| 奥氏体不锈钢低温超饱和渗碳实验及热动力学模拟研究* |
荣冬松,姜勇,巩建鸣( ) |
| 南京工业大学机械与动力工程学院, 南京 211816 |
|
| EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL |
Dongsong RONG,Yong JIANG,Jianming GONG( ) |
| College of Mechanical and Power Engineering, Nanjing Tech University, Nanjing 211816 |
引用本文:
荣冬松,姜勇,巩建鸣. 奥氏体不锈钢低温超饱和渗碳实验及热动力学模拟研究*[J]. 金属学报, 2015, 51(12): 1516-1522.
Dongsong RONG,
Yong JIANG,
Jianming GONG.
EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 2015, 51(12): 1516-1522.
| [1] | Bowen A W, Leak G M. Metall Trans, 1970; 1: 2767 | | [2] | Bell T, Sun Y. Heat Treat Met, 2002; 29: 57 | | [3] | Qu J, Blau P J, Jolly B C. Wear, 2007; 263: 719 | | [4] | Ceschini L, Minak G. Surf Coat Technol, 2008; 202: 1778 | | [5] | Tokaji K, Kohyama K, Akita M. Int J Fatigue, 2004; 26: 543 | | [6] | Li P, Pan L, Zhang L J, Yang M H, Zhu Y F, Ma F. China Surf Eng, 2013; 26(2): 26 | | [6] | (李 朋, 潘 邻, 张良界, 杨闽红, 朱云峰, 马 飞. 中国表面工程, 2013; 26(2): 26) | | [7] | Li P, Pan L, Zhang L J, Yang M H, Zhu Y F, Ma F, Wang C H. Surf Technol, 2013; 42(4): 18 | | [7] | (李 朋, 潘 邻, 张良界, 杨闽红, 朱云峰, 马 飞, 王成虎. 表面技术, 2013; 42(4): 18) | | [8] | Yang M H, Li P, Pan L, Zhang L J, Dong G C. Mater Prot, 2012; 45(7): 60 | | [8] | (杨闽红, 李 朋, 潘 邻, 张良界, 董根成. 材料保护, 2012; 45(7): 60) | | [9] | Yu Y N. Fundamentals of Materials Science. Beijing: Higher Education Press, 2006: 466 | | [9] | (余永宁. 材料科学基础. 北京: 高等教育出版社, 2006: 466) | | [10] | Andersson J O, Helander T, H?glund L, Shi P, Sundman B. Calphad, 2002; 26: 273 | | [11] | Sudha C, Sivai Bharasi N, Anand R, Shaikh H, Dayal R K, Vijayalakshmi M. J Nucl Mater, 2010; 402: 186 | | [12] | Turpin T, Dulcy J, Gantois M. Metall Mater Trans, 2005; 36A: 2751 | | [13] | Rowan O K, Sisson Jr R D. J Phase Equilib Diff, 2009; 30: 235 | | [14] | Garcia J, Prat O. Appl Surf Sci, 2011; 257: 8894 | | [15] | H?glund L, ?gren J. J Phase Equilib Diff, 2010; 31: 212 | | [16] | Okafor I C I, Carlson O N, Martin D. Metall Trans, 1982; 13A: 1713 | | [17] | Tahara M, Senbokuya H, Kitano K, Hayashida T. Eur Pat, 0678589A1, 1995 | | [18] | Rong D S, Gong J M, Jiang Y, Geng L Y. China Pat, 103323355A, 2013 | | [18] | (荣冬松, 巩建鸣, 姜 勇, 耿鲁阳. 中国专利, 103323355A, 2013) | | [19] | Michal G M, Ernst F, Heuer A H. Metall Mater Trans, 2006; 37A: 1819 | | [20] | Zhoukov A A, Krishtal M A. Met Sci Heat Treat, 1975; 17: 626 | | [21] | Lei N, Zhou C Y, Hu G M, Chen C. Iron Steel Res, 2010; 22(1): 43 | | [21] | (雷 娜, 周昌玉, 胡桂明, 陈 成. 钢铁研究学报, 2010; 22(1): 43) | | [22] | Lin H L. Master Thesis, Shanghai Jiao Tong University, 2007 | | [22] | (梁海林. 上海交通大学硕士学位论文, 2007) | | [23] | Gao W, Long J M, Kong L, Hodgson P D. ISIJ Int, 2004; 44: 869 | | [24] | Edenhofer B. Heat Treat Met, 1995; 22(3): 55 | | [25] | Gupta G S, Chaudhuri A, Kumar P V. Mater Sci Technol, 2002; 18: 1188 | | [26] | Gao W M, Kong L X, John M L, Hodgson P D. J Mater Process Technol, 2009; 209: 497 | | [27] | Gu X T, Michal G M, Ernst F, Kahn H, Heuer A H. Metall Mater Trans, 2014; 45A: 4268 | | [28] | ?gren J. Curr Opin Solid State Mater, 1996; 1: 355 | | [29] | J?nsson B. Int J Mater Res, 1994; 85: 498 | | [30] | Yang F. Mater?Sci Eng,?2005; A409: 153 | | [31] | Parascandola S, M?ller W, Williamson D L. Appl Phys Lett, 2000; 76: 2194 | | [32] | M?ller W, Parascandola S, Kruse O, Günzel R, Richter E. Surf Coat Technol, 1999; 116: 1 | | [33] | Scheuer C J, Cardoso R P, Zanetti F I, Amaral T, Brunatto S F. Surf Coat Technol, 2012; 206: 5085 | | [34] | Ge Y, Ernst F, Kahn H, Heuer A H. Metall Mater Trans, 2014; 45B: 2338 |
|
|