-AlN异构纳米复合材料的组织构型与热稳定性 [J]. 金属学报, 2022, 58: 1497
doi: 10.11900/0412.1961.2022.00305
|
| [27] |
Jiang Z H, Qiu W T, Gong S, et al. Preparation and properties of lightweight HfO2@CNT/polymer/CuAlMn composite with high strength and high damping [J]. Acta Metall. Sin., 2024, 60: 287
|
| [27] |
蒋招汉, 邱文婷, 龚 深 等. 轻质高强高阻尼HfO2@CNT/聚合物/CuAlMn复合材料的制备及性能 [J]. 金属学报, 2024, 60: 287
doi: 10.11900/0412.1961.2022.00210
|
| [28] |
Senthilraj K, Rajamurugan G. Influence of Al2TiO5 particles on AA6061 composites fabricated by bottom pouring stir casting technique [J]. Mater. Lett., 2023, 338: 134085
doi: 10.1016/j.matlet.2023.134085
|
| [29] |
Cui S, Shao G S, Zhang K, et al. Microstructure and mechanical properties of graphene reinforced Al-matrix composites prepared by stirring casting [J]. Nonferrous Met. Mater. Eng., 2022, 43(2): 19
|
| [29] |
崔 松, 邵国森, 张 柯 等. 搅拌铸造法制备石墨烯增强铝基复合材料的组织和力学性能研究 [J]. 有色金属材料与工程, 2022, 43(2): 19
|
| [30] |
Bai Y L, Zhang Z F, Fan J Z, et al. Preparation of particle reinforced aluminum matrix composites by semi-solid stirring [J]. Spec. Cast. Nonferrous Alloys, 2021, 41: 402
|
| [30] |
白月龙, 张志峰, 樊建中 等. 半固态搅拌制备颗粒增强铝基复合材料 [J]. 特种铸造及有色合金, 2021, 41: 402
doi: 10.15980/j.tzzz.2021.04.002
|
| [31] |
El-Sabbagh A M, Soliman M, Taha M A, et al. Effect of rolling and heat treatment on tensile behaviour of wrought Al-SiCp composites prepared by stir-casting [J]. J. Mater. Process. Technol., 2013, 213: 1669
doi: 10.1016/j.jmatprotec.2013.04.013
|
| [32] |
Samal P, Vundavilli P R, Meher A, et al. Recent progress in aluminum metal matrix composites: A review on processing, mechanical and wear properties [J]. J. Manuf. Process., 2020, 59: 131
doi: 10.1016/j.jmapro.2020.09.010
|
| [33] |
Yang W S, Zhao Q Q, Xin L, et al. Microstructure and mechanical properties of graphene nanoplates reinforced pure Al matrix composites prepared by pressure infiltration method [J]. J. Alloys Compd., 2018, 732: 748
doi: 10.1016/j.jallcom.2017.10.283
|
| [34] |
Ma G J, Ding Y T, Jin P P, et al. Research on powder metallurgy processing for preparing Al matrix composites [J]. Mater. Rep., 2013, 27(15): 149
|
| [34] |
马国俊, 丁雨田, 金培鹏 等. 粉末冶金法制备铝基复合材料的研究 [J]. 材料导报, 2013, 27(15): 149
|
| [35] |
Liu R X, Wu C D, Zhang J, et al. Microstructure and mechanical behaviors of the ultrafine grained AA7075/B4C composites synthesized via one-step consolidation [J]. J. Alloys Compd., 2018, 748: 737
doi: 10.1016/j.jallcom.2018.03.152
|
| [36] |
Bi J, Lei Z L, Chen Y B, et al. Microstructure and mechanical properties of a novel Sc and Zr modified 7075 aluminum alloy prepared by selective laser melting [J]. Mater. Sci. Eng., 2019, A768: 138478
|
| [37] |
Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys [J]. Nature, 2017, 549: 365
doi: 10.1038/nature23894
|
| [38] |
Fan J L, Han Y, Li P F, et al. Micro/Nano composited tungsten material and its high thermal loading behavior [J]. J. Nucl. Mater., 2014, 455: 717
doi: 10.1016/j.jnucmat.2014.09.037
|
| [39] |
Jiang L, Ma K K, Yang H, et al. The microstructural design of trimodal aluminum composites [J]. JOM, 2014, 66: 898
doi: 10.1007/s11837-014-0906-2
|
| [40] |
