李雄兵, 宋永锋, 倪培君, 刘锋. 面向晶粒尺寸的超声多尺度衰减评价方法[J]. 金属学报, 2015, 51(1): 121-128.
Xiongbing LI,
Yongfeng SONG,
Peijun NI,
Feng LIU.
ULTRASONIC EVALUATION METHOD FOR GRAIN SIZE BASED ON MULTI-SCALE ATTENUATION[J]. Acta Metall Sin, 2015, 51(1): 121-128.
| [1] |
Prasad K S, Rao C S, Rao D N. Acta Metall Sin (Engl Lett), 2012; 25: 179
|
| [2] |
Wang S H, Liu Z Y, Wang G D. Acta Metall Sin, 2009; 45: 61
|
| [2] |
(王书晗, 刘振宇, 王国栋. 金属学报, 2009; 45: 61)
|
| [3] |
Zhao Y, Chen Z, Long J, Yang T. Acta Metall Sin (Engl Lett), 2014; 27: 81
|
| [4] |
Lehto P, Remes H, Saukkonen T, Hänninen H, Romanoff J. Mater Sci Eng, 2014; A592: 28
|
| [5] |
Andrés R, Galvis E, Hormaza W. Eng Fail Anal, 2011; 18: 1791
|
| [6] |
Voort G F V. Prakt Metall, 2013; 50: 239
|
| [7] |
Schwartz A J, Kumar M, Adams B L, Field D P. Electron Backscatter Diffraction in Materials Science. New York: Springer, 2009: 1
|
| [8] |
Sabbagh E H, Sabbagh H A, Murphy R K, Sheila-Vadde A, Blodgett M P, Knopp J, Aldrin J C. In: Thompson D O, Chimenti D E eds., Review of Progress in Quantitative Nondestructive Evaluation, New York: American Institute of Physics, 2009: 742
|
| [9] |
Guo Y, Thompson R B, Margetan F J. In: Thompson D O, Chimenti D E, eds., Review of Progress in Quantitative Nondestructive Evaluation, New York: American Institute of Physics, 2003: 1347
|
| [10] |
Panetta P D, Bland L G, Tracy M, Hassan W. In: The Minerals, Metals & Materials Society (TMS) ed., TMS2014 Annual Meeting Supplemental Proceedings, Hoboken: John Wiley & Sons Inc, 2014: 721
|
| [11] |
Ünal R, Sarpün I H, Yalım H A, Erol A, Özdemir T, Tuncel S. Mater Charact, 2006; 56: 241
|
| [12] |
Zuev L B, Semukhin B S, Zarikovskaya N V. Int J Solids Struct, 2003; 40: 941
|
| [13] |
Laux D, Cros B, Despaux G, Baron D. J Nucl Mater, 2002; 300: 192
|
| [14] |
Aghaie-Khafri M, Honarvar F, Zanganeh S. J Nondestruct Eval, 2012; 31: 191
|
| [15] |
Őzkan V, Sarpünb I H. Acta Phys Pol, 2012; 121A: 184
|
| [16] |
Zeng F, Agnew S R, Raeisinia B, Myneni G R. J Nondestruct Eval, 2010; 29: 93
|
| [17] |
Kumar A, Jayakumar T, Palanichamy P, Raj B. Scr Mater, 1999; 40: 333
|
| [18] |
Sharma G K, Kumar A, Babu Rao C, Jayakumar T, Raj B. NDT&E Int, 2013; 53: 1
|
| [19] |
Dong J K. Heat Treat Met, 2011; 36: 133
|
| [19] |
(董加坤. 金属热处理, 2011; 36: 133)
|
| [20] |
Eberhart R C, Shi Y. In: Zalzala A ed., IEEE Proceedings of the Congress Evolutionary Computation, New York: IEEE, 2000: 84
|
| [21] |
Le T P, Argoul P. J Sound Vib, 2004; 277: 73
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|