高熵合金涂层研究进展 |
崔洪芝1,2( ), 姜迪2 |
1. 中国海洋大学 材料科学与工程学院 青岛 266100 2. 山东科技大学 材料科学与工程学院 青岛 266590 |
|
Research Progress of High-Entropy Alloy Coatings |
CUI Hongzhi1,2( ), JIANG Di2 |
1. School of Materials Science and Engineering, Ocean University of China, Qingdao 266100, China 2. School of Materials Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China |
引用本文:
崔洪芝, 姜迪. 高熵合金涂层研究进展[J]. 金属学报, 2022, 58(1): 17-27.
Hongzhi CUI,
Di JIANG.
Research Progress of High-Entropy Alloy Coatings[J]. Acta Metall Sin, 2022, 58(1): 17-27.
1 |
Yeh J W , Chen S K , Lin S J , et al . Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299
|
2 |
Wang Y Q , Liu B , Yan K , et al . Probing deformation mechanisms of a FeCoCrNi high-entropy alloy at 293 and 77 K using in situ neutron diffraction [J]. Acta Mater., 2018, 154: 79
|
3 |
Hsu C Y , Juan C C , Wang W R , et al . On the superior hot hardness and softening resistance of AlCoCr x FeMo0.5Ni high-entropy alloys [J]. Mater. Sci. Eng., 2011, A528: 3581
|
4 |
Song Q T , Xu Y K , Xu J . Dry-sliding wear behavior of (TiZrNb-Ta)90Mo10 high-entropy alloy against Al2O3 [J]. Acta Metall. Sin., 2020, 56: 1507
|
4 |
宋芊汀, 徐映坤, 徐 坚 . (TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为 [J]. 金属学报, 2020, 56: 1507
|
5 |
Yang H O , Shang X L , Wang L L , et al . Effect of constituent elements on the corrosion resistance of single-phase CoCrFeNi high-entropy alloys in NaCl solution [J]. Acta Metall. Sin., 2018, 54: 905
|
5 |
杨海欧, 尚旭亮, 王理林 等 . 单相CoCrFeNi高熵合金的组成元素对其在NaCl溶液中的耐蚀性能的影响 [J]. 金属学报, 2018, 54: 905
|
6 |
Li Z Z , Zhao S T , Ritchie R O , et al . Mechanical properties of high-entropy alloys with emphasis on face-centered cubic alloys [J]. Prog. Mater. Sci., 2019, 102: 296
|
7 |
Cantor B , Chang I T H , Knight P , et al . Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213
|
8 |
Wang W R , Wang W L , Wang S C , et al . Effects of Al addition on the microstructure and mechanical property of Al x CoCrFeNi high-entropy alloys [J]. Intermetallics, 2012, 26: 44
|
9 |
Singh S , Wanderka N , Murty B S , et al . Decomposition in multi-component AlCoCrCuFeNi high-entropy alloy [J]. Acta Mater., 2011, 59: 182
|
10 |
Jiang H L , Hu Z F , Yuan X T , et al . Microstructure and mechanical properties of TiZrHfNbSc refractory high entropy alloy [J]. Rare Met. Mater. Eng., 2020, 49: 2820
|
10 |
江洪林, 胡志方, 袁学韬 等 . TiZrHfNbSc难熔高熵合金的组织和力学性能 [J]. 稀有金属材料与工程, 2020, 49: 2820
|
11 |
Qiu Y , Thomas S , Gibson M A , et al . Corrosion of high entropy alloys [J]. npj Mater. Degrad., 2017, 1: 15
|
12 |
Turnbull D . Under what conditions can a glass be formed? [J]. Contem. Phys., 1969, 10: 473
|
13 |
Inoue A . Stabilization of metallic supercooled liquid and bulk amorphous alloys [J]. Acta Mater., 2000, 48: 279
|
14 |
Cheng J L , Chen G , Gao P , et al . The critical cooling rate and microstructure evolution of Zr41.2Ti13.8Cu12.5Ni10Be22.5 composites by Bridgman solidification [J]. Intermetallics, 2010, 18: 115
|
15 |
Shen J , Chen Q J , Sun J F , et al . Exceptionally high glass-forming ability of an FeCoCrMoCBY alloy [J]. Appl. Phys. Lett., 2005, 86: 151907
