| Mn18Cr18N奥氏体不锈钢的压缩拉伸连续加载变形行为* |
李飞,张华煜,何文武,陈慧琴( ),郭会光 |
| 太原科技大学材料科学与工程学院, 太原 030024 |
|
| COMPRESSION AND TENSILE CONSECUTIVE DEFORMATION BEHAVIOR OF Mn18Cr18N AUSTENITE STAINLESS STEEL |
Fei LI,Huayu ZHANG,Wenwu HE,Huiqin CHEN( ),Huiguang GUO |
| School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China |
引用本文:
李飞,张华煜,何文武,陈慧琴,郭会光. Mn18Cr18N奥氏体不锈钢的压缩拉伸连续加载变形行为*[J]. 金属学报, 2016, 52(8): 956-964.
Fei LI,
Huayu ZHANG,
Wenwu HE,
Huiqin CHEN,
Huiguang GUO.
COMPRESSION AND TENSILE CONSECUTIVE DEFORMATION BEHAVIOR OF Mn18Cr18N AUSTENITE STAINLESS STEEL[J]. Acta Metall Sin, 2016, 52(8): 956-964.
| [1] | Gavriljuk V G, Berns H.High Nitrogen Steels: Structures, Properties, Manufacture, Apllicantions. Berlin: Springer, 1999: 271 | | [2] | Wang Z H, Fu W T, Sun S H, Lv Z Q, Zhang W H.J. Mater Sci Technol, 2010; 26: 798 | | [3] | Lee T H, Oh C S, Kim S J, Takaki S.Acta Mater, 2007; 55: 3649 | | [4] | Stein G, Hucklenbroich I, Feichtinger H. Mater Sci Forum, 1999; 318~320: 151 | | [5] | Mao G G.Electric Power, 2006; 39(7): 15 | | [5] | (毛国光. 中国电力, 2006; 39(7): 15) | | [6] | Jiang Z H, Liu X H, Zhao L.Special Steel, 1999; 20(special issue): 82 | | [6] | (姜周华, 刘喜海, 赵林. 特殊钢, 1999; 20(特刊): 82) | | [7] | Peng X H, Gao Z H, Ma M T, Yan Z X.Acta Metall Sin, 1993; 29: 429 | | [7] | (彭向和, 高芝晖, 马鸣图, 颜在先. 金属学报, 1993; 29: 429) | | [8] | Wang Y Q, Chang T, Shi Y J.J Southeast Univ (Nat Sci Ed), 2012; 42: 1175 | | [8] | (王元清, 常婷, 石永久. 东南大学学报(自然科学版), 2012; 42: 1175) | | [9] | Shi G, Wang F, Dai G X, Wang Y Q, Shi Y J.J Southeast Univ (Nat Sci Ed), 2011; 41: 1259 | | [9] | (施刚, 王飞, 戴国欣, 王元清, 石永久. 东南大学学报(自然科学版), 2011; 41: 1259) | | [10] | Dusicka P, Itani A M, Buckle I G.J Constr Steel Res, 2007; 63(2): 156 | | [11] | Wu Q, Chen Y Y, Zhou F.J Build Struct, 2014; 35(2): 89 | | [11] | (吴旗, 陈以一, 周锋. 建筑结构学报, 2014; 35(2): 89) | | [12] | Soppa E A, Kohler C, Roos E.Mater Sci Eng, 2014; A597: 128 | | [13] | Mishra A, Chellapandi P, Kumar R S, Sasikala G.Trans Indian Inst Met, 2015; 68: 623 | | [14] | Eisenmeier G, Holzwarth B, Hoppel H W, Mughrabi H.Mater Sci Eng, 2001; A319: 578 | | [15] | Yin S M, Yang H J, Li S X, Wu S D, Yang F.Scr Mater, 2008; 58: 751 | | [16] | Mo D F, He G Q, Zhu Z Y, Liu X S, Zhang W H,Acta Metall Sin, 2009; 45: 861 | | [16] | (莫德峰, 何国球, 朱正宇, 刘晓山, 张卫华. 金属学报, 2009; 45: 861) | | [17] | Zhang K S, Dong S H, Xu L B, Huang S H, Yuan Q P.Chin J Solid Mech, 2013; 34: 450 | | [17] | (张克实, 董书惠, 许凌波, 黄世鸿, 袁秋平. 固体力学学报, 2013; 34: 450) | | [18] | Shin J H, Lee J W.Mater Charact, 2014; 91(5): 19 | | [19] | Kocks U F,Philos Mag, 1966; 13: 541 | | [20] | Fletham P, Meakin J D.Acta Metall, 1957; 5: 555 | | [21] | Argon A S.Strengthening Mechanisms in Crystal Plasticity. New York: Oxford University Press, 2008: 283 | | [22] | Wang S T, Yang K, Shan Y Y, Li L F.Acta Metall Sin, 2007; 43: 713 | | [22] | (王松涛, 杨柯, 单以银, 李来风. 金属学报, 2007; 43: 713) | | [23] | Lou C, Zhang X Y, Wang R H, Duan G L, Liu Q.Acta Metall Sin, 2013; 49: 291 | | [23] | (娄超, 张喜燕, 王润红, 段高林, 刘庆. 金属学报, 2013; 49: 291) | | [24] | Wang Y Y, Sun X, Wang Y D, Hu X H, Zbib H M.Mater Sci Eng, 2014; A607: 206 | | [25] | Shi D K, Liu J H.Acta Metall Sin, 1989; 25: 282 | | [25] | (石德珂, 刘军海. 金属学报, 1989; 25: 282) | | [26] | Chen Y Y, Zheng Z Q, Cai B, Xu J Q, She L J, Li H.Rare Met Mater Eng, 2011; 40: 1926 | | [26] | (陈圆圆, 郑子樵, 蔡彪, 徐建秋, 佘玲娟, 李海. 稀有金属材料与工程, 2011, 40: 1926) |
|
|