| 镍基单晶高温合金中温稳态蠕变期间的变形机制* |
苏勇1,2,田素贵1( ),于慧臣3,于莉丽1 |
1 沈阳工业大学材料科学与工程学院, 沈阳 110870 2 沈阳化工大学能源与动力工程学院, 沈阳 110142 3 中航工业北京航空材料研究院航空材料检测与评价北京市重点实验室,先进高温结构材料国防科技重点实验室, 北京 100095 |
|
| DEFORMATION MECHANISMS OF Ni-BASED SINGLE CRYSTAL SUPERALLOYS DURING STEADY-STATE CREEP AT INTERMEDIATE TEMPERATURES |
Yong SU1,2,Sugui TIAN1( ),Huichen YU3,Lili YU1 |
1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870 2 School of Energy and Power Engineering, Shenyang University of Chemical Technology, Shenyang 110142 3 Science and Technology on Advanced High Temperature Structural Materials Laboratory, Beijing Key Laboratory of Aeronautical Materials Testing and Evaluation, AVIC Beijing Institute of Aeronautical Materials, Beijing 100095 |
引用本文:
苏勇,田素贵,于慧臣,于莉丽. 镍基单晶高温合金中温稳态蠕变期间的变形机制*[J]. 金属学报, 2015, 51(12): 1472-1480.
Yong SU,
Sugui TIAN,
Huichen YU,
Lili YU.
DEFORMATION MECHANISMS OF Ni-BASED SINGLE CRYSTAL SUPERALLOYS DURING STEADY-STATE CREEP AT INTERMEDIATE TEMPERATURES[J]. Acta Metall Sin, 2015, 51(12): 1472-1480.
| [1] | Tian S G, Zhang S, Liang F S, Li A N, Li J J. Mater Sci Eng, 2011; A528: 4988? | | [2] | Xia Y F, Jin Y L. J?Northeast?Univ (Nat Sci), 2008; 29: 1053 | | [2] | (夏永发, 金玉龙. 东北大学学报(自然科学版), 2008; 29: 1053) | | [3] | Liu L, Huang T W, Zhang J, Fu H Z. Mater Lett, 2007; 61: 227 | | [4] | Reed R C, Tao T, Warnken N. Acta Mater, 2009; 57: 5898 | | [5] | Ma W Y, Li S S, Qiao M, Gong S K, Zheng Y R, Han Y F. Chin J Nonferrous Met, 2006; 16: 937 | | [5] | (马文有, 李树索, 乔 敏, 宫声凯, 郑运荣, 韩雅芳. 中国有色金属学报, 2006; 16: 937) | | | ?Zhang J, Li J G, Jin T, Sun X F, Hu Z Q. Mater Sci Eng, 2010; A527: 3051? | | [7] | Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H. Acta Mater, 2003; 51: 5073 | | [8] | Rae C M F, Matan N, Reed R C. Mater Sci Eng, 2001; A300: 125 | | [9] | Kear B K, Leverant G R, Oblak J M. Trans ASM,1969; 62: 639 | | [10] | Leverant G R, Kear B H. Metall Trans, 1970; 1: 491 | | [11] | Kear B H, Oblak J M, Giamei A F. Metall Trans, 1970; 1: 2477 | | [12] | Link T, Feller-Kniepmeier M. Metall Trans, 1992; 23A: 99 | | [13] | Yu X F, Tian S G, Du H Q, Wang M G, Meng F L. Rare Met Mater Eng, 2007; 36: 2148 | | [13] | (于兴福, 田素贵, 杜洪强, 王明罡, 孟凡来. 稀有金属材料与工程, 2007; 36: 2148) | | [14] | Sass V, Glatzel U, Feller-Kniepmeier M. In: Kissinger R D, Deye D J, Anton D L,Cetel A D, Natal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale, PA: TMS, 1996: 283 | | [15] | Sass V, Glatzel U, Feller-Kniepmeier M. Acta Metall Mater, 1996; 44: 1967 | | [16] | Matan N, Cox D C, Carter P, Rist M A, Rae C M F, Reed R C. Acta Mater, 1999; 47: 1549 | | [17] | Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 | | [18] | Lin D L, Lin T L, Wen M. Mater Sci Eng, 1989; A113: 207 | | [19] | Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2005; 41: 1215 | | [19] | (刘丽荣, 金 涛, 赵乃仁, 王志辉, 孙晓峰, 管恒荣, 胡壮麒. 金属学报, 2005; 41: 1215) | | [20] | Tian S G, Ding X, Guo Z G, Xie J, Xue Y C, Shu D L. Mater Sci Eng, 2014; A594: 7 | | [21] | Yang H, Li Z H, Huang M S. Comput Mater Sci, 2013; 75: 52 | | [22] | Peng Z F, Ren Y Y, Fan B Z,Yan P, Zhao J C,Wang Y Q, Sun J H. Acta Metall Sin, 1999; 35: 9 | | [22] | (彭志方, 任遥遥, 樊宝珍, 燕 平, 赵京晨, 王延庆, 孙家华. 金属学报, 1999; 35: 9) | | [23] | Tian S G, Wu J, Shu D L, Su Y, Yu H C, Qian B J. Mater Sci Eng, 2014; A616: 260 | | [24] | Milligan W W, Antolovich S D. Metall Trans, 1991; 22A: 2309 | | [25] | Gabb T P, Draper S L, Hull D R, Mackay R A, Nathal M V. Mater Sci Eng, 1989; A118: 59 | | [26] | Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, Hu Z Q. Mater Sci Eng, 2000; A279: 160 | | [27] | Gabrisch H, Mukherji D. Acta Mater, 2000; 48: 3157 | | [28] | Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H, Masaki Jr S. Metall Mater Trans, 2003; 33A: 3741 | | [29] | Doun J, Veyssiere P, Beachamp P. Philos Mag, 1986; 54A: 375 | | [30] | Veyssiere P, Doun J, Beachamp P. Philos Mag, 1985; 51A: 469 | | [31] | Foiles S M, Daw M S. J Mater Res, 1987; 2: 5 | | [32] | Chen S P, Voter A F, Srolovitz D J. Scr Metall, 1986; 20: 1389 | | [33] | Kear B H, Wilsdorf H G F. Trans Met Soc, 1962; 224: 382 | | [34] | Liu J L, Jin T, Zhang J H, Hu Z Q. Acta Metall Sin, 2001; 37: 1233 | | [34] | (刘金来, 金 涛, 张静华, 胡壮麒. 金属学报, 2001; 37: 1233) | | [35] | Vitek V. Prog Mater Sci, 1992; 36(1): 1 | | [36] | Yamaguchi M, Umakoshi Y. Prog Mater Sci, 1992; 34(1): 1 | | [37] | Vitek V. Intermetallics, 1998; 6: 579 |
|
|