|
16 |
Wu C L , Zhang S , Zhang C H , et al . Phase evolution of FeCoCrAlCuNiMo x coatings by laser high-entropy alloying on stainless steels [J]. Acta Metall. Sin., 2016, 52: 797
|
16 |
吴臣亮, 张 松, 张春华 等 . 不锈钢表面FeCoCrAlCuNiMo x 激光高熵合金化层的相演变 [J]. 金属学报, 2016, 52: 797
|
17 |
Zhao K , Xia X X , Bai H Y , et al . Room temperature homogeneous flow in a bulk metallic glass with low glass transition temperature [J]. Appl. Phys. Lett., 2011, 98: 141913
|
18 |
Zhang S Y , Gao Y Y , Zhang Z B , et al . Research progress in corrosion resistance of high-entropy metallic glasses [J]. J. Mater. Eng., 2021, 49(1): 44
|
18 |
张舒研, 高洋洋, 张志彬 等 . 高熵非晶合金耐腐蚀性能研究进展 [J]. 材料工程, 2021, 49(1): 44
|
19 |
Sun H J , Man Q K , Dong Y Q , et al . Effect of Nb addition on the glass-forming ability, mechanical and soft-magnetic properties in (Co0.942Fe0.058)72 - x Nb x B22.4Si5.6 bulk glassy alloys [J]. J. Alloys Compd., 2010, 504: S31
|
20 |
Shen B L , Zhou Y J , Chang C T , et al . Effect of B to Si concentration ratio on glass-forming ability and soft-magnetic properties in (Co0.705Fe0.045B0.25 - x Si x )96Nb4 glassy alloys [J]. J. Appl. Phys., 2007, 101: 09N101
|
21 |
Amiya K , Inoue A . Fe-(Cr, Mo)-(C, B)-Tm bulk metallic glasses with high strength and high glass-forming ability [J]. Mater. Trans., 2006, 47: 1615
|
22 |
Müller F , Gorr B , Christ H J , et al . On the oxidation mechanism of refractory high entropy alloys [J]. Corros. Sci., 2019, 159: 108161
|
23 |
Guo Y X , Liu Q B . MoFeCrTiWAlNb refractory high-entropy alloy coating fabricated by rectangular-spot laser cladding [J]. Intermetallics, 2018, 102: 78
|
24 |
Ye F X , Jiao Z P , Yan S , et al . Microbeam plasma arc remanufacturing: Effects of Al on microstructure, wear resistance, corrosion resistance and high temperature oxidation resistance of Al x CoCr-FeMnNi high-entropy alloy cladding layer [J]. Vacuum, 2020, 174: 109178
|
25 |
Xiang K , Chen L Y , Chai L J , et al . Microstructural characteristics and properties of CoCrFeNiNb x high-entropy alloy coatings on pure titanium substrate by pulsed laser cladding [J]. Appl. Surf. Sci., 2020, 517: 146214
|
26 |
Zhang M N , Zhou X L , Yu X N , et al . Synthesis and characterization of refractory TiZrNbWMo high-entropy alloy coating by laser cladding [J]. Surf. Coat. Technol., 2017, 311: 321
|
27 |
Song P F , Jiang F L , Wang Y L , et al . Advances in the preparation of high entropy alloy coatings by laser cladding [J]. Surf. Technol., 2021, 50(1): 242
|
27 |
宋鹏芳, 姜芙林, 王玉玲 等 . 激光熔覆制备高熵合金涂层研究进展 [J]. 表面技术, 2021, 50(1): 242
|
28 |
Cheng J B , Liu D , Liang X B , et al . Evolution of microstructure and mechanical properties of in situ synthesized TiC-TiB2/CoCr-CuFeNi high entropy alloy coatings [J]. Surf. Coat. Technol., 2015, 281: 109
|
29 |
Peng Y B , Zhang W , Li T C , et al . Microstructures and mechanical properties of FeCoCrNi high entropy alloy/WC reinforcing particles composite coatings prepared by laser cladding and plasma cladding [J]. Int. J. Refract. Met. Hard Mater., 2019, 84: 105044
|
30 |
