| 新型高氮钢的腐蚀和空蚀交互作用研究* |
乔岩欣1( ),王硕1,刘彬1,郑玉贵2,李花兵3,姜周华3 |
1 江苏科技大学材料科学与工程学院, 镇江 212003 2 中国科学院金属研究所, 沈阳 110016 3 东北大学冶金学院, 沈阳110819 |
|
| SYNERGISTIC EFFECT OF CORROSION AND CAVITATION EROSION OF HIGH NITROGEN STAINLESS STEEL |
Yanxin QIAO1( ),Shuo WANG1,Bin Liu1,Yugui ZHENG2,Huabing LI3,Zhouhua JIANG3 |
1 Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3 School of Metallurgy, Northeastern University, Shenyang 110819, China |
引用本文:
乔岩欣,王硕,刘彬,郑玉贵,李花兵,姜周华. 新型高氮钢的腐蚀和空蚀交互作用研究*[J]. 金属学报, 2016, 52(2): 233-240.
Yanxin QIAO,
Shuo WANG,
Bin Liu,
Yugui ZHENG,
Huabing LI,
Zhouhua JIANG.
SYNERGISTIC EFFECT OF CORROSION AND CAVITATION EROSION OF HIGH NITROGEN STAINLESS STEEL[J]. Acta Metall Sin, 2016, 52(2): 233-240.
| [1] | Yu H.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007 | | [1] | (于宏. 中国科学院金属研究所博士学位论文, 沈阳, 2007) | | [2] | Luo S Z, Zheng Y G, Li M C, Yao Z M, Ke W.Corrosion, 2003; 59: 597 | | [3] | Tomlinson W J, Talks M G.Tribol Int, 1991; 24: 67 | | [4] | Bregliozzia G, Di-Schino A, Ahmed S I U, Kenny J M, Haefke H.Wear, 2005; 258: 503 | | [5] | Kwok C T, Man H C, Leung L K.Wear, 1997; 211: 84 | | [6] | Ogino K, Hida A, Kishima S.Corrosion, 1988; 44: 97 | | [7] | Fu W T, Zheng Y Z, Jing T F, Yao M.Wear, 1997; 205: 28 | | [8] | Fu W T, Zheng Y Z, Jing T F, Yao M. Wear, 2001; 249: 788 | | [9] | Mills D J, Knutsen R D.Wear, 1998; 215: 83 | | [10] | Liu W.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2001 | | [10] | (柳伟. 中国科学院金属研究所博士学位论文, 沈阳, 2001) | | [11] | Luo S Z.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2003 | | [11] | (骆素珍. 中国科学院金属研究所博士学位论文, 沈阳, 2003) | | [12] | Zheng Y G, Luo S Z, Ke W.Tribol Int, 2008; 41: 1181 | | [13] | Qiao Y X, Zheng Y G, Wu X Q, Ke W, Yang K, Jiang Z H.Tribol Mater Surf Int, 2007; 1: 165 | | [14] | Hoeppner D W, Goss G L.Wear, 1974; 27: 61 | | [15] | Zheng Y G, Luo S Z, Ke W.Wear, 2007; 262: 1308 | | [16] | Luo S Z, Zheng Y G, Liu W, Jing H M, Yao Z M, Ke W. J Mater Sci Technol, 2003; 19: 346 | | [17] | Al-Hashem A, Caceres P G, Abdullah A, Shalaby H M.Corrosion, 1997; 52: 103 | | [18] | Liu W, Zheng Y G, Liu C S, Yao Z M, Ke W.Wear, 2003; 254: 713 | | [19] | Mesa D H, Garzón C M, Tschiptschin A P.Wear, 2011; 271: 1372 | | [20] | Santos J F, Garzón C M, Tschiptschin A P.Mater Sci Eng, 2004; A382: 378 | | [21] | Kwok C T, Man H C, Cheng F T.Mater Sci Eng, 1998; A242: 108 | | [22] | Engelberg G, Yahalom J.Corros Sci, 1972; 12: 469 | | [23] | Zheng Y G, Yao Z M, Zhang Y S, Wei X Y, Ke W.Acta Metall Sin, 2000; 36: 51 | | [23] | (郑玉贵, 姚治铭, 张玉生, 魏翔云, 柯伟. 金属学报, 2000: 36: 51) | | [24] | Kwok C T, Cheng F T, Man H C.Mater Sci Eng, 2000; A290: 145 | | [25] | Zheng Y G, Yao Z M, Wei X Y, Ke W. Wear, 1995; 186-187: 555 | | [26] | Feng D.Physics of Metals. Beijing: Science Press, 1999: 1 | | [26] | (冯端. 金属物理. 北京:科学出版社, 1999: 1) | | [27] | Qiao L J, Chu W Y, Mao X.Corrosion, 1996; 52: 275 | | [28] | Chu W, Liu T, Hsiao C, Li S. Corrosion, 1981; 37: 320 |
|
|