Jiang L, Yang H, Yee J K, et al. Toughening of aluminum matrix nanocomposites via spatial arrays of boron carbide spherical nanoparticles [J]. Acta Mater., 2016, 103: 128
doi: 10.1016/j.actamat.2015.09.057
|
| [41] |
Zhang Z M, Fan G L, Tan Z Q, et al. Bioinspired multiscale Al2O3-rGO/Al laminated composites with superior mechanical properties [J]. Composites, 2021, 217B: 108916
|
| [42] |
Wang X, Jiang X S, Sun H L, et al. Microstructures and mechanical properties of Al nanocomposites hybrid-reinforced with B4C, carbon nanotubes and graphene nanoplatelets [J]. Mater. Sci. Eng., 2023, B293: 116457
|
| [43] |
Şenel M C, Gürbüz M, Koç E. Fabrication and characterization of synergistic Al-SiC-GNPs hybrid composites [J]. Composites, 2018, 154B: 1
|
| [44] |
Wang X, Jiang X S, Sun H L, et al. Microstructure and mechanical properties of bioinspired laminated Al matrix hybrid reinforced with B4C and graphene nanoplatelets [J]. Mater. Charact., 2022, 193: 112307
doi: 10.1016/j.matchar.2022.112307
|
| [45] |
Herzallah H, Elsayd A, Shash A, et al. Effect of carbon nanotubes (CNTs) and silicon carbide (SiC) on mechanical properties of pure Al manufactured by powder metallurgy [J]. J. Mater. Res. Technol., 2020, 9: 1948
doi: 10.1016/j.jmrt.2019.12.027
|
| [46] |
Van Trinh P, Lee J, Kang B, et al. Mechanical and wear properties of SiCp/CNT/Al6061 hybrid metal matrix composites [J]. Diam. Relat. Mater., 2022, 124: 108952
doi: 10.1016/j.diamond.2022.108952
|
| [47] |
Guo B S, Zhang X M, Cen X, et al. Ameliorated mechanical and thermal properties of SiC reinforced Al matrix composites through hybridizing carbon nanotubes [J]. Mater. Charact., 2018, 136: 272
doi: 10.1016/j.matchar.2017.12.032
|
| [48] |
Qiu F, Tong H T, Gao Y Y, et al. Microstructures and compressive properties of Al matrix composites reinforced with bimodal hybrid in-situ nano-/micro-sized TiC particles [J]. Materials, 2018, 11: 1284
doi: 10.3390/ma11081284
|
| [49] |
David Raja Selvam J, Dinaharan I, Vibin Philip S, et al. Microstructure and mechanical characterization of in situ synthesized AA6061/(TiB2 + Al2O3) hybrid aluminum matrix composites [J]. J. Alloys Compd., 2018, 740: 529
doi: 10.1016/j.jallcom.2018.01.016
|
| [50] |
Li S S. Prepare SiCp (in situ CNT) reinforced aluminum matrix composites and study on its properties [D]. Shanghai: Shanghai Jiao Tong University, 2017
|
| [50] |
李士胜. 碳化硅颗粒原位自生碳纳米管增强铝基复合材料的制备与性能研究 [D]. 上海: 上海交通大学, 2017
|
| [51] |
Liu Z Y, Xiao B L, Wang W G, et al. Modelling of carbon nanotube dispersion and strengthening mechanisms in Al matrix composites prepared by high energy ball milling-powder metallurgy method [J]. Composites, 2017, 94A: 189
|
| [52] |
Cao L, Chen B, Wan J, et al. Unraveling the dispersion mechanism of carbon nanotubes in aluminum powder particles during high energy ball milling by FIB-TEM study [J]. Powder Technol., 2023, 419: 118339
doi: 10.1016/j.powtec.2023.118339
|
| [53] |
Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59
doi: 10.11900/0412.1961.2018.00461
|
| [53] |
肖伯律, 黄治冶, 马 凯 等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59
doi: 10.11900/0412.1961.2018.00461
|
| [54] |