Shu F Y , Liu S , Zhao H Y , et al . Structure and high-temperature property of amorphous composite coating synthesized by laser cladding FeCrCoNiSiB high-entropy alloy powder [J]. J. Alloys Compd., 2018, 731: 662
|
31 |
Cheng J B , Sun B , Ge Y Y , et al . Effect of B/Si ratio on structure and properties of high-entropy glassy Fe25Co25Ni25(B x Si1 - x )25 coating prepared by laser cladding [J]. Surf. Coat. Technol., 2020, 402: 126320
|
32 |
Cao S L , Liang J , Zhou J S , et al . Microstructure evolution and wear resistance of in-situ nanoparticles reinforcing Fe-based amorphous composite coatings [J]. Surf. Interface, 2020, 21: 100652
|
33 |
Li G , Gan Y Y , Liu C H , et al . Corrosion and wear resistance of Fe-based amorphous coatings [J]. Coatings, 2020, 10: 73
|
34 |
Huang G K , Qu L D , Lu Y Z , et al . Corrosion resistance improvement of 45 steel by Fe-based amorphous coating [J]. Vacuum, 2018, 153: 39
|
35 |
Hou X C , Du D , Wang K M , et al . Microstructure and wear resistance of Fe-Cr-Mo-Co-C-B amorphous composite coatings synthesized by laser cladding [J]. Metals, 2018, 8: 622
|
36 |
Zhu Y Y , Li Z G , Li R F , et al . High power diode laser cladding of Fe-Co-B-Si-C-Nb amorphous coating: Layered microstructure and properties [J]. Surf. Coat. Technol., 2013, 235: 699
|
37 |
Zhu Y Y , Li Z G , Li R F , et al . Microstructure and property of Fe-Co-B-Si-C-Nb amorphous composite coating fabricated by laser cladding process [J]. Appl. Surf. Sci., 2013, 280: 50
|
38 |
Zhu Y Y , Li Z G , Huang J , et al . Amorphous structure evolution of high power diode laser cladded Fe-Co-B-Si-Nb coatings [J]. Appl. Surf. Sci., 2012, 261: 896
|
39 |
Li R F , Li Z G , Huang J , et al . Dilution effect on the formation of amorphous phase in the laser cladded Ni-Fe-B-Si-Nb coatings after laser remelting process [J]. Appl. Surf. Sci., 2012, 258: 7956
|
40 |
Li R F , Li Z G , Huang J , et al . Effect of Ni-to-Fe ratio on structure and properties of Ni-Fe-B-Si-Nb coatings fabricated by laser processing [J]. Appl. Surf. Sci., 2011, 257: 3554
|
41 |
Shu F Y , Wu L , Zhao H Y , et al . Microstructure and high-temperature wear mechanism of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coating [J]. Mater. Lett., 2018, 211: 235
|
42 |
Shu F Y , Zhang B L , Liu T , et al . Effects of laser power on microstructure and properties of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coatings [J]. Surf. Coat. Technol., 2019, 358: 667
|
43 |
Jin Y J , Li R F , Zheng Q C , et al . Structure and properties of laser-cladded Ni-based amorphous composite coatings [J]. Mater. Sci. Technol., 2016, 32: 1206
|
44 |
Wang H Z , Cheng Y H , Zhang X C , et al . Effect of laser scanning speed on microstructure and properties of Fe based amorphous/nanocrystalline cladding coatings [J]. Mater. Chem. Phys., 2020, 250: 123091
|
45 |
Cheng J B , Sun B , Ge Y Y , et al . Nb doping in laser-cladded Fe25Co25Ni25(B0.7Si0.3)25 high entropy alloy coatings: Microstructure evolution and wear behavior [J]. Surf. Coat. Technol., 2020, 402: 126321
|
46 |
