| Ag替换Cu对Zr-Ti-Cu-Al非晶合金性能的影响 |
蔡正清1, 尹大伟1, 杨靓1, 王文祥1, 王飞龙1,2, 温永清1,3, 马明臻1( ) |
1 燕山大学 亚稳材料制备技术与科学国家重点实验室 秦皇岛 066004 2 南京钢铁股份有限公司 南京 210000 3 包头稀土研究院 包头 014010 |
|
| Effect of Ag Substitution of Cu on Properties of Zr-Ti-Cu-Al Amorphous Alloys |
CAI Zhengqing1, YIN Dawei1, YANG Liang1, WANG Wenxiang1, WANG Feilong1,2, WEN Yongqing1,3, MA Mingzhen1( ) |
1 State Key Laboratory of Metastable Materials Preparation Technology and Science, Yanshan University, Qinhuangdao 066004, China 2 Nanjing Iron and Steel Co. Ltd., Nanjing 210000, China 3 Baotou Rare Earth Research Institute, Baotou 014010, China |
引用本文:
蔡正清, 尹大伟, 杨靓, 王文祥, 王飞龙, 温永清, 马明臻. Ag替换Cu对Zr-Ti-Cu-Al非晶合金性能的影响[J]. 金属学报, 2025, 61(4): 572-582.
Zhengqing CAI,
Dawei YIN,
Liang YANG,
Wenxiang WANG,
Feilong WANG,
Yongqing WEN,
Mingzhen MA.
Effect of Ag Substitution of Cu on Properties of Zr-Ti-Cu-Al Amorphous Alloys[J]. Acta Metall Sin, 2025, 61(4): 572-582.
| 1 |
El-Eskandarany M S, Ali N, Saeed M. Glass-forming ability and soft magnetic properties of (Co75Ti25)100 - x Fe x (x; 0-20 at.%) systems fabricated by SPS of mechanically alloyed nanopowders [J]. Nanomaterials, 2020, 10: 849
|
| 2 |
Zhang C, Li N, Pan J, et al. Enhancement of glass-forming ability and bio-corrosion resistance of Zr-Co-Al bulk metallic glasses by the addition of Ag [J]. J. Alloys Compd., 2010, 504: S163
|
| 3 |
Chang C T, Shen B L, Inoue A. FeNi-based bulk glassy alloys with superhigh mechanical strength and excellent soft-magnetic properties [J]. Appl. Phys. Lett., 2006, 89: 051912
|
| 4 |
Schroers J. Processing of bulk metallic glass [J]. Adv. Mater., 2010, 22: 1566
|
| 5 |
Inoue A, Takeuchi A. Recent development and application products of bulk glassy alloys [J]. Acta Mater., 2011, 59: 2243
|
| 6 |
Peker A, Johnson W L. A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 [J]. Appl. Phys. Lett., 1993, 63: 2342
|
| 7 |
Inoue A, Zhang T. Fabrication of bulk glassy Zr55Al10Ni5Cu30 alloy of 30 mm in diameter by a suction casting method [J]. Mater. Trans. JIM, 1996, 37: 185
|
| 8 |
Inoue A, Gook J S. Fe-based ferromagnetic glassy alloys with wide supercooled liquid region [J]. Mater. Trans. JIM, 1995, 36: 1180
|
| 9 |
Inoue A, Shinohara Y, Gook J S. Thermal and magnetic properties of bulk Fe-based glassy alloys prepared by copper mold casting [J]. Mater. Trans. JIM, 1995, 36: 1427
|
| 10 |
Inoue A, Nishiyama N, Kimura H. Preparation and thermal stability of bulk amorphous Pd40Cu30Ni10P20 alloy cylinder of 72 mm in diameter [J]. Mater. Trans. JIM, 2007, 38: 179
|
| 11 |
He Y, Schwarz R B, Archuleta J I. Bulk glass formation in the Pd-Ni-P system [J]. Appl. Phys. Lett., 1996, 69: 1861
|
| 12 |
Shen Y, Ma E, Xu J. A group of Cu(Zr)-based BMGs with critical diameter in the range of 12 to 18 mm [J]. J. Mater. Sci. Technol., 2008, 24: 149
|
| 13 |
Zhang Q S, Zhang W, Inoue A. New Cu-Zr-based bulk metallic glasses with large diameters of up to 1.5 cm [J]. Scr. Mater., 2006, 55: 711
