316L奥氏体不锈钢低温表面渗碳的数值分析* |
彭亚伟,巩建鸣( ),荣冬松,姜勇,付明辉,余果 |
南京工业大学机械与动力工程学院, 南京 211816 |
|
NUMERICAL ANALYSIS OF LOW-TEMPERATURE SURFACE CARBURIZATION FOR 316L AUSTENITIC STAINLESS STEEL |
Yawei PENG,Jianming GONG( ),Dongsong RONG,Yong JIANG,Minghui FU,Guo YU |
School of Mechanical and Power Engineering, Nanjing Tech University, Nanjing 211816 |
引用本文:
彭亚伟,巩建鸣,荣冬松,姜勇,付明辉,余果. 316L奥氏体不锈钢低温表面渗碳的数值分析*[J]. 金属学报, 2015, 51(12): 1500-1506.
Yawei PENG,
Jianming GONG,
Dongsong RONG,
Yong JIANG,
Minghui FU,
Guo YU.
NUMERICAL ANALYSIS OF LOW-TEMPERATURE SURFACE CARBURIZATION FOR 316L AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 2015, 51(12): 1500-1506.
[1] | Heuer A H, Qu J, O'Donnell L. Encyclopedia of Tribology. New York: Springer US, 2013: 2017 | [2] | Lo R H, Shek C H, Lai J K L. Mater Sci Eng, 2009; R65: 39 | [3] | Leyland A, Lewis D B, Stevenson P R, Matthews A. Surf Coat Technol, 1993; 62: 608 | [4] | Lewis D B, Leyland A, Stevenson P R, Matthews A. Surf Coat Technol, 1993; 60: 416 | [5] | Karabelchtchikova O, Sisson R D. J Phase Equilib Diff, 2006; 27: 598 | [6] | Gu X T, Michal G M, Ernst F, Kahn H, Heuer A H. Metall Mater Trans, 2014; 45A: 3790 | [7] | Wang Y F, Gong J M, Rong D S, Gao F. Acta Metall Sin, 2014; 50: 409 | [7] | (王艳飞, 巩建鸣, 荣冬松, 高 峰. 金属学报, 2014; 50: 409) | [8] | Agarwal N, Kahn H, Avishai A, Michal G, Ernst F, Heuer A H. Acta Mater, 2007; 55: 5572 | [9] | Michal G M, Ernst F, Kahn H, Cao Y, Oba F, Agarwal N, Heuer A H. Acta Mater, 2006; 54: 1597 | [10] | Christiansen T, Somers M A J. Mater Sci Eng, 2006; A424: 181 | [11] | M?ller W, Parascandola S, Telbizoiva T, Gunzel G, Richter E. Surf Coat Technol, 2001; 73: 136 | [12] | Zhang Z P, Li P. Vacuum, 2014; 101: 321 | [13] | Parascandola S, M?ller W, Williamson D L. Appl Phys Lett, 2000; 76: 2194 | [14] | Rong D S, Gong J M, Jiang Y, Geng L Y. Chin Pat, 103323355 A, 2013 | [14] | (荣冬松, 巩建鸣, 姜 勇, 耿鲁阳. 中国专利, 103323355 A, 2013) | [15] | Jackson W B, Tsai C C. Phys Rev, 1992; 45B: 12 | [16] | Abrasonis G, Rivie?re J P, Templier C, Pranevic?ius L, Barradas N P. J App Phys, 2005; 97: 124906 | [17] | Sun Y, Chin L Y. Surf Eng, 2002; 18: 443 | [18] | Liu W J, Brimacombe J K, Hawbolt E B. Acta Metall Mater, 1991; 39: 2373 | [19] | Agarwala R P, Naik M C, Anand M S, Paul A R. J Nucl Mater, 1970; 36: 41 | [20] | Farkas D, Delgado J. Scr Metall, 1983; 17: 261 | [21] | Ernst F, Li D Q, Kahn H, Harold, Michal G M. Heuer A H. Acta Mater, 2011; 59: 2268 | [22] | Agren J. Scr Metall, 1986; 20: 1507 | [23] | Sharghi-Moshtaghin R, Kahn H, Ge Y, Gu X, Martin F J, Natishan P M, Rayne R J, Michal G M, Ernst F, Heuer A H. Metall Mater Trans, 2010; 41A: 2022 | [24] | Grabke H J. Mater Corros, 2003; 5: 736 | [25] | Raic K T. Scand J Metall, 1993; 22: 50 | [26] | Munts V A, Baskakov A P. Met Sci Heat Treat, 1983; 25: 98 | [27] | Ernst F, Avishai F, Kahn H, Gu X, Michal G M, Heuer A H. Metall Mater Trans, 2009; 40A: 1768 | [28] | Ernst F, Cao Y, Michal G M, Heuer A H. Acta Mater, 2007; 55: 1895 |
|
|