| 低合金多相钢中残余奥氏体对塑性和韧性的影响* |
谢振家,尚成嘉( ),周文浩,吴彬彬 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| EFFECT OF RETAINED AUSTENITE ON DUCTILITY AND TOUGHNESS OF A LOW ALLOYED MULTI-PHASE STEEL |
Zhenjia XIE,Chengjia SHANG( ),Wenhao ZHOU,Binbin WU |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
谢振家,尚成嘉,周文浩,吴彬彬. 低合金多相钢中残余奥氏体对塑性和韧性的影响*[J]. 金属学报, 2016, 52(2): 224-232.
Zhenjia XIE,
Chengjia SHANG,
Wenhao ZHOU,
Binbin WU.
EFFECT OF RETAINED AUSTENITE ON DUCTILITY AND TOUGHNESS OF A LOW ALLOYED MULTI-PHASE STEEL[J]. Acta Metall Sin, 2016, 52(2): 224-232.
| [1] | Weng Y Q, Yang C F, Shang C J.Iron Steel, 2011; (9): 1 | | [1] | (翁宇庆, 杨才福, 尚成嘉. 钢铁, 2011; (9): 1) | | [2] | Wang X M, Shang C J, Yang S W.Acta Metall Sin, 2005; 41: 1256 | | [2] | (王学敏, 尚成嘉, 杨善武. 金属学报, 2005; 41: 1256) | | [3] | Wang X M, Shang C J, Yang S W, He X L, Liu X Y. Mater Sci Eng, 2006; A438-440: 162 | | [4] | Shu W, Wang X M, Li S R, He X L.Acta Metal Sin, 2011; 47: 435 | | [4] | (舒玮, 王学敏, 李书瑞, 贺信莱. 金属学报, 2011; 47: 435) | | [5] | Sakuma Y, Matsumura O, Takechi H.Metall Mater Trans, 1991; 22A: 489 | | [6] | Herrera C, Ponge D, Raabe D.Acta Mater, 2011; 59: 4653 | | [7] | Zhou W H, Guo H, Xie Z J, Wang X M, Shang C J.Mater Sci Eng, 2013; A587: 365 | | [8] | Zackay V F, Parker E R, Fahr D, Busch R.ASM Trans Quart, 1967; 60: 252 | | [9] | Allaina S, Chateau J P, Bouaziz O. Mater Sci Eng, 2004; A387-389: 143 | | [10] | Bouaziza O, Allain S, Scott C P, Cugy P, Barbier D.Curr Opin Solid State Mater Sci, 2011; 15(4): 141 | | [11] | Lei M, Guo Y Y.Acta Metall Sin (Engl Lett), 1989; 2: 244 | | [12] | Fultz B, Kim J I, Kim Y H, Kim H J, Fior G O, Morris J W Jr.Metall Trans, 1985; 16A: 2237 | | [13] | Xu L S, Yu W, Zhang Y M, Lu X J.J Univ Sci Technol Beijing, 2012; 34: 125 | | [13] | (徐立善, 余伟, 张烨铭, 卢小节. 北京科技大学学报, 2012; 34: 125) | | [14] | Xie Z J, Yuan S F, Zhou W H, Yang J R, Guo H, Shang C J.Mater Des, 2014; 59: 193 | | [15] | You Y, Shang C J, Chen L, Subramanian S.Mater Sci Eng, 2012; A546: 111 | | [16] | Santofimia M J, Nguyen-Minh T, Zhao L, Petrovb R, Sabirovd I, Sietsmab J.Mater Sci Eng, 2010; A527: 6429 | | [17] | Jacques P, Delannay F, Cornet X, Harlet P, Ladriere J.Metall Mater Trans, 1998; 29A: 2383 | | [18] | Colla V, DeSanctis M, Dimatteo A, Lovicu G, Solina A, Valentini R.Metall Mater Trans, 2009; 40A: 2557 | | [19] | Shi J, Sun X J, Wang M Q, Hui W J, Dong H, Cao W Q.Scr Mater, 2010; 63: 815 | | [20] | Ren Y Q, Xie Z J, Zhang H W, Yuan S F, Song T T, Shang C J.Acta Metall Sin, 2013; 49: 1558 | | [20] | (任勇强, 谢振家, 张宏伟, 袁胜福, 宋婷婷, 尚成嘉. 金属学报, 2013; 49: 1558) | | [21] | Wang Y, Zhang K, Guo Z H, Chen N L, Rong Y H.Acta Metall Sin, 2012; 48: 641 | | [21] | (王颖, 张柯, 郭正洪, 陈乃录, 戎咏华. 金属学报, 2012; 48: 641) | | [22] | Xie Z J, Ren Y Q, Zhou W H, Yang J R, Shang C J, Misra R D K.Mater Sci Eng, 2014; A603: 69 | | [23] | Brophy G R, Miller A J.Trans ASM, 1949; 41: 1185 | | [24] | Tamate O.Int J Fract Mech, 1968; 4: 257 | | [25] | Rack H J, Kalish D.Metall Trans, 1971; 2: 3011 | | [26] | Ahlquist C N.Acta Metall, 1975; 23: 239 | | [27] | Syn C K, Fultz B, Morris J W Jr.Metall Trans, 1978; 9A: 1735 | | [28] | Fultz B, Morris J W Jr.Metall Trans, 1985; 16A: 173 | | [29] | Antolovich S D, Singh B.Metall Trans, 1971; 2: 2135 | | [30] | Lai G Y, Wood W E, Clark R A, Zackay V F, Parker E R.Metall Trans, 1974; 5: 1663 | | [31] | Kim K J, Schwartz L H.Mater Sci Eng, 1978; 33: 5 | | [32] | Kang J, Wang C, Wang G D.Mater Sci Eng, 2012; A553: 96 | | [33] | Santofimia M J, Zhao L, Sietsmab J.Metall Mater Trans, 2009; 40A: 46 | | [34] | Cullity B D.Elements of X-ray Diffraction. Massachusetts: Addison-Wesley, 1978: 359 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|