|
| 14 |
Inoue A, Ohtera K, Kita K, et al. New amorphous Mg-Ce-Ni alloys with high strength and good ductility [J]. Jpn. J. Appl. Phys., 1988, 27: L2248
|
| 15 |
Inoue A, Nishiyama N, Amiya K, et al. Al-La-Ni amorphous alloys with a wide supercooled liquid region [J]. Mater. Trans. JIM, 1989, 30: 965
|
| 16 |
Shi H Q, Zhao W B, Wei X W, et al. Effect of Ti addition on mechanical properties and corrosion resistance of Ni-free Zr-based bulk metallic glasses for potential biomedical applications [J]. J. Alloys Compd., 2020, 815: 152636
|
| 17 |
Hua N B, Li R, Wang H, et al. Formation and mechanical properties of Ni-free Zr-based bulk metallic glasses [J]. J. Alloys Compd., 2011, 509(): S175
|
| 18 |
Wataha J C, Lockwood P E, Schedle A. Effect of silver, copper, mercury, and nickel ions on cellular proliferation during extended, low‐dose exposures [J]. J. Biomed. Mater. Res., 2000, 52: 360
|
| 19 |
Jin Z S, Yang Y J, Zhang Z P, et al. Effect of Hf substitution Cu on glass-forming ability, mechanical properties and corrosion resistance of Ni-free Zr-Ti-Cu-Al bulk metallic glasses [J]. J. Alloys Compd., 2019, 806: 668
|
| 20 |
Zhang W, Jia F, Zhang Q S, et al. Effects of additional Ag on the thermal stability and glass-forming ability of Cu-Zr binary glassy alloys [J]. Mater. Sci. Eng., 2007, 459A: 330
|
| 21 |
Hua N B, Pang S J, Li Y, et al. Ni- and Cu-free Zr-Al-Co-Ag bulk metallic glasses with superior glass-forming ability [J]. J. Mater. Res., 2011, 26: 539
|
| 22 |
Saini S, Srivastava A P, Neogy S. The effect of Ag addition on the crystallization kinetics and glass forming ability of Zr-(CuAg)-Al bulk metallic glass [J]. J. Alloys Compd., 2019, 772: 961
|
| 23 |
Hua N B, Zhang T. Glass-forming ability, crystallization kinetics, mechanical property, and corrosion behavior of Zr-Al-Ni-Ag glassy alloys [J]. J. Alloys Compd., 2014, 602: 339
|
| 24 |
Yang Y J, Cheng B Y, Lv J W, et al. Effect of Ag substitution for Ti on glass-forming ability, thermal stability and mechanical properties of Zr-based bulk metallic glasses [J]. Mater. Sci. Eng., 2019, A746: 229
|
| 25 |
Wan Y Z, Raman S, He F, et al. Surface modification of medical metals by ion implantation of silver and copper [J]. Vacuum, 2007, 81: 1114
|
| 26 |
Lu Z P, Bei H, Liu C T. Recent progress in quantifying glass-forming ability of bulk metallic glasses [J]. Intermetallics, 2007, 15: 618
|
| 27 |
Turnbull D. Kinetics of solidification of supercooled liquid mercury droplets [J]. J. Chem. Phys., 1952, 20: 411
|
| 28 |
Sohrabi S, Gholamipour R. Effect of Nb minor addition on the crystallization kinetics of Zr-Cu-Al-Ni metallic glass [J]. J. Non-Cryst. Solids, 2021, 560: 120731
|
| 29 |
Qiao J C, Pelletier J M. Isochronal and isothermal crystallization in Zr55Cu30Ni5Al10 bulk metallic glass [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 577
|
| 30 |
Chen Q Z, Thouas G A. Metallic implant biomaterials [J]. Mater. Sci. Eng., 2015, R87: 1
|
| 31 |
Wang W H, Dong C, Shek C H. Bulk metallic glasses [J]. Mater. Sci. Eng., 2004, R44: 45
|
| 32 |
Conner R D, Choi-Yim H, Johnson W. Mechanical properties of Zr57Nb5Al10Cu15.4Ni12.6 metallic glass matrix particulate composites [J]. J. Mater. Res., 1999, 14: 3292
|
| 33 |
Kusy M, Kühn U, Concustell A, et al. Fracture surface morphology of compressed bulk metallic glass-matrix-composites and bulk metallic glass [J]. Intermetallics, 2006, 14: 982
|
| 34 |
Xi X K, Zhao D Q, Pan M X, et al. Fracture of brittle metallic glasses: Brittleness or plasticity [J]. Phys. Rev. Lett., 2005, 94: 125510
|
| 35 |
Zhang Y, Zhou M, Zhao X Y, et al. Co substituted Zr-Cu-Al-Ni metallic glasses with enhanced glass-forming ability and high plasticity [J]. J. Non-Cryst. Solids, 2017, 473: 120
|
| 36 |
Wang W H, Wei Q, Friedrich S. Microstructure, decomposition, and crystallization in Zr41Ti14Cu12.5Ni10Be22.5 bulk metallic glass [J]. Phys. Rev., 1998, 57B: 8211
|
| 37 |
Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element [J]. Mater. Trans., 2005, 46: 2817
|
| 38 |
Zhang Q S, Zhang W, Louzguine-Luzgin D V, et al. High glass-forming ability and unusual deformation behavior of new Zr-Cu-Fe-Al bulk metallic glasses [J]. Mater. Sci. Forum, 2010, 654-656: 1042
|
| 39 |
Cui X, Zu F Q, Jiang W X, et al. Achieving superior glass forming ability of Zr-Cu-Al-Ni-Ti/Ag bulk metallic glasses by element substitution [J]. J. Non-Cryst. Solids, 2013, 375: 83
|
| 40 |
Trexler M M, Thadhani N N. Mechanical properties of bulk metallic glasses [J]. Prog. Mater. Sci., 2010, 55: 759
|
| 41 |
Hua N B, Huang L, He W, et al. A Ni-free high-zirconium-based bulk metallic glass with enhanced plasticity and biocompatibility [J]. J. Non-Cryst. Solids, 2013, 376: 133
|
| 42 |
Park E S, Lee J Y, Kim D H. Effect of Ag addition on the improvement of glass-forming ability and plasticity of Mg-Cu-Gd bulk metallic glass [J]. J. Mater. Res., 2005, 20: 2379
|
| 43 |
Li B, Sun W C, Qi H N, et al. Effects of Ag substitution for Fe on glass-forming ability, crystallization kinetics, and mechanical properties of Ni-free Zr-Cu-Al-Fe bulk metallic glasses [J]. J. Alloys Compd., 2020, 827: 154385
|
| 44 |
Sun Y, Huang Y J, Fan H B, et al. In vitro and in vivo biocompatibility of an Ag-bearing Zr-based bulk metallic glass for potential medical use [J]. J. Non-Cryst. Solids, 2015, 419: 82
|
| 45 |
Hua N B, Huang L, Wang J F, et al. Corrosion behavior and in vitro biocompatibility of Zr-Al-Co-Ag bulk metallic glasses: An experimental case study [J]. J. Non-Cryst. Solids, 2012, 358: 1599
|
| 46 |
Li W R, Xie X B, Shi Q S, et al. Antibacterial activity and mechanism of silver nanoparticles on Escherichia coli [J]. Appl. Microbiol. Biotechnol., 2010, 85: 1115
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|