    					| 单晶高温合金共晶溶解行为的差热分析 |  
						| 张少华(  ), 谢光, 董加胜, 楼琅洪 |  
					| 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 |  
						|  |  
    					| Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry |  
						| ZHANG Shaohua(  ), XIE Guang, DONG Jiasheng, LOU Langhong |  
						| Shi -Changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |  
								张少华, 谢光, 董加胜, 楼琅洪. 单晶高温合金共晶溶解行为的差热分析[J]. 金属学报, 2021, 57(12): 1559-1566.	
																												Shaohua ZHANG,
																								Guang XIE,
																								Jiasheng DONG,
																												Langhong LOU. 
				Investigation on Eutectic Dissolution Behavior of Single Crystal Superalloy by Differential Scanning Calorimetry[J]. Acta Metall Sin, 2021, 57(12): 1559-1566.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																																															
																| 1 | Sims C T, Stoloff N S, Hagel W C. Superalloys II [M]. New York: John Wiley, 1987: 615 |  
																| 2 | Gell M, Duhl D N, Giamei A F. The development of single crystal superalloy turbine blades [A]. Superalloys 1980 [C]. Warrendale, PA: TMS, 1980: 205 |  
																| 3 | Zhang J, Wang L, Wang D, et al. Recent progress in research and development of nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2019, 55: 1077 |  
																| 3 | 张 健, 王 莉, 王 栋等. 镍基单晶高温合金的研发进展 [J]. 金属学报, 2019, 55: 1077 |  
																| 4 | Kearsey R M, Beddoes J C, Jones P, et al. Compositional design considerations for microsegregation in single crystal superalloy systems [J]. Intermetallics, 2004, 12: 903 |  
																| 5 | Chen J Y, Feng Q, Sun Z Q. Topologically close-packed phase promotion in a Ru-containing single crystal superalloy [J]. Scr. Mater., 2010, 63: 795 |  
																| 6 | Wilson B C, Hickman J A, Fuchs G E. The effect of solution heat treatment on a single-crystal Ni-based superalloy [J]. JOM, 2003, 55(3): 35 |  
																| 7 | Fuchs G E. Solution heat treatment response of a third generation single crystal Ni-base superalloy [J]. Mater. Sci. Eng., 2001, A300: 52 |  
																| 8 | Zhang J H, Zhang Z Y, Li Y A. Investigation of the heat treatment in a single crystal nickel-base superalloy [J]. Dev. Appl. Mater., 1997, 12(1): 27 |  
																| 8 | 张静华, 张志亚, 李英敖. DD8单晶镍基高温合金热处理制度研究 [J]. 材料开发与应用, 1997, 12(1): 27 |  
																| 9 | Han M, Luo Y S. Study on modified heat treatment for DD3 single crystal superalloys [J]. J. Aeronaut. Mater., 2009, 29(2): 34 |  
																| 9 | 韩 梅, 骆宇时. 改进DD3单晶高温合金热处理工艺的研究 [J]. 航空材料学报, 2009, 29(2): 34 |  
																| 10 | Li J R, Liu S Z, Wang X G, et al. Development of a low-cost third generation single crystal superalloy DD9 [A]. Superalloys 2016: Proceedings of the 13th Intenational Symposium of Superalloys [C]. Seven Springs, Pennsylvania: TMS, 2016: 57 |  
																| 11 | Su X L, Xu Q Y, Wang R N, et al. Microstructural evolution and compositional homogenization of a low Re-bearing Ni-based single crystal superalloy during through progression of heat treatment [J]. Mater. Des., 2018, 141: 296 |  
																| 12 | Ai C, Xi L G, Wang B, et al. Investigation on solution heat treatment response and γ′ solvus temperature of a Mo-rich second generation Ni based single crystal superalloy [J]. Intermetallics, 2020, 125: 106896 |  
