| 电流强度对冷坩埚定向凝固Ni3Al金属间化合物微观组织的影响 |
王国田, 丁宏升( ), 陈瑞润, 郭景杰, 傅恒志 |
| 哈尔滨工业大学材料科学与工程学院金属精密热加工国家重点实验室 哈尔滨 150001 |
|
| Effect of Current Intensity on Microstructure of Ni3Al Intermetallics Prepared by Directional Solidification Electromagnetic Cold Crucible Technique |
Guotian WANG, Hongsheng DING( ), Ruirun CHEN, Jingjie GUO, Hengzhi FU |
| National Key Laboratory for Precision Hot Processing of Metals, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China |
引用本文:
王国田, 丁宏升, 陈瑞润, 郭景杰, 傅恒志. 电流强度对冷坩埚定向凝固Ni3Al金属间化合物微观组织的影响[J]. 金属学报, 2017, 53(11): 1461-1468.
Guotian WANG,
Hongsheng DING,
Ruirun CHEN,
Jingjie GUO,
Hengzhi FU.
Effect of Current Intensity on Microstructure of Ni3Al Intermetallics Prepared by Directional Solidification Electromagnetic Cold Crucible Technique[J]. Acta Metall Sin, 2017, 53(11): 1461-1468.
| [1] | Raju S V, Oni A A, Godwal B K, et al.Effect of B and Cr on elastic strength and crystal structure of Ni3Al alloys under high pressure[J]. J. Alloys Compd., 2015, 619: 616 | | [2] | Ivanovski V N, Umi?evi? A, Belo?evi?-?avor J, et al. Local structure study of Fe dopants in Ni-deficit Ni3Al alloys[J]. J. Alloys Compd., 2015, 651: 705 | | [3] | Zhang H J, Xiao J F, Wen W D, et al.Study on a statistical unit cell model for Ni3Al-base superalloy[J]. Mech. Mater., 2016, 98: 1 | | [4] | Liu W, Krol T, Nembach E.Precipitation strengthening, yield stress anomaly and strain rate sensitivity of an L12-ordered intermetallic (Ni, Co)3(Al, Ti) alloy[J]. Scr. Mater., 1998, 39: 1419 | | [5] | Sun B D, Li D Q, Xu Y, et al.The effects of RE on as cast morphology of (NiAl+Ni3Al) intermetallics[J]. J. Shanghai Jiaotong Univ., 1997, 31(1): 83(孙宝德, 郦定强, 徐颍等. 稀土对(NiAl+Ni3Al)双相区金属间化合物铸态组织的影响[J]. 上海交通大学学报, 1997, 31(1): 83) | | [6] | Peng P, Zhou Z, Xie Q, et al.Development of rapidly solidified NiAlFe based shape memory alloys[J]. Mater. Rev., 1996, (3): 20(彭平, 周征, 谢泉等. 快速凝固NiAlFe系形状记忆合金的研究进展[J]. 材料导报, 1996, (3): 20) | | [7] | Taniguchi S, Yasuda H, Takatani K.Preface to the special issue on “advanced application of electromagnetic force to materials processing”[J]. ISIJ Int., 2003, 43: 799 | | [8] | Feonychev A I, Bondareva N V.Effect of a rotating magnetic field on convection stability and crystal growth in zero gravity and on the ground[J]. J. Eng. Phys. Thermophys., 2003, 77: 731 | | [9] | Misra A K.A novel solidification technique of metals and alloys: Under the influence of applied potential[J]. Metall. Trans., 1985, 16A: 1354 | | [10] | Misra A K.Misra technique1 applied to solidification of cast iron[J]. Metall. Trans., 1986, 17A: 358 | | [11] | Ahmed S, Bond R, McKannan E C. Solidification processing superalloys in an electric field[J]. Adv. Mater. Proc., 1991, 140: 30 | | [12] | Ahmed S, McKannan E. Control of γ' morphologyin nickel base superalloys through alloy design and densification processing under electric field[J]. Mater. Sci. Technol., 1994, 10: 941 | | [13] | Ding H S, Zhang Y, Jiang S Y, et al.Influences of pulse electric current treatment on solidification microstructures and mechanical properties of Al-Si piston alloys[J]. China Foundry, 2009, 6: 24 | | [14] | Wang J, Yin J J, Ding Y T, et al.Effect of direct current electric field on the microstructure of ZA27 alloy[J]. Foundry, 2003, 52: 84(王劲, 尹建军, 丁雨田等. 