| 铀基非晶复合材料的相分离与凝固序列研究 |
张雷, 施韬( ), 黄火根, 张培, 张鹏国, 吴敏, 法涛 |
| 中国工程物理研究院材料研究所 江油 621907 |
|
| Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites |
ZHANG Lei, SHI Tao( ), HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao |
| Institute of Materials, China Academy of Engineering Physics, Jiangyou 621907, China |
引用本文:
张雷, 施韬, 黄火根, 张培, 张鹏国, 吴敏, 法涛. 铀基非晶复合材料的相分离与凝固序列研究[J]. 金属学报, 2022, 58(2): 225-230.
Lei ZHANG,
Tao SHI,
Huogen HUANG,
Pei ZHANG,
Pengguo ZHANG,
Min WU,
Tao FA.
Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. Acta Metall Sin, 2022, 58(2): 225-230.
| 1 |
Li G X , Wu S . Nuclear Fuels [M]. Beijing: Chemical Industry Press, 2007: 13
|
| 1 |
李冠兴, 武 胜 . 核燃料 [M]. 北京: 化学工业出版社, 2007: 13
|
| 2 |
Paukov M , Tkach I , Huber F , et al . U-Zr alloy: XPS and TEM study of surface passivation [J]. Appl. Surf. Sci., 2018, 441: 113
|
| 3 |
Banos A , Harker N J , Scott T B . A review of uranium corrosion by hydrogen and the formation of uranium hydride [J]. Corros. Sci., 2018, 136: 129
|
| 4 |
Bazley S G , Petherbridge J R , Glascott J . The influence of hydrogen pressure and reaction temperature on the initiation of uranium hydride sites [J]. Solid State Ionics, 2012, 211: 1
|
| 5 |
Sowa S , Kim-Ngan N T H , Krupska M , et al . Structure and properties of U alloys with selected d-metals and their hydrides [J]. Physica, 2018, 536B: 546
|
| 6 |
Li F F , Lu L , Meng X D , et al . An enhanced hydrogen corrosion by the Ti(C,N) inclusions in U-0.79 wt%Ti alloy [J]. J. Alloys Compd., 2020: 820: 153124
|
| 7 |
Beevers C J , Newman G T . Hydrogen embrittlement in uranium [J]. J. Nucl. Mater., 1967, 23: 10
|
| 8 |
Ji H F , Chen X L , Shi P , et al . The effects of microstructure on the hydriding for 500oC/2 h aged U-13at.%Nb alloy [J]. J. Nucl. Mater., 2017, 488: 252
|
| 9 |
Taylor C D , Lillard R S . Ab-initio calculations of the hydrogen-uranium system: Surface phenomena, absorption, transport and trapping [J]. Acta Mater., 2009, 57: 4707
|
| 10 |
Taylor C D , Lookman T , Lillard R S . Ab initio calculations of the uranium-hydrogen system: Thermodynamics, hydrogen saturation of α-U and phase-transformation to UH3 [J]. Acta Mater., 2010, 58: 1045
|
| 11 |
Jones C P , Scott T B , Petherbridge J R , et al . A surface science study of the initial stages of hydrogen corrosion on uranium metal and the role played by grain microstructure [J]. Solid State Ionics, 2013, 231: 81
|
| 12 |
Kaltenboeck G , Demetriou M D , Roberts S , et al . Shaping metallic glasses by electromagnetic pulsing [J]. Nat. Commun., 2016, 7: 10576
|
| 13 |
Wang W H . The nature and properties of amorphous matter [J]. Prog. Phys., 2013, 33: 177
|
| 13 |
汪卫华 . 非晶态物质的本质和特性 [J]. 物理学进展, 2013, 33: 177
|
| 14 |
Chen M W . A brief overview of bulk metallic glasses [J]. NPG Asia Mater., 2011, 3: 82
|
| 15 |
