| 基于晶体塑性理论的晶界压痕行为研究 |
闫五柱1,2, 张嘉振1,2( ), 周振功2, 岳珠峰3 |
1 中国商用飞机有限责任公司北京民用飞机技术研究中心, 北京 102211 2 哈尔滨工业大学复合材料与结构研究所, 哈尔滨 150080 3 西北工业大学工程力学系, 西安 710129 |
|
| STUDY ON THE INDENTATION BEHAVIORS OF BICRYSTALS BASED ON CRYSTAL PLASTICITY THEORY |
YAN Wuzhu1,2, ZHANG Jiazhen1,2( ), ZHOU Zhengong2, YUE Zhufeng3 |
1 Beijing Aeronautical Science and Technology Research Institute of COMAC, Beijing 102211 2 Center for Composite Materials and Structures, Harbin Institute of Technology, Harbin 150080 3 Department of Engineering Mechanics, Northwestern Polytechnical University, Xi'an 710129 |
引用本文:
闫五柱, 张嘉振, 周振功, 岳珠峰. 基于晶体塑性理论的晶界压痕行为研究[J]. 金属学报, 2015, 51(1): 100-106.
Wuzhu YAN,
Jiazhen ZHANG,
Zhengong ZHOU,
Zhufeng YUE.
STUDY ON THE INDENTATION BEHAVIORS OF BICRYSTALS BASED ON CRYSTAL PLASTICITY THEORY[J]. Acta Metall Sin, 2015, 51(1): 100-106.
| [1] |
Cheng Y T, Cheng C M. Mater Sci Eng, 2004; R44: 91
|
| [2] |
Diard O, Leclereq S, Rousselier G, Cailletaud G. Int J Plast, 2005; 21: 691
|
| [3] |
Raabe D, Sachtleber M, Zhao Z, Roters F, Zaefferer S. Acta Mater, 2001; 49: 3433
|
| [4] |
Wu X, Kalidindi S R, Necker C, Salem A A. Acta Mater, 2007; 55: 423
|
| [5] |
Ma Q, Clarke D R. J Mater Res, 1995; 10: 853
|
| [6] |
Nix W D, Gao H. J Mech Phys Solids, 1998; 46: 411
|
| [7] |
Taylor G I. J Inst Met, 1938; 62: 307
|
| [8] |
Hill R, Rice J R. J Mech Phys Solids, 1972; 20: 401
|
| [9] |
Li H W, Feng L, Yang H. Trans Nonferrous Met Soc China, 2013; 23: 3729
|
| [10] |
Wen Z X, Yue Z F. Comput Mater Sci, 2007; 40: 140
|
| [11] |
Segurado J, LLorca J. Int J Plast, 2010; 26: 806
|
| [12] |
Dong Z G, Huang H, Kang R. Mater Sci Eng, 2010; A527: 4177
|
| [13] |
Huang H, Wu Y Q, Wang S L, He Y H, Zou J, Huang B Y, Liu C T. Mater Sci Eng, 2009; A523: 193
|
| [14] |
Chicot D. Mater Sci Eng, 2009; A499: 454
|
| [15] |
Kang S, Jung Y, Yoo B, Jang J, Lee Y. Mater Sci Eng, 2012; A532: 500
|
| [16] |
Xu B X. Yonezu A, Yue Z F, Chen X. Comput Mater Sci, 2009; 46: 275
|
| [17] |
Liu Y, Wang B, Yoshino M, Roy S, Lu H, Komanduri R. J Mech Phys Solids, 2005; 53: 2718
|
| [18] |
Li L, Shen L M, Proust G, Moy C K S, Ranzi G. Mater Sci Eng, 2013; A579: 41
|
| [19] |
Yan W Z, Wen S F, Liu J, Yue Z F. Mater Sci Eng, 2010; A527: 1850
|
| [20] |
Peirce D, Asaro R J, Needleman A. Acta Metall, 1982; 30: 1087
|
| [21] |
Anand L, Kothari M. J Mech Phys Solids, 1996; 44: 525
|
| [22] |
Fang X, Yan W Z, Gao H S, Yue Z F, Liu J, Wang F S. Finite Elem Anal Des, 2012; 60: 64
|
| [23] |
Wan J S, Yue Z F. Appl Math Mech, 2004; 25(1): 39
|
| [23] |
(万建松, 岳珠峰. 应用数学和力学, 2004; 25(1): 39)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|