直流电场对ZA27合金凝固组织的影响[J]. 铸造, 2003, 52: 84) | | [15] | Pfann W G, Wagner R S.Principles of field freezing[J]. Trans. Metall. Soc. AIME, 1962, 224: 1139 | | [16] | Xu Q G, Wu B L, Wan G, et al.Effect of direct current electric fieid on structure of directionally solidified Al-4.5%Cu alloy[J]. J. Aeronaut. Mater., 2006, 26(1): 16(徐前刚, 武保林, 万刚等. 直流电场对Al-4.5%Cu合金定向凝固组织的影响[J]. 航空材料学报, 2006, 26(1): 16) | | [17] | Guo F J, Li L Z, Cang D Q, et al.Solute activity change model of binary liquid alloys in electrical field[J]. J. Univ. Sci. Technol. Beijing, 2005, 27: 27(郭发军, 李玲珍, 苍大强等. 电场作用下二元液态合金中溶质活度变化理论模型[J]. 北京科技大学学报, 2005, 27: 27) | | [18] | Chang G W, Yuan Y J, Wang Z D, et al.Effect of electric current density on columnar crystal spacing during continuous unidirectional solidification[J]. Acta Metall. Sin., 2000, 36: 30(常国威, 袁永军, 王自东等. 电流密度对定向凝固组织中柱状晶间距的影响[J]. 金属学报, 2000, 36: 30) | | [19] | Li W F, Yang Y S, Yu L, et al.Effect of direct current electric field on the microstructure of nickel-based superalloy K417G[J]. J. Mater. Eng., 2001, (9): 7(李万锋, 杨院生, 于力等. 直流电场作用对K417G镍基高温合金凝固组织的影响[J]. 材料工程, 2001, (9): 7) | | [20] | Prodhan A, Sanyal D.Cooling curves analysis of aluminium solidified without and with magnetic or electric field[J]. J. Mater. Sci. Lett., 1997, 16: 958 | | [21] | ?ad?rl? E, Kaya H, Gündüz M.Effect of growth rates and temperature gradients on the lamellar spacing and the undercooling in the directionally solidified Pb-Cd eutectic alloy[J]. Mater. Res. Bull., 2003, 38: 1457 | | [22] | B?yük U, Mara?l? N, Kaya H, et al.Directional solidification of Al-Cu-Ag alloy[J]. Appl. Phys., 2009, 95A: 923 | | [23] | Tian S.The Physical Properties of Materials [M]. Beijing: Beihang University Press, 2004: 38(田莳. 材料物理性能 [M]. 北京: 北京航空航天大学出版社, 2004: 38) | | [24] | Fu D J, Huang L G, Li S.Effect of DC electric field on microstructure and properties of Al-5Fe based alloy[J]. Ordnance Mater. Sci. Eng., 2013, 36(5): 46(付大军, 黄立国, 李爽. 直流电场对Al-5Fe基合金组织和性能的影响[J]. 兵器材料科学与工程, 2013, 36(5): 46) | | [25] | He S X, Wang J, Zhou Y H.Application of electric current during metal solidification process[J]. Spec. Casting Nonferrous Alloys, 2001, (5): 28(何树先, 王俊, 周尧和. 电流在金属凝固过程中的应用[J]. 特种铸造及有色合金, 2001, (5): 28) | | [26] | Liu J, Li Z H, Cen Q H, et al.Effect of external electric field on solidification structure of alloy[J]. Foundry, 2012, 61: 877(刘瑾, 黎振华, 岑启宏等. 外加电场对合金凝固组织的影响[J]. 铸造, 2012, 61: 877) | | [27] | Wiegel M E K, Matthiesen D H. Determination of the peltier coe-fficient of germanium in a vertical Bridgman-Stockbarger furnace[J]. J. Cryst. Growth, 1997, 174: 194 | | [28] | Corre S, Duffar T, Bernard M, et al.Numerical simulation and validation of the Peltier pulse marking of solid/liquid interfaces[J]. J. Cryst. Growth, 1997, 180: 604 | | [29] | Huang L G, Fu D J, Gao Z Y.Application of continuous electric field in metal solidification[J]. J. Mater. Eng., 2011, (4): 94(黄立国, 付大军, 高志玉. 连续电流场在金属凝固过程中的应用研究[J]. 材料工程, 2011, (4): 94) | | [30] | Gu G D, Xu Y Y, An G Y, et al.Cellular growth of Sn-5%Bi alloy in electric field[J]. Chin. J. Mech. Eng., 1991, 27(5): 37(顾根大, 徐雁允, 安阁英等. 电场作用下Sn-5%Bi合金的胞晶生长[J]. 机械工程学报, 1991, 27(5): 37) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|