																| 13 | Hu Z Q, Liu L R, Jin T. et al. Development of the Ni-base single crystal superalloys [J]. Aeroengine, 2005, 31(3): 1 |  
																| 13 | 胡壮麒, 刘丽荣, 金 涛等. 镍基单晶高温合金的发展 [J]. 航空发动机, 2005, 31(3): 1 |  
																| 14 | Zhang Y B, Liu L, Huang T W, et al. Investigation on a ramp solution heat treatment for a third generation nickel-based single crystal superalloy [J]. J. Alloys Compd., 2017, 723: 922 |  
																| 15 | Pang H T, Zhang L J, Hobbs R A, et al. Solution heat treatment optimization of fourth-generation single-crystal nickel-base superalloys [J]. Metall. Mater. Trans., 2012, 43A: 3264 |  
																| 16 | Zhang Y B, Liu L, Huang T W, et al. Investigation on remelting solution heat treatment for nickel-based single crystal superalloys [J]. Scr. Mater., 2017, 136: 74 |  
																| 17 | Yue X D, Li J R, Shi Z X, et al. Designing of the homogenization-solution heat treatment for advanced single crystal superalloys [J]. Rare Met. Mater. Eng., 2017, 46: 1530 |  
																| 18 | Hegde S R, Kearsey R M, Beddoes J C. Designing homogenization-solution heat treatments for single crystal superalloys [J]. Mater. Sci. Eng., 2010, A527: 5528 |  
																| 19 | Lee H S, Kim D H, Kim D S, et al. Microstructural changes by heat treatment for single crystal superalloy exposed at high temperature [J]. J. Alloys Compd., 2013, 56: 135 |  
																| 20 | Wen Y H, Lill J V, Chen S L, et al. A ternary phase-field model incorporating commercial CALPHAD software and its application to precipitation in superalloys [J]. Acta Mater., 2010, 58: 875 |  
																| 21 | Zhang S H, Xie G, Zhang G, et al. Differential thermal analysis method for measuring initial melting teperature of single crystal superalloy [P]. Chin Pat, 202010283750.X, 2020 |  
																| 21 | 张少华, 谢 光, 张 功等. 一种测量单晶高温合金初熔温度的差热分析方法 [P]. 中国专利, 202010283750.X, 2020) |  
																| 22 | Yang Y F, Zhu K H, Wang Y J, et al. Analysis and discussion of differential thermal figures in physichemical experiment [J]. J. Zhejiang Norm. Univ. (Nat. Sci.), 2002, 25: 279 |  
																| 22 | 杨元法, 朱凯汉, 王月娟等. 物理化学实验中差热图谱的解析讨论 [J]. 浙江师范大学学报(自然科学版), 2002, 25: 279 |  
																| 23 | Wagner M. Thermal Analysis in Practice [M]. Munich: Hanser, 2018: 101 |  
																| 24 | Avrami M. Kinetics of phase change. I General theory [J]. J. Chem. Phys., 1939, 7: 1103 |  
																| 25 | Avrami M. Kinetics of phase change. II Transformation-time relations for random distribution of nuclei [J]. J. Chem. Phys., 1940, 8: 212 |  
																| 26 | Avrami M. Granulation, phase change, and microstructure kinetics of phase change. III [J]. J. Chem. Phys., 1941, 9: 177 |  
																| 27 | Sun Z Y, Liu C M. Diffusion and Phase Transformation in Alloys [M]. Shenyang: Northeastern University Press, 2002: 39 |  
																| 27 | 孙振岩, 刘春明. 合金中的扩散与相变 [M]. 沈阳: 东北大学出版社, 2002: 39 |  
																| 28 | Karunaratne M S A, Cox D C, Carter P, et al. Modelling of the microsegregation in CMSX-4 superalloy and its homogenisation during heat treatment [A]. Superalloys 2000 [C]. Pennsylvania: TMS, 2000: 263 |  
																| 29 | Jiang C, Gleeson B. Site preference of transition metal elements in Ni3Al [J]. Scr. Mater., 2006, 55: 433 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |