| N掺杂对磁控溅射Ta涂层微观结构与耐磨损性能的影响 |
杨莎莎1,2,杨峰3,陈明辉4( ),牛云松1,朱圣龙1,王福会4 |
1. 中国科学院金属研究所 沈阳 110016 2. 中国科学技术大学材料科学与工程学院 沈阳 110016 3. 沈阳理工大学装备工程学院 沈阳 110159 4. 东北大学沈阳材料科学国家研究中心东北大学联合研究分部 沈阳 110819 |
|
| Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering |
Shasha YANG1,2,Feng YANG3,Minghui CHEN4( ),Yunsong NIU1,Shenglong ZHU1,Fuhui WANG4 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2. School of Material Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3. School of Equipment Engineering, Shenyang Ligong University, Shenyang 110159, China 4. Shenyang National Key Laboratory for Materials Science, Northeastern University, Shenyang 110819, China |
引用本文:
杨莎莎,杨峰,陈明辉,牛云松,朱圣龙,王福会. N掺杂对磁控溅射Ta涂层微观结构与耐磨损性能的影响[J]. 金属学报, 2019, 55(3): 308-316.
Shasha YANG,
Feng YANG,
Minghui CHEN,
Yunsong NIU,
Shenglong ZHU,
Fuhui WANG.
Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering[J]. Acta Metall Sin, 2019, 55(3): 308-316.
| [1] | Sopok S, Rickard C, Dunn S. Thermal-chemical-mechanical gun bore erosion of an advanced artillery system part one: Theories and mechanisms [J]. Wear, 2005, 258: 659 | | [2] | Chen X J, Yan Q, Ma Q, Influence of the laser pre-quenched substrate on an electroplated chromium coating/steel substrate [J]. Appl. Surf. Sci., 2017, 405: 273 | | [3] | Van Phuong N, Kwon S C, Lee J Y, et al. The effects of pH and polyethylene glycol on the Cr(III) solution chemistry and electrodeposition of chromium [J]. Surf. Coat. Technol., 2012, 206: 4349 | | [4] | Quan C, He Y D. Properties of nanocrystalline Cr coatings prepared by cathode plasma electrolytic deposition from trivalent chromium electrolyte [J]. Surf. Coat. Technol., 2015, 269: 319 | | [5] | Lee S L, Windover D, Audino M, et al. High-rate sputter deposited tantalum coating on steel for wear and erosion mitigation [J]. Surf. Coat. Technol., 2002, 149: 62 | | [6] | Maeng S M, Axe L, Tyson T A, et al. Corrosion behavior of magnetron sputtered α-Ta coatings on smooth and rough steel substrates [J]. Surf. Coat. Technol., 2006, 200: 5717 | | [7] | Hu X F, Xu Q. Preparation of tantalum by electro-deoxidation in a CaCl2-NaCl melt [J]. Acta Metall. Sin., 2006, 42: 285 | | [7] | 胡小锋, 许 茜. CaCl2-NaCl熔盐电脱氧法制备金属Ta [J]. 金属学报, 2006, 42: 285 | | [8] | Matson D W, McClanahan E D, Lee S L, et al. Properties of thick sputtered Ta used for protective gun tube coatings [J]. Surf. Coat. Technol., 2001, 146-147: 344 | | [9] | Wang S, Xiong D S, Li J L, et al. Wear and erosion resistance properties of electroplating Ta coating in molten salt [J]. China Surf. Eng., 2015, 28(2): 101 | | [9] | 王 升, 熊党生, 李建亮等. 熔盐电镀钽及其耐磨损烧蚀性能 [J]. 中国表面工程, 2015, 28(2): 101 | | [10] | Myers S, Lin J L, Souza R M, et al. The β to α phase transition of tantalum coatings deposited by modulated pulsed power magnetron sputtering [J]. Surf. Coat. Technol., 2013, 214: 38 | | [11] | Lundin D, Sarakinos K. An introduction to thin film processing using high-power impulse magnetron sputtering [J]. J. Mater. Res., 2012, 27: 780 | | [12] | Lin J L, Moore J J, Sproul W D, et al. Effect of negative substrate bias on the structure and properties of Ta coatings deposited using modulated pulse power magnetron sputtering [J]. IEEE Trans. Plasma Sci., 2010, 38: 3071 | | [13] | Ferreira F, Sousa C, Cavaleiro A, et al. Phase tailoring of tantalum thin films deposited in deep oscillation magnetron sputtering mode [J]. Surf. Coat. Technol., 2017, 314: 97 | | [14] | Frank S, Gruber P A, Handge U A, et al. In situ studies on the cohesive properties of α- and β-Ta layers on polyimide substrates [J]. Acta Mater., 2011, 59: 5881 | | [15] | Niu Y S, Chen M H, Wang J L, et al. Preparation and thermal shock performance of thick α-Ta coatings by direct current magnetron sputtering (DCMS) [J]. Surf. Coat. Technol., 2017, 321: 19 | | [16] | Lou B Y, Wang Y X. Effects of Mo content on the micro-structure and tribological properties of CrMoAlN films [J]. Acta Metall. Sin., 2016, 52: 727 | | [16] | 楼白杨, 王宇星. Mo含量对CrMoAlN薄膜微观结构和摩擦磨损性能的影响 [J]. 金属学报, 2016, 52: 727 | | [17] | Han K C, Liu Y Q, Lin G Q, et al. Study on atomic-scale strengthening mechanism of transition-metal nitride MNx(M=Ti,Zr,Hf) films within wide composition ranges [J]. Acta Metall. Sin., 2016, 52: 1601 | | [17] | 韩克昌, 刘一奇, 林国强等. 宽固溶区过渡金属氮化物MNx(M=Ti, Zr, Hf)硬质薄膜原子尺度强化机制研究 [J]. 金属学报, 2016, 52: 1601 | | [18] | Cui W F, Cao D, Qin G W. Microstructure and wear resistance of Ti/TiN multilayer films deposited by magnetron sputtering [J]. Acta Metall. Sin., 2015, 51: 1531 | | [18] | 崔文芳, 曹 栋, 秦高悟. 磁控溅射沉积Ti/TiN多层膜的组织特征及耐磨损性能 [J]. 金属学报, 2015, 51: 1531 | | [19] | Zhao S L, Zhang Z, Zhang J, et al. Microstructure and wear resistance of TiAlZrCr/(Ti, Al, Zr, Cr)N gradient films deposited by multi-arc ion plating [J]. Acta Metall. Sin., 2016, 52: 747 | | [19] | 赵时璐, 张 震, 张 钧等. 多弧离子镀TiAlZrCr/(Ti, Al, Zr, Cr)N梯度膜的微观结构与耐磨损性能 [J]. 金属学报, 2016, 52: 747 | | [20] | Raole P M, Narsale A M, Kothari D C, et al. Glancing-angle X-ray diffraction and X-ray photoelectron spectroscopy studies of nitrogen-implanted tantalum [J]. Mater. Sci. Eng., 1989, A115: 73 | | [21] | Rogers J D, Sundaram V S, Kleiman G G, et al. High resolution study of the M45N67N67 and M45N45N67 Auger transitions in the 5d series [J]. J. Phys., 1982, 12F: 2097 | | [22] | Takano I, Isobe S, Sasaki T A, et al. Nitrogenation of various transition metals by N+2-ion implantation [J]. Appl. Surf. Sci., 1989, 37: 25 | | [23] | Stavrev M, Fischer D, Wenzel C, et al. Crystallographic and morphological characterization of reactively sputtered Ta, Ta-N and Ta-N-O thin films [J]. Thin Solid Films, 1997, 307: 79 | | [24] | Zhu S L, Wang F H, Wu W T. Theory and Application of Reactive Sputtering Kinetics [M]. Beijing: China Science and Technology Press, 1999: 18 | | [24] | 朱圣龙, 王福会, 吴维?. 反应溅射动力学理论及应用 [M]. 北京: 中国科学技术出版社, 1999: 18 | | [25] | Pelleg J, Zevin L Z, Lungo S, et al. Reactive-sputter-deposited TiN films on glass substrates [J]. Thin Solid Films, 1991, 197: 117 | | [26] | Wang X, Wang Z Y, Feng Z X, et al. Effect of N doping on microstructure, mechanical and tribological properties of V-Al-C coatings [J]. Acta Metall. Sin., 2017, 53: 709 | | [26] | 王 鑫, 王振玉, 冯再新等. N掺杂对V-Al-C涂层微观结构、力学及摩擦性能的影响 [J]. 金属学报, 2017, 53: 709 | | [27] | Xu S, Xu J, Munroe P, et al. Nanoporosity improves the damage tolerance of nanostructured tantalum nitride coatings [J]. Scr. Mater., 2017, 133: 86 | | [28] | Hakamada M, Nakamoto Y, Matsumoto H, et al. Relationship between hardness and grain size in electrodeposited copper films [J]. Mater. Sci. Eng., 2007, A457: 120 | | [29] | Yamamoto T, Kawate M, Hasegawa H, et al. Effects of nitrogen concentration on microstructures of WNx films synthesized by cathodic arc method [J]. Surf. Coat. Technol., 2005, 193: 372 | | [30] | Cheng G A, Han D Y, Liang C L, et al. Influence of residual stress on mechanical properties of TiAlN thin films [J]. Surf. Coat. Technol., 2013, 228: S328 | | [31] | Yu L H, Dong H Z, Xu J H. Influence of C content on microstructure, mechanical properties and friction and wear properties of TiWCN composite films [J]. Acta Metall. Sin., 2014, 50: 1350 | | [31] | 喻利花, 董鸿志, 许俊华. C含量对TiWCN复合膜微结构、力学性能和摩擦磨损性能的影响 [J]. 金属学报, 2014, 50: 1350 | | [32] | Aliofkhazraei M, Rouhaghdam A S. Fabrication of TiC/WC ultra hard nanocomposite layers by plasma electrolysis and study of its characteristics [J]. Surf. Coat. Technol., 2010, 205: S51 |
|
|