| 一种新型镍基合金在超临界多种离子共存环境下的腐蚀行为* |
欧美琼1,2,刘扬3,查向东1,马颖澈1,4( ),程乐明3,刘奎1 |
1 中国科学院金属研究所, 沈阳 110016 2 中国科学技术大学材料科学与工程学院, 合肥 230026 3 新奥科技发展有限公司煤基低碳能源国家重点实验室, 廊坊 065001 4 江苏图南合金股份有限公司, 丹阳 212352 |
|
| CORROSION BEHAVIOR OF A NEW NICKEL BASE ALLOY IN SUPERCRITICAL WATERCONTAINING DIVERSE IONS |
Meiqiong OU1,2,Yang LIU3,Xiangdong ZHA1,Yingche MA1,4( ),Leming CHENG3,Kui LIU1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Hefei 230026, China 3 State Key Laboratory of Coal-Based Low Carbon Energy, ENN Science and Technology Development Co., Ltd. Langfang 065001, China 4 Jiangsu Toland Alloy Co., Danyang 212352, China |
引用本文:
欧美琼,刘扬,查向东,马颖澈,程乐明,刘奎. 一种新型镍基合金在超临界多种离子共存环境下的腐蚀行为*[J]. 金属学报, 2016, 52(12): 1557-1564.
Meiqiong OU,
Yang LIU,
Xiangdong ZHA,
Yingche MA,
Leming CHENG,
Kui LIU.
CORROSION BEHAVIOR OF A NEW NICKEL BASE ALLOY IN SUPERCRITICAL WATERCONTAINING DIVERSE IONS[J]. Acta Metall Sin, 2016, 52(12): 1557-1564.
| [1] | Chen Z, Wang G W, Yin F J, Chen H Z, Xu Y J.Chem Eng J, 2015; 269: 343 | | [2] | Kritzer P, Dinjus E.Chem Eng J, 2001; 83: 207 | | [3] | Kritzer P.J Supercrit Fluids, 2004; 29: 1 | | [4] | Zhang Q, Tang R, Yin K J, Luo X, Zhang L F.Corros Sci, 2009; 51: 2092 | | [5] | Chang K H, Huang J H, Yan C B, Yeh T K, Chen F R, Kai J J.Prog Nucl Energy, 2012; 57: 20 | | [6] | Tang X Y, Wang S Z, Qian L L, Li Y H, Lin Z H, Xu D H, Zhang Y P.Chem Eng Res Des, 2015; 100: 530 | | [7] | Mitton D B, Orzalli J C, Latanision R M.ACS Symp Ser, 1995; 608: 327 | | [8] | Kim H J, Mitton D B, Latanision R M.Corros Sci, 2010; 52: 801 | | [9] | Marrone P A, Hong G T.J Supercrit Fluids, 2009; 51: 83 | | [10] | Gao X, Wu X Q, Zhang Z E, Guan H, Han E H.J Supercrit Fluids, 2007; 42: 157 | | [11] | Tan L, Ren X, Sridharan K, Allen T R.Corros Sci, 2008; 50: 3056 | | [12] | Sun M C, Wu X Q, Zhang Z E, Han E H. J Supercrit Fluids, 2008; 47: 309 | | [13] | Ma Y C, Zhao X J, Gao M, Liu K.J Mater Sci Technol, 2011; 27: 841 | | [14] | Zhao X, Zha X D, Liu Y, Zhang L, Liang T, Ma Y C, Cheng L M.Acta Metall Sin, 2015; 51: 249 | | [14] | (赵霞, 查向东, 刘扬, 张龙, 梁田, 马颖澈, 程乐明. 金属学报, 2015; 51: 249) | | [15] | Ren X, Sridharan K, Allen T R.Corrosion, 2007; 63: 603 | | [16] | Terachi T, Totsuka N, Yamada T, Nakagawa T, Deguchi H, Horiuchi M, Oshitani M.J Nucl Sci Technol, 2003; 40: 509 | | [17] | Chang K H, Chen S M, Yeh T K, Kai J J.Corros Sci, 2014; 81: 21 | | [18] | Otsuka N, Fujikawa H.Corrosion, 1991; 47: 240 | | [19] | Li H F, Fan H Y, Zhang Q, Qiu S Y, Wang J.Nucl Power Eng, 2011; 32(3): 38 | | [19] | (李海丰, 范洪远, 张强, 邱绍宇, 王均. 核动力工程, 2011; 32(3): 38) | | [20] | Liu Z H, Fang L, Tao H C.J Northeast Agric Univ, 2012; 43: 108 | | [20] | (刘振华, 方琳, 陶虎春. 东北农业大学学报, 2012; 43: 108) | | [21] | Zhu W, Xu Z R, Li L, He C.Chem Eng J, 2011; 171: 190 | | [22] | Machet A, Galtayries A, Marcus P, Combrade P, Jolivet P, Scott P.Surf Interface Anal, 2002; 34: 197 | | [23] | Biesinger M C, Brown C, Mycroft J R, Davidson R D, Mclntyre N S.Surf Interface Anal, 2004; 36: 1550 | | [24] | Zhang L, Han E-H, Zhang Z E, Guan H, Ke W.Acta Metall Sin, 2003; 39: 649(张丽, 韩恩厚, 张召恩, 关辉, 柯伟. 金属学报, 2003; 39: 649) | | [25] | Xu D H, Wang S Z, Zhang F, Huang C B, Tang X Y, Guo Y.Chem Ind Eng Prog, 2014; 33: 1015(徐东海, 王树众, 张峰, 黄传宝, 唐兴颖, 郭洋. 化工进展, 2014; 33: 1015) | | [26] | Zhong X Y, Wu X Q, Han E-H.Acta Metall Sin, 2011; 47: 932 | | [26] | (钟祥玉, 吴欣强, 韩恩厚. 金属学报, 2011; 47: 932) | | [27] | Ziemniak S E, Hanson M.Corros Sci, 2003; 45: 1595 | | [28] | Tan L, Ren X, Sridharan K, Allen T R.Corros Sci, 2008; 50: 2040 |
|
|