| 高温短时间时效处理对Mg-3Nd-1Zn合金微观组织及力学性能的影响* |
王文辉1,2,吴迪1( ),陈荣石1,娄长胜2 |
1 中国科学院金属研究所, 沈阳 110016 2 沈阳理工大学材料科学与工程学院, 沈阳 110159 |
|
| EFFECTS OF HIGH TEMPERATURE SHORT TIMEAGEING TREATMENT ON THE MICROSTRUC-TURES AND MECHANICAL PROPERTIES OFMg-3Nd-1Zn ALLOY |
Wenhui WANG1,2,Di WU1( ),Rongshi CHEN1,Changsheng LOU2 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, Shenyang Ligong University, Shenyang 110159, China |
引用本文:
王文辉,吴迪,陈荣石,娄长胜. 高温短时间时效处理对Mg-3Nd-1Zn合金微观组织及力学性能的影响*[J]. 金属学报, 2016, 52(5): 567-574.
Wenhui WANG,
Di WU,
Rongshi CHEN,
Changsheng LOU.
EFFECTS OF HIGH TEMPERATURE SHORT TIMEAGEING TREATMENT ON THE MICROSTRUC-TURES AND MECHANICAL PROPERTIES OFMg-3Nd-1Zn ALLOY[J]. Acta Metall Sin, 2016, 52(5): 567-574.
| [1] | Nie J F, Muddle B C.Acta Mater, 2000; 48: 1691 | | [2] | Wang X N, Han L Z, Gu J F.Acta Metall Sin, 2014; 50: 355 | | [2] | (王小娜, 韩利战, 顾剑锋. 金属学报, 2014; 50: 355) | | [3] | Liu Q.Acta Metall Sin, 2010; 46: 1458 | | [3] | (刘庆. 金属学报, 2010; 46: 1458) | | [4] | Tang W, Han E H, Xu Y B, Liu L.Acta Metall Sin, 2005; 41: 1199 | | [4] | (唐伟, 韩恩厚, 徐永波, 刘路. 金属学报, 2005; 41: 1199) | | [5] | Li D J, Wang Q D.Mater Sci Eng, 2009; A526: 150 | | [6] | Liu X B, Chen R S, Han E H.Mater Sci Eng, 2008; A497: 326 | | [7] | Li J H, Sha G, Wang T Y, Jie W Q, Ringer S P.Mater Sci Eng, 2012; A534: 1 | | [8] | Liu H, Gao Y, Zhu Y M, Wang Y, Nie J F.Acta Mater, 2014; 77: 133 | | [9] | Fu P H, Peng L M, Jiang H Y, Ma L, Zhai C Q.Mater Sci Eng, 2008; A496: 177 | | [10] | Dai J, Huang J, Li M, Li Z, Dong J, Wu Y.Mater Sci Eng, 2011; A529: 401 | | [11] | Ma L, Mishra R K, Balogh M P, Peng L, Luo A A, Sachdev A K, Ding W.Mater Sci Eng, 2012; A543: 12 | | [12] | Wu D, Chen R S, Ke W.Mater Des, 2014; 58: 324 | | [13] | Zheng X W, Dong J, Zhou N, Fu P H, Yao S S, Ding W J.Mater Sci Technol, 2011; 27: 275 | | [14] | Ning Z L, Wang G J, Cao F Y, Sun J F, Du J F.J Mater Sci, 2009; 44: 4264 | | [15] | Wang K F, Zhou Z J, Wang Y C, Mi G F.Hot Working Technol, 2011; 40: 39 | | [16] | Wang W H, Wu D, Shah S S A, Chen R S, Lou C S.Mater Sci Eng, 2016; A649: 214 | | [17] | Nie J F.Metall Mater Trans, 2012; 43A: 3891 | | [18] | Pike T J, Noble B.J Less Common Met, 1973; 30: 63 | | [19] | Fu P H, Peng L M, Jiang H Y, Chang T W, Zhai C Q.Mater Sci Eng, 2008; A486: 183 | | [20] | Wang W H, Wu D, Chen R S, Lou C S.Mater Sci Forum, 2015; 816: 362 | | [21] | Zhu S M, Nie J F.Scr Mater, 2004; 50: 51 | | [22] | Wei L Y, Dunlop G L, Westengen H. J Mater Sci, 1996; 31: 387 | | [23] | Ardell A J.Metall Trans, 1985; 16A: 2131 | | [24] | Nie J F.Scr Mater, 2003; 48: 1009 | | [25] | Cui Z Q.Metallography and Heat Treatment. Harbin: China Machine Press, 2007: 175 | | [25] | (崔忠圻. 金属学与热处理. 哈尔滨: 机械工业出版社, 2007: 175) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|