Schuh C A , Hufnagel T C , Ramamurty U . Mechanical behavior of amorphous alloys [J]. Acta Mater., 2007, 55: 4067
|
| 16 |
Huang H G , Wang Y M , Chen L , et al . Study on formation and corrosion resistance of amorphous alloy in U-Co system [J]. Acta Metall. Sin., 2015, 51: 623
|
| 16 |
黄火根, 王英敏, 陈 亮 等 . U-Co系非晶合金的形成与耐蚀性研究 [J]. 金属学报, 2015, 51: 623
|
| 17 |
Huang H G , Ke H B , Wang Y M , et al . Stable U-based metallic glasses [J]. J. Alloys Compd., 2016, 684: 75
|
| 18 |
Xu H Y , Ke H B , Huang H G , et al . U-based metallic glasses with superior glass forming ability [J]. J. Nucl. Mater., 2018, 499: 372
|
| 19 |
Huang H G , Xu H Y , Zhang P G , et al . U-Cr binary alloys with anomalous glass-forming ability [J]. Acta Metall. Sin., 2017, 53: 233
|
| 19 |
黄火根, 徐宏扬, 张鹏国 等 . 具有反常非晶形成能力的U-Cr二元合金 [J]. 金属学报, 2017, 53: 233
|
| 20 |
Elliott R O , Giessen B C . On the formation of metallic glasses based on U, Np or Pu [J]. Acta Metall., 1982, 30: 785
|
| 21 |
Drehman A J , Poon S J . Anomalous glass-forming ability of uranium-based alloys [J]. J. Non-Cryst. Solids, 1985, 76: 321
|
| 22 |
Qiao J W , Jia H L , Liaw P K . Metallic glass matrix composites [J]. Mater. Sci. Eng., 2016, R100: 1
|
| 23 |
Telford M . The case for bulk metallic glass [J]. Mater. Today, 2004, 7: 36
|
| 24 |
Peker A , Johnson W L . A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 [J]. Appl. Phys. Lett., 1993, 63: 2342
|
| 25 |
Huang H G , Ke H B , Zhang P , et al . U-involved sphere-dispersed metallic glass matrix composites [J]. Mater. Des., 2018, 157: 371
|
| 26 |
Kim D H , Kim W T , Park E S , et al . Phase separation in metallic glasses [J]. Prog. Mater. Sci., 2013, 58: 1103
|
| 27 |
Chen H S . Glass temperature, formation and stability of Fe, Co, Ni, Pd and Pt based glasses [J]. Mater. Sci. Eng., 1976, 23: 151
|
| 28 |
Liu Z G , Wu X J , Chen Y , et al . Heterogeneity in Fe82.3Ni1.7B16 glass [J]. J. Non-Cryst. Solids, 1989, 109: 262
|
| 29 |
Kharkov E I , Lysov V I , Ishchenko A M . The relation of high-temperature stability of amorphous alloys with nucleation and growth of the crystalline phases [J]. J. Non-Cryst. Solids, 1990, 117-118: 244
|
| 30 |
Walter J L , Bacon F , Luborsky F E . An Auger analysis of the embrittlement of the amorphous alloy Ni40Fe40P14B6 [J]. Mater. Sci. Eng., 1976, 24: 239
|
| 31 |
Freed R L , Sande J B V . A study of the crystallization of two non-crystalline Cu-Zr alloys [J]. J. Non-Cryst. Solids, 1978, 27: 9
|
| 32 |
Oh J C , Ohkubo T , Kim Y C , et al . Phase separation in Cu43Zr43Al7Ag7 bulk metallic glass [J]. Scr. Mater., 2005, 53: 165
|
| 33 |
Wilkinson W D . Uranium Metallurgy. Volume II: Uranium Corrosion and Alloys [M]. New York: Interscience Publishers, 1962: 1414
|
| 34 |
De Boer F R , Boom R , Mattens W C M . Cohesion in Metals: Transition Metal Alloys [M]. Amsterdam: North Holland, 1988: 133, 314, 375
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|