Zhao N Q, Liu X H, Pu B W. Progress on multi-dimensional carbon nanomaterials reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin., 2019, 55: 1
doi: 10.11900/0412.1961.2018.00456
|
| [54] |
赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展 [J]. 金属学报, 2019, 55: 1
doi: 10.11900/0412.1961.2018.00456
|
| [55] |
Oh S I, Lim J Y, Kim Y C, et al. Fabrication of carbon nanofiber reinforced aluminum alloy nanocomposites by a liquid process [J]. J. Alloys Compd., 2012, 542: 111
doi: 10.1016/j.jallcom.2012.07.029
|
| [56] |
Ding H, Cui X P, Xu C S, et al. Fabrication and mechanical characteristics of multi-laminated aluminum matrix composites reinforced by continuous basalt fibers [J]. Acta Metall. Sin., 2018, 54: 1171
|
| [56] |
丁 浩, 崔喜平, 许长寿 等. 连续玄武岩纤维增强铝基层状复合材料的制备与力学特性 [J]. 金属学报, 2018, 54: 1171
|
| [57] |
Sharma A, Narsimhachary D, Sharma V M, et al. Surface modification of Al6061-SiC surface composite through impregnation of graphene, graphite & carbon nanotubes via FSP: A tribological study [J]. Surf. Coat. Technol., 2019, 368: 175
doi: 10.1016/j.surfcoat.2019.04.001
|
| [58] |
Geng K, Li S F, Yang Y F, et al. 3D printing of Al matrix composites through in situ impregnation of carbon nanotubes on Al powder [J]. Carbon, 2020, 162: 465
doi: 10.1016/j.carbon.2020.02.087
|
| [59] |
Zhu Z G, Hu Z H, Seet H L, et al. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: Microstructure, properties, and applications [J]. Int. J. Mach. Tools Manuf., 2023, 190: 104047
doi: 10.1016/j.ijmachtools.2023.104047
|
| [60] |
Aikin R M, Christodoulou L. The role of equiaxed particles on the yield stress of composites [J]. Scr. Metall. Mater., 1991, 25: 9
doi: 10.1016/0956-716X(91)90345-2
|
| [61] |
Le Roy G, Embury J D, Edwards G, et al. A model of ductile fracture based on the nucleation and growth of voids [J]. Acta Metall., 1981, 29: 1509
doi: 10.1016/0001-6160(81)90185-1
|
| [62] |
Ryu H J, Cha S I, Hong S H. Generalized shear-lag model for load transfer in SiC/Al metal-matrix composites [J]. J. Mater. Res., 2003, 18: 2851
doi: 10.1557/JMR.2003.0398
|
| [63] |
Hansen N. Hall-Petch relation and boundary strengthening [J]. Scr. Mater., 2004, 51: 801
doi: 10.1016/j.scriptamat.2004.06.002
|
| [64] |
Liu K, Cui Q F, Shi L, et al. Grain structure tailoring strategy for heterogeneous lamella SiCp/2024Al composites with exceptional strength-ductility synergy [J]. Composites, 2024, 280B: 111491
|
| [65] |
Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties [J]. Mater. Res. Lett., 2017, 5: 527
doi: 10.1080/21663831.2017.1343208
|
| [66] |
Han Q H, Asgari A, Hodgson P D, et al. Strain partitioning in dual-phase steels containing tempered martensite [J]. Mater. Sci. Eng., 2014, A611: 90
|
| [67] |
Zhu Y T, Wu X L. Perspective on hetero-deformation induced (HDI) hardening and back stress [J]. Mater. Res. Lett., 2019, 7: 393
doi: 10.1080/21663831.2019.1616331
|
| [68] |
Wang G, Ouyang H, Su Y S, et al. Heterostructured bulk aluminum with controllable gradient structure: Fabrication strategy and deformation mechanisms [J]. Scr. Mater., 2021, 196: 113762
doi: 10.1016/j.scriptamat.2021.113762
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|