金属学报  2015, Vol. 51 Issue (1): 100-106    DOI: 10.11900/0412.1961.2014.00335
  本期目录 | 过刊浏览 |
基于晶体塑性理论的晶界压痕行为研究
闫五柱1,2, 张嘉振1,2(), 周振功2, 岳珠峰3
1 中国商用飞机有限责任公司北京民用飞机技术研究中心, 北京 102211
2 哈尔滨工业大学复合材料与结构研究所, 哈尔滨 150080
3 西北工业大学工程力学系, 西安 710129
STUDY ON THE INDENTATION BEHAVIORS OF BICRYSTALS BASED ON CRYSTAL PLASTICITY THEORY
YAN Wuzhu1,2, ZHANG Jiazhen1,2(), ZHOU Zhengong2, YUE Zhufeng3
1 Beijing Aeronautical Science and Technology Research Institute of COMAC, Beijing 102211
2 Center for Composite Materials and Structures, Harbin Institute of Technology, Harbin 150080
3 Department of Engineering Mechanics, Northwestern Polytechnical University, Xi'an 710129
引用本文:

闫五柱, 张嘉振, 周振功, 岳珠峰. 基于晶体塑性理论的晶界压痕行为研究[J]. 金属学报, 2015, 51(1): 100-106.
Wuzhu YAN, Jiazhen ZHANG, Zhengong ZHOU, Zhufeng YUE. STUDY ON THE INDENTATION BEHAVIORS OF BICRYSTALS BASED ON CRYSTAL PLASTICITY THEORY[J]. Acta Metall Sin, 2015, 51(1): 100-106.

全文: PDF(2603 KB)   HTML
摘要: 

为了研究晶界的压痕行为, 采用晶体塑性理论对单晶和双晶的压痕行为进行了有限元模拟, 得到了压痕表面和晶界位置处的应力分布. 结果表明, 相邻晶粒的晶体取向对压痕深度-载荷响应以及分解切应力分布均有较显著的影响. 压载荷作用下, 晶界位置处存在应力集中, 且晶体取向差异越大, 晶界应力越大.

关键词 压痕晶体塑性单晶双晶晶界有限元    
Abstract

In the past decades, the indentation test has been widely used to determine the mechanical properties of materials. For the micro- or nano- indentation, the indentation response is complex since only one or two grains can be indented by the indenter. In order to investigate the indentation behavior of the grain boundary, the crystal plasticity theory was implemented into finite element model to simulate the indentation behavior of single crystals and bicrystals. The stress distributions on the indented surface and grain boundary were obtained. The results showed that the crystallographic orientations of the neighboring grains had a remarkable influence on the depth-load response and the resolved shear stress distribution of the indented bicrystals. Under the indentation load, stress concentration occurred at the grain boundary, and the stress at the grain boundary increases with the increase of mis-orientation angle of the two neighboring grains.

Key wordsindentation    crystal plasticity    single crystal    bicrystal    grain boundary    finite element
    
ZTFLH:  TG111.91  
基金资助:* 国家自然科学基金项目资助51271067
作者简介: null

闫五柱, 男, 1985年生, 博士

图1  压痕模型示意图
图2  模型有限元网格
Crystal Case Grain No. j / (o) q / (o) f / (o)
Single crystal A 1 0.0 0.0 0.0
B 1 45.0 0.0 0.0
C 1 65.21 50.76 -63.35
Bicrystal D 1 45.0 0.0 0.0
2 0.0 0.0 0.0
E 1 65.21 50.76 -63.35
2 0.0 0.0 0.0
F 1 65.21 50.76 -63.35
2 45.0 0.0 0.0
表1  晶粒Euler角
图3  晶体取向对深度-载荷取向的影响
Mechanical parameter Value Unit
Poisson′s ratio n 0.33
Young′s modulus E 210 GPa
Shear modulus G