Shu F Y , Yang B , Dong S Y , et al . Effects of Fe-to-Co ratio on microstructure and mechanical properties of laser cladded FeCoCrBNiSi high-entropy alloy coatings [J]. Appl. Surf. Sci., 2018, 450: 538
|
47 |
Gostin P F , Gebert A , Schultz L . Comparison of the corrosion of bulk amorphous steel with conventional steel [J]. Corros. Sci., 2010, 52: 273
|
48 |
Yang L , Yu T B , Li M , et al . Microstructure and wear resistance of in-situ synthesized Ti(C, N) ceramic reinforced Fe-based coating by laser cladding [J]. Ceram. Int., 2018, 44: 22538
|
49 |
Sun S T , Fu H G , Ping X L , et al . Reinforcing behavior and microstructure evolution of NbC in laser cladded Ni45 coating [J]. Appl. Surf. Sci., 2018, 455: 160
|
50 |
Zhang C , Wu B Q , Wang Q T , et al . Microstructure and properties of FeCrNiCoMnB x high-entropy alloy coating prepared by laser cladding [J]. Rare Met. Mater. Eng., 2017, 46: 2639
|
50 |
张 冲, 吴炳乾, 王乾廷 等 . 激光熔覆FeCrNiCoMnB x 高熵合金涂层的组织结构与性能 [J]. 稀有金属材料与工程, 2017, 46: 2639
|
51 |
Zhang B S , Cheng J B , Xu B S . (CuCoCrFeNi)95B5 high-entropy alloy coatings prepared by plasma transferred arc cladding process [J]. Rare Met. Mater. Eng., 2014, 43: 1128
|
51 |
张保森, 程江波, 徐滨士 . 等离子熔覆(CuCoCrFeNi)95B5高熵合金涂层研究 [J]. 稀有金属材料与工程, 2014, 43: 1128
|
52 |
Wang J Y , Zhang B S , Yu Y Q , et al . Study of high temperature friction and wear performance of (CoCrFeMnNi)85Ti15 high-entropy alloy coating prepared by plasma cladding [J]. Surf. Coat. Technol., 2020, 384: 125337
|
53 |
Wei S Y , Peng W Y , Zhao W C , et al . Research on parameter optimization and microstructure and properties of CoCrFeMnNi high entropy alloy coating cladded by plasma arc welding [J]. Mater. Rev., 2020, 34: 17052
|
53 |
魏仕勇, 彭文屹, 赵文超 等 . 等离子熔覆CoCrFeMnNi高熵合金涂层参数优化及组织与性能研究 [J]. 材料导报, 2020, 34: 17052
|
54 |
Yuan J J , Wang Q Z , Liu X Y , et al . Microstructures and high-temperature wear behavior of NiAl/WC-Fe x coatings on carbon steel by plasma cladding [J]. J. Alloys Compd., 2020, 842: 155850
|
55 |
Wu J , Zhang S D , Sun W H , et al . Enhanced corrosion resistance in Fe-based amorphous coatings through eliminating Cr-depleted zones [J]. Corros. Sci., 2018, 136: 161
|
56 |
Zhang S D , Wu J , Qi W B , et al . Effect of porosity defects on the long-term corrosion behaviour of Fe-based amorphous alloy coated mild steel [J]. Corros. Sci., 2016, 110: 57
|
57 |
Zhang S D , Zhang W L , Wang S G , et al . Characterisation of three-dimensional porosity in an Fe-based amorphous coating and its correlation with corrosion behaviour [J]. Corros. Sci., 2015, 93: 211
|
58 |
Wu J , Cui J P , Zheng Q J , et al . Insight into the corrosion evolution of Fe-based amorphous coatings under wet-dry cyclic conditions [J]. Electrochim. Acta, 2019, 319: 966
|
59 |
Xiao J K , Wu Y Q , Chen J , et al . Microstructure and tribological properties of plasma sprayed FeCoNiCrSiAl x high entropy alloy coatings [J]. Wear, 2020, 448-449: 203209
|
60 |
Li W , Liu P , Liaw P K . Microstructures and properties of high-entropy alloy films and coatings: A review [J]. Mater. Res. Lett., 2018, 6: 199
|
61 |
