| 搅拌头转速对2507双相不锈钢搅拌摩擦加工组织及性能的影响 |
陈果1,2, 王新波1,2, 张仁晓1,2, 马成悦1,2, 杨海峰1,2, 周利1,2( ), 赵运强3 |
1.哈尔滨工业大学 先进焊接与连接国家重点实验室 哈尔滨 150001 2.哈尔滨工业大学(威海) 山东省特种焊接技术重点实验室 威海 264209 3.广东省科学院中乌焊接研究所 广东省现代焊接技术重点实验室 广州 510651 |
|
| Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel |
CHEN Guo1,2, WANG Xinbo1,2, ZHANG Renxiao1,2, MA Chengyue1,2, YANG Haifeng1,2, ZHOU Li1,2( ), ZHAO Yunqiang3 |
1.State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China 2.Shandong Provincial Key Laboratory of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264209, China 3.Guangdong Provincial Key Laboratory of Advanced Welding Technology, China-Ukraine Institute of Welding, Guangdong Academy of Sciences, Guangzhou 510651, China |
引用本文:
陈果, 王新波, 张仁晓, 马成悦, 杨海峰, 周利, 赵运强. 搅拌头转速对2507双相不锈钢搅拌摩擦加工组织及性能的影响[J]. 金属学报, 2021, 57(6): 725-735.
Guo CHEN,
Xinbo WANG,
Renxiao ZHANG,
Chengyue MA,
Haifeng YANG,
Li ZHOU,
Yunqiang ZHAO.
Effect of Tool Rotation Speed on Microstructure and Properties of Friction Stir Processed 2507 Duplex Stainless Steel[J]. Acta Metall Sin, 2021, 57(6): 725-735.
| 1 |
Verma J, Taiwade R V. Effect of welding processes and conditions on the microstructure, mechanical properties and corrosion resistance of duplex stainless steel weldments—A review [J]. J. Manuf. Proc., 2017, 25: 134
|
| 2 |
Sathiya P, Aravindan S, Soundararajan R, et al. Effect of shielding gases on mechanical and metallurgical properties of duplex stainless-steel welds [J]. J. Mater. Sci., 2009, 44: 114
|
| 3 |
Deng B, Jiang Y M, Gong J, et al. Critical pitting and repassivation temperatures for duplex stainless steel in chloride solutions [J]. Electrochim. Acta, 2008, 53: 5220
|
| 4 |
Tavares S S M, Silva V G, Pardal J M, et al. Investigation of stress corrosion cracks in a UNS S32750 superduplex stainless steel [J]. Eng. Fail. Anal., 2013, 35: 88
|
| 5 |
Ma Z Y. Friction stir processing technology: A review [J]. Metall. Mater. Trans., 2008, 39A: 642
|
| 6 |
Ji S D, Huang R F, Wu B S. Review on friction stir welding repair [J]. J. Shenyang Aero. Univ., 2017, 34(5): 1
|
| 6 |
姬书得, 黄若飞, 吴宝生. 搅拌摩擦焊修复技术的研究现状 [J]. 沈阳航空航天大学学报, 2017, 34(5): 1
|
| 7 |
Chen W L. The precipitation behavior of the σ phase and its effect on performance in 2707 duplex stainless steel [D]. Taiyuan: Taiyuan University of Technology, 2018
|
| 7 |
陈万里. 2707双相不锈钢中σ相析出行为及其对性能的影响 [D]. 太原: 太原理工大学, 2018
|
| 8 |
Liu X L. Study on the microstructure and properties of friction stir welded hyper stainless steel SAF2707 joint [D]. Taiyuan: Taiyuan University of Technology, 2017
|
| 8 |
刘兴龙. 特超级双相不锈钢SAF2707搅拌摩擦焊接头显微组织和性能研究 [D]. 太原: 太原理工大学, 2017
|
| 9 |
Esmailzadeh M, Shamanian M, Kermanpur A, et al. Microstructure and mechanical properties of friction stir welded lean duplex stainless steel [J]. Mater. Sci. Eng., 2013, A561: 486
|
| 10 |
Santos T F D A, Torres E A, Ramirez A J. Friction stir welding of duplex stainless steels [J]. Weld. Int., 2017, 32: 103
|
| 11 |
