先进镍基单晶高温合金组织稳定性及力学行为的研究进展 |
金涛( ),周亦胄,王新广,刘金来,孙晓峰,胡壮麒 |
|
RESEARCH PROCESS ON MICROSTRUCTURAL STABILITY AND MECHANICAL BEHAVIOR OF ADVANCED Ni-BASED SINGLE CRYSTAL SUPERALLOYS |
Tao JIN( ),Yizhou ZHOU,Xinguang WANG,Jinlai LIU,Xiaofeng SUN,Zhuangqi HU |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
金涛,周亦胄,王新广,刘金来,孙晓峰,胡壮麒. 先进镍基单晶高温合金组织稳定性及力学行为的研究进展[J]. 金属学报, 2015, 51(10): 1153-1162.
Tao JIN,
Yizhou ZHOU,
Xinguang WANG,
Jinlai LIU,
Xiaofeng SUN,
Zhuangqi HU.
RESEARCH PROCESS ON MICROSTRUCTURAL STABILITY AND MECHANICAL BEHAVIOR OF ADVANCED Ni-BASED SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2015, 51(10): 1153-1162.
[1] | Reed R C. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 19 | [2] | Hu Z Q, Liu L R, Jin T, Sun X F. Aeroengine, 2005; 31(3): 1 (胡壮麒, 刘丽荣, 金 涛, 孙晓峰. 航空发动机, 2005; 31(3): 1) | [3] | Sun X F, Jin T, Zhou Y Z, Hu Z Q. Mater China, 2012; 31(12): 1 (孙晓峰, 金 涛, 周亦胄, 胡壮麒. 中国材料进展, 2012; 31(12): 1) | [4] | Darolia R, Lahrman D F, Field R D, Sisson R. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1988, Champion, PA: TMS, 1988: 255 | [5] | Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Jo C Y. Philos Mag Lett, 2012; 92: 556 | [6] | Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Yoo Y S, Jo C Y. Metall Mater Trans, 2012; 43A: 3608 | [7] | Tan X P, Hong H U, Choi B G, Kim I S, Jo C Y, Jin T, Hu Z Q. J Mater Sci, 2013; 48: 1085 | [8] | Argence D, Vernault C, Desvallées Y, Fournier D. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Champion, PA: TMS, 2000: 829 | [9] | Zhang J X, Koizumi Y, Kobayashi T, Murakumo T, Harada H. Metall Mater Trans, 2004; 35A: 1911 | [10] | Wang X G, Liu J L, Jin T, Sun X F. Mater Sci Eng, 2014; A598: 154 | [11] | Wang X G, Liu J L, Jin T, Sun X F, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Mater Des, 2015; 67: 543 | [12] | Murakumo T, Kobayashi T, Koizumi Y, Harada H. Acta Mater, 2004; 52: 3737 | [13] | Mughrabi H. Mater Sci Technol, 2009; 25: 191 | [14] | Pollock T M, Argon A S. Acta Metall, 1994; 42: 1859 | [15] | Wang X G. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2015 (王新广. 中国科学院金属研究所博士学位论文, 沈阳, 2015) | [16] | Tan X P, Liu J L, Jin T, Hu Z Q, Hong H U, Choi B G, Kim I S, Jo C Y. Mater Sci Eng, 2013; A580: 21 | [17] | Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Adv Eng Mater, 2015; 17: 1034 | [18] | Rae C M F, Reed R C. Acta Mater, 2001; 49: 4113 | [19] | Seiser B, Drautz R, Pettifor D G. Acta Mater, 2011; 59: 749 | [20] | Yeh A C, Tin S. Metall Mater Trans, 2006; 37A: 2621 | [21] | Hobbs R A, Zhang L, Rae C M F, Tin S. Metall Mater Trans, 2008; 39A: 1014 | [22] | Ofori A P, Humphreys C J, Tin S, Jones C N. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Champion, PA: TMS, 2004: 787 | [23] | Sato A, Harada H, Yokokawa T, Murakumo T, Koizumi Y, Kobayashi T, Imai H. Scr Mater, 2006; 54: 1679 | [24] | Gao S, Zhou Y Z, Li C F, Cui J P, Liu Z Q, Jin T. J Alloys Compd, 2014; 610: 589 | [25] | Cheng K Y. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2009 (成魁宇. 中国科学院金属研究所博士学位论文, 沈阳, 2009) | [26] | Tan X P. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012 (谭喜鹏. 中国科学院金属研究所博士学位论文, 沈阳, 2012) | [27] | Luo Y P. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2014 (罗银屏. 中国科学院金属研究所硕士学位论文, 沈阳, 2014) | [28] | Chen J Y, Feng Q, Sun Z Q. Scr Mater, 2010; 63: 795 | [29] | Pollock T M, Argon A S. Acta Metall, 1992; 40: 1 | [30] | Field R D, Pollock T M, Murphy W H. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Champion, PA: TMS, 1992: 557 | [31] | Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H, Masaki S. Metall Mater Trans, 2002; 33A: 3741 | [32] | Huang M, Cheng Z Y, Xiong J C, Li J R, Hu J Q, Liu Z L, Zhu J. Acta Mater, 2014; 76: 294 | [33] | Gabrisch H, Mukherji D. Acta Mater, 2000; 48: 3157 | [34] | Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Mater Sci Eng, 2015; A626: 406 | [35] | Eggeler G, Dlouhy A. Acta Mater, 1997; 45: 4251 | [36] | Srinivasan R, Eggeler G F, Mills M J. Acta Mater, 2000; 48: 4867 | [37] | Zhang J X, Murakumo T, Koizumi Y, Kobayashi T, Harada H. Acta Mater, 2003; 51: 5073 | [38] | Reed R C, Cox D C, Rae C M F. Mater Sci Eng, 2007; A448: 88 | [39] | le Graverend J B, Cormier J, Jouiad M, Gallerneau F, Paulmier P, Hanmon F. Mater Sci Eng, 2010; A527: 5295 | [40] | Caron P. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Champion, PA: TMS, 2000: 737 | [41] | Li Q Q. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012 (李芹芹. 中国科学院金属研究所硕士学位论文, 沈阳, 2012) | [42] | Li P, Li Q Q, Jin T, Zhou Y Z, Li J G, Sun X F, Zhang Z F. Int J Fatigue, 2014; 63: 137 | [43] | Auerswald J, Mukherji D, Chen W, Wahi R P. Z Metallkd, 1997; 88: 652 | [44] | Wang X G, Liu J L, Jin T, Sun X F, Zhou Y Z, Hu Z Q, Do J H, Choi B G, Kim I S, Jo C Y. Scr Mater, 2015; 99: 57 | [45] | Zhang X. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006 (张 炫. 中国科学院金属研究所博士学位论文, 沈阳, 2006) | [46] | Gabb T P, Welsch G E. Scr Metall, 1986; 20: 1049 | [47] | Gabb T P, Welsch G E. Acta Metall, 1989; 37: 2507 | [48] | Milligan W W, Jayaraman N. Mater Sci Eng, 1986; 82: 127 | [49] | Zhou H, Ro Y, Harada H, Aoki Y, Arai M. Mater Sci Eng, 2004; A381: 20 | [50] | Han G M. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010 (韩国明. 中国科学院金属研究所硕士学位论文, 沈阳, 2010) | [51] | Kraft S, Zauter R, Mughrabi H. Fatigue Fract Eng Mater Struct, 1993; 16: 237 | [52] | Liu F, Wang Z G, Ai S H, Wang Y C, Sun X F, Jin T, Guan H R. Scr Mater, 2003; 48: 1265 | [53] | Zhang J X, Harada H, Ro Y, Koizumi Y, Kobayashi T. Acta Mater, 2008; 56: 2975 | [54] | Moverare J J, Johansson S, Reed R R. Acta Mater, 2009; 57: 2266 | [55] | Zhang J. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006 (张 剑. 中国科学院金属研究所博士学位论文, 沈阳, 2006) | [56] | Xu Y B. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2013 (徐砚博. 中国科学院金属研究所硕士学位论文, 沈阳, 2013) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|