Wu T , Duan J W , Chen X M , et al . Research progress of the effect of alloying element on laser cladding high-entropy alloy coatings [J]. Mater. Rev., 2020, 34(suppl.): 413
|
61 |
吴 韬, 段佳伟, 陈小明 等 . 合金元素对激光熔覆高熵合金涂层影响的研究进展 [J]. 材料导报, 2020, 34(): 413
|
62 |
Guo Y J , Li C G , Zeng M , et al . In-situ TiC reinforced CoCrCuFeNiSi0.2 high-entropy alloy coatings designed for enhanced wear performance by laser cladding [J]. Mater. Chem. Phys., 2020, 242: 122522
|
63 |
Jiang P F , Zhang C H , Zhang S , et al . Fabrication and wear behavior of TiC reinforced FeCoCrAlCu-based high entropy alloy coatings by laser surface alloying [J]. Mater. Chem. Phys., 2020, 255: 123571
|
64 |
Juan Y F , Li J , Jiang Y Q , et al . Modified criterions for phase prediction in the multi-component laser-clad coatings and investigations into microstructural evolution/wear resistance of FeCrCoNiAlMo x laser-clad coatings [J]. Appl. Surf. Sci., 2019, 465: 700
|
65 |
Jia C T , Sha M H , Li S L , et al . Research progress on corrosion performance of high entropy alloy Coatings [J]. Corros. Sci. Prot. Technol., 2019, 31: 343
|
65 |
贾春堂, 沙明红, 李胜利 等 . 高熵合金涂层腐蚀性能研究进展 [J]. 腐蚀科学与防护技术, 2019, 31: 343
|
66 |
Wei L , Wang Z J , Wu Q J , et al . Effect of Mo element and heat treatment on corrosion resistance of Ni2CrFeMo x high-entropy alloy in NaCl solution [J]. Acta Metall. Sin., 2019, 55: 840
|
66 |
魏 琳, 王志军, 吴庆峰 等 . Mo元素及热处理对Ni2CrFeMo x 高熵合金在NaCl溶液中耐蚀性能的影响 [J]. 金属学报, 2019, 55: 840
|
67 |
Liu J , Liu H , Chen P J , et al . Microstructural characterization and corrosion behaviour of AlCoCrFeNiTi x high-entropy alloy coatings fabricated by laser cladding [J]. Surf. Coat. Technol., 2019, 361: 63
|
68 |
Bao Y Y , Ji X L , Ji C C , et al . Corrosion and slurry erosion properties of FeCrNiCoCuAl x high-entropy alloy coatings prepared by laser cladding [J]. J. Mater. Eng., 2019, 47(11): 141
|
68 |
鲍亚运, 纪秀林, 姬翠翠 等 . 激光熔覆FeCrNiCoCuAl x 高熵合金涂层的耐腐蚀与抗冲蚀性能 [J]. 材料工程, 2019, 47(11): 141
|
69 |
Jiang Y Q , Li J , Juan Y F , et al . Evolution in microstructure and corrosion behavior of AlCoCr x FeNi high-entropy alloy coatings fabricated by laser cladding [J]. J. Alloys Compd., 2019, 775: 1
|
70 |
Qiu X W . Corrosion behavior of Al2CrFeCo x CuNiTi high-entropy alloy coating in alkaline solution and salt solution [J]. Results Phys., 2019, 12: 1737
|
71 |
Qiu X W , Liu C G . Microstructure and properties of Al2CrFeCoCuTiNi x high-entropy alloys prepared by laser cladding [J]. J. Alloys Compd., 2013, 553: 216
|
72 |
Meghwal A , Anupam A , Murty B S , et al . Thermal spray high-entropy alloy coatings: A review [J]. J. Therm. Spray Technol., 2020, 29: 857
|
73 |
Wang W R , Qi W , Xie L , et al . Microstructure and corrosion behavior of (CoCrFeNi)95Nb5 high-entropy alloy coating fabricated by plasma spraying [J]. Materials, 2019, 12: 694
|
74 |
Vallimanalan A , Kumaresh Babu S P , Muthukumaran S , et al . Corrosion behaviour of thermally sprayed Mo added AlCoCrNi high entropy alloy coating [J]. Mater. Today: Proc., 2020, 27: 2398
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|