Mishra M K, Gunasekaran G, Rao A G, et al. Effect of multipass friction stir processing on mechanical and corrosion behavior of 2507 super duplex stainless steel [J]. J. Mater. Eng. Perform., 2017, 26: 849
|
| 12 |
Magnani M, Terada M, Lino A O, et al. Microstructural and electrochemical characterization of friction stir welded duplex stainless steels [J]. Int. J. Electrochem. Sci., 2014, 9: 2966
|
| 13 |
Li G H, Zhou L, Luo S F, et al. Microstructure and mechanical properties of self-reacting friction stir welded AA2219-T87 aluminium alloy [J]. Sci. Technol. Weld. Join., 2019, 25: 142
|
| 14 |
Sato Y S, Kokawa H, Ikeda K, et al. Microtexture in the friction-stir weld of an aluminum alloy [J]. Metall. Mater. Trans., 2001, 32A: 941
|
| 15 |
Saeid T, Abdollah-Zadeh A, Assadi H, et al. Effect of friction stir welding speed on the microstructure and mechanical properties of a duplex stainless steel [J]. Mater. Sci. Eng., 2008, A496: 262
|
| 16 |
Santos T F D A, López E A T, Da Fonseca E B, et al. Friction stir welding of duplex and superduplex stainless steels and some aspects of microstructural characterization and mechanical performance [J]. Mater. Res., 2016, 19: 117
|
| 17 |
Ma M. Hot deformation behavior and microstructural evolution of duplex stainless steels [D]. Shenyang: Northeastern University, 2016
|
| 17 |
马 明. 双相不锈钢热变形行为及组织演变 [D]. 沈阳: 东北大学, 2016
|
| 18 |
Zhang Z Y, Zhang H Z, Hu J, et al. Microstructure evolution and mechanical properties of briefly heat-treated SAF 2507 super duplex stainless steel welds [J]. Constr. Build. Mater., 2018, 168: 338
|
| 19 |
Giorjão R A R, Pereira V F, Terada M, et al. Microstructure and mechanical properties of friction stir welded 8 mm pipe SAF 2507 super duplex stainless steel [J]. J. Mater. Res. Technol., 2018, 340: 1
|
| 20 |
Santos T F A, Marinho R R, Paes M T P, et al. Microstructure evaluation of UNS S32205 duplex stainless steel friction stir welds [J]. Rem Rev. Esc. Minas., 2013, 66: 187
|
| 21 |
Sato Y S, Nelson T W, Sterling C J, et al. Microstructure and mechanical properties of friction stir welded SAF 2507 super duplex stainless steel [J]. Mater. Sci. Eng., 2005, A397: 376
|
| 22 |
Steel R J, Sterling C J. Friction stir welding of 2205 duplex stainless and 3Cr12 steels [A]. The Fourteenth International Offshore and Polar Engineering Conference [C]. California: International Society of Offshore and Polar Engineers, 2004: 67
|
| 23 |
Ralston K D, Birbilis N, Davies C H J. Revealing the relationship between grain size and corrosion rate of metals [J]. Scr. Mater., 2010, 63: 1201
|
| 24 |
Atapour M, Sarlak H, Esmailzadeh M. Pitting corrosion susceptibility of friction stir welded lean duplex stainless steel joints [J]. Int. J. Adv. Manuf. Technol., 2016, 83: 721
|
| 25 |
Sarlak H, Atapour M, Esmailzadeh M. Corrosion behavior of friction stir welded lean duplex stainless steel [J]. Mater. Des., 2015, 66: 209
|
| 26 |
Wang X Y, Li D Y. Mechanical and electrochemical behavior of nanocrystalline surface of 304 stainless steel [J]. Electrochim. Acta, 2002, 47: 3939
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|