| 厚度对Bi薄膜表面特性和电学性质的影响 |
董彩虹1, 刘永利2, 祁阳2( ) |
1 东北大学理学院 沈阳 110819 2 东北大学材料科学与工程学院 沈阳 110819 |
|
| Effect of Thickness on the Surface and Electronic Properties of Bi Film |
Caihong DONG1, Yongli LIU2, Yang QI2( ) |
1 College of Science, Northeastern University, Shenyang 110819, China 2 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China |
引用本文:
董彩虹, 刘永利, 祁阳. 厚度对Bi薄膜表面特性和电学性质的影响[J]. 金属学报, 2018, 54(6): 935-942.
Caihong DONG,
Yongli LIU,
Yang QI.
Effect of Thickness on the Surface and Electronic Properties of Bi Film[J]. Acta Metall Sin, 2018, 54(6): 935-942.
| [1] | Özçelik V O, Aktürk O Ü, Durgun E, et al.Prediction of a two-dimensional crystalline structure of nitrogen atoms[J]. Phys. Rev., 2015, 92B: 125420 | | [2] | Li L K, Yu Y J, Ye G J, et al.Black phosphorus field-effect transistors[J]. Nat. Nanotechnol., 2014, 9: 372 | | [3] | Zhu Z, Tománek D.Semiconducting layered blue phosphorus: A computational study[J]. Phys. Rev. Lett., 2014, 112: 176802 | | [4] | Kamal C, Ezawa M.Arsenene: Two-dimensional buckled and puckered honeycomb arsenic systems[J]. Phys. Rev., 2015, 91B: 085423 | | [5] | Aktürk O Ü, Özçelik V O, Ciraci S.Single-layer crystalline phases of antimony: Antimonenes[J]. Phys. Rev., 2015, 91B: 235446 | | [6] | Zhang S L, Yan Z, Li Y F, et al.Atomically thin arsenene and antimonene: Semimetal-semiconductor and indirect-direct band-gap transitions[J]. Angew. Chem. Int. Ed., 2015, 54: 3112 | | [7] | Ast C R, Höchst H.Electronic structure of a bismuth bilayer[J]. Phys. Rev., 2003, 67B: 113102 | | [8] | Hofmann P, Gayone J E, Bihlmayer G, et al.Electronic structure and Fermi surface of Bi(100)[J]. Phys. Rev., 2005, 71B: 195413 | | [9] | Hirahara T, Nagao T, Matsuda I, et al.Role of spin-orbit coupling and hybridization effects in the electronic structure of ultrathin Bi films[J]. Phys. Rev. Lett., 2006, 97: 146803 | | [10] | Jnawali G, Klein C, Wagner T, et al.Manipulation of electronic transport in the Bi(111) surface state[J]. Phys. Rev. Lett., 2012, 108: 266804 | | [11] | Yang J, Huang G Q, Zhu X F.Thickness evolution of phonon properties in ultrathin Bi(111) films[J]. Phys. Status Solidi, 2013, 250B: 1937 | | [12] | Koroteev Y M, Bihlmayer G, Gayone J E, et al.Strong spin-orbit splitting on Bi surfaces[J]. Phys. Rev. Lett., 2004, 93: 046403 | | [13] | Tichovolsky E J, Mavroides J G.Magnetoreflection studies on the band structure of bismuth-antimony alloys[J]. Solid State Commun., 1969, 7: 927 | | [14] | Ohtsubo Y, Perfetti L, Goerbig M O, et al.Non-trivial surface-band dispersion on Bi(111)[J]. New J. Phys., 2013, 15: 033041 | | [15] | Liu Z, Liu C X, Wu Y S, et al.Stable nontrivial Z2 topology in ultrathin Bi(111) films: A first-principles study[J]. Phys. Rev. Lett., 2011, 107: 136805 | | [16] | Murakami S.Quantum spin hall effect and enhanced magnetic response by spin-orbit coupling[J]. Phys. Rev. Lett., 2006, 97: 236805 | | [17] | Wada M, Murakami S, Freimuth F, et al.Localized edge states in two-dimensional topological insulators: Ultrathin Bi films[J]. Phys. Rev., 2011, 83B: 121310 | | [18] | Sun J, Mikkelsen A, Jensen M F, et al.Structural determination of the Bi(110) semimetal surface by LEED analysis and ab initio calculations[J]. Phys. Rev., 2006, 74B: 245406 | | [19] | Koroteev Y M, Bihlmayer G, Chulkov E V, et al.First-principles investigation of structural and electronic properties of ultrathin Bi films[J]. Phys. Rev., 2008, 77B: 045428 | | [20] | Nagao T, Sadowski J T, Saito M, et al.Nanofilm allotrope and phase transformation of ultrathin Bi film on Si(111)-7×7[J]. Phys. Rev. Lett., 2004, 93: 105501 | | [21] | Krenzer B, Hanisch-Blicharski A, Schneider P, et al.Phonon confinement effects in ultrathin epitaxial bismuth films on silicon studied by time-resolved electron diffraction[J]. Phys. Rev., 2009, 80B: 024307 | | [22] | Kresse G, Furthmüller J.Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set[J]. Phys. Rev., 1996, 54B: 11169 | | [23] | Aguilera I, Friedrich C, Blügel S.Electronic phase transitions of bismuth under strain from relativistic self-consistent GW calculations[J]. Phys. Rev., 2015, 91B: 125129 | | [24] | Blöchl P E.Projector augmented-wave method[J]. Phys. Rev., 1994, 50B: 17953 | | [25] | Perdew J P, Burke K, Ernzerhof M.Generalized gradient approximation made simple[J]. Phys. Rev. Lett., 1996, 77: 3865 | | [26] | Qi J S, Shi D N, Zhao J J, et al.Stable structures and electronic properties of the oriented Bi nanowires and nanotubes from first-principle calculations[J]. J. Phys. Chem., 2008, 112C: 10746 | | [27] | Aktürk E, Aktürk O Ü, Ciraci S.Single and bilayer bismuthene: Stability at high temperature and mechanical and electronic properties[J]. Phys. Rev., 2016, 94B: 014115 | | [28] | Mönig H, Sun J, Koroteev Y M, et al.Structure of the (111) surface of bismuth: LEED analysis and first-principles calculations[J]. Phys. Rev., 2005, 72B: 085410 | | [29] | Hirahara T, Nagao T, Matsuda I, et al.Quantum well states in ultrathin Bi films: angle-resolved photoemission spectroscopy and first-principles calculations study[J]. Phys. Rev., 2007, 75B: 035422 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|