| 650 MPa级V-N微合金化汽车大梁钢强化机制研究* |
惠亚军1( ),潘辉1,周娜2,李瑞恒2,李文远1,刘锟1 |
1 首钢技术研究院薄板研究所, 北京 100043 2 首钢股份公司迁安钢铁公司技术质量部, 迁安 064400 |
|
| STUDY ON STRENGTHENING MECHANISM OF 650 MPa GRADE V-N MICROALLOYED AUTOMOBILE BEAM STEEL |
Yajun HUI1( ),Hui PAN1,Na ZHOU2,Ruiheng LI2,Wenyuan LI1,Kun LIU1 |
1 Sheet Metal Research Institute, Shougang Research Institute of Technology, Beijing 100043 2 Technology and Quality Division, Qian'an Iron & Steel Company, Shougang Co., Ltd., Qian'an 064400 |
引用本文:
惠亚军,潘辉,周娜,李瑞恒,李文远,刘锟. 650 MPa级V-N微合金化汽车大梁钢强化机制研究*[J]. 金属学报, 2015, 51(12): 1481-1488.
Yajun HUI,
Hui PAN,
Na ZHOU,
Ruiheng LI,
Wenyuan LI,
Kun LIU.
STUDY ON STRENGTHENING MECHANISM OF 650 MPa GRADE V-N MICROALLOYED AUTOMOBILE BEAM STEEL[J]. Acta Metall Sin, 2015, 51(12): 1481-1488.
| [1] | Bewlay B P, Jackson M R, Lipsitt H A. Metall Mater Trans, 1996; 27A: 3801 | | [2] | Yang D J, Fang Y, Du Q, Zhao Y T. Hot Working Technol, 2013; 42(2): 46 | | [2] | (阳代军, 方 圆, 杜 倩, 赵运堂. 热加工工艺, 2013; 42(2): 46) | | [3] | Guo J, Shang C J, Yang S W, Guo H, Wang X M, He X L. Mater Des, 2009; 30: 129 | | [4] | Manohar P A, Chandra T, Killmore C R. ISIJ Int, 1996; 36: 1486 | | [5] | Chen J, Chen X W, Tang S, Liu Z Y, Wang G D. Mater Sci Forum, 2013; 749: 243 | | [6] | Cizek P, Wynne B P, Davies C H J, Muddle B C, Hodgson P D. Metall Mater Trans, 2002; 33A: 1331 | | [7] | Sakuma T, Honeycombe R W K. Met Sci, 1984; 18: 449 | | [8] | Dunlop G L, Carlsson C J, Frimodig G. Metall Trans, 1978; 9A: 261 | | [9] | Freeman S, Honeycombe R W K. Met Sci, 1977; 11: 59 | | [10] | Honeycombe R W K, Medalist R F. Metall Trans, 1976; 7A: 915 | | [11] | Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945 | | [12] | Yen H W, Chen P Y, Huang C Y, Yang J R. Acta Mater, 2011; 59: 6264 | | [13] | Balliger N K, Honeycombe R W K. Metall Trans, 1980; 11A: 421 | | [14] | Naylor D J. Iron Making Steel Making, 1990; 17(1): 17 | | [15] | Ishikawa F, Takahashi T. ISIJ Int, 1995; 20: 1128 | | [16] | Yong Q L. The Second Phase in Steels. Beijing: Metallurgical Industry Press, 2006: 175 | | [16] | (雍岐龙.钢铁材料中的第二相.北京: 冶金工业出版社, 2006: 175) | | [17] | Zajac S, Hutchinson B, Lagneborge B. Scand J Metall, 2009; 48: 39 | | [18] | Fang F, Yong Q L, Yang C F. Acta Metall Sin, 2005; 45: 625 | | [18] | (方 芳, 雍岐龙, 杨才福. 金属学报, 2005; 45: 625) | | [19] | Medina S F, Gomez M, Rancel L. Scr Mater, 2008; 58: 1110 | | [20] | Foreman A J E, Makin M J. Can J Phys, 1967; 45: 511. | | [21] | De Aedo A J, Garela C I, Palmiere E J. ASM Handbook. Vol.4, Materials Park, OH: ASM International, 1990: 237 | | [22] | Yong Q L. Microalloyed Steel—Physical and Mechanical Metallurgy. Beijing: China Machine Press, 1989: 57 | | [22] | (雍岐龙. 微合金钢—物理和力学冶金.北京: 机械工业出版社, 1989: 57) | | [23] | Pickering F B. Physical Metallurgy and the Design of Steels. London: Applied Science Publishing Ltd., 1978: 63 | | [24] | Chen J, Lv M Y, Tang S, Liu Z Y, Wang G D. Mater Sci Eng, 2014; A594: 389 | | [25] | Ashby M F. Strengthening Methods in Crystals. London: Applied Science Publishers Ltd., 1971: 137 | | [26] | Chen J, Chen X W, Tang S, Liu Z Y, Wang G D. Mater Sci Forum, 2013; 749: 243 | | [27] | Brito R M, Kestenbach H J. J Mater Sci, 1981; 16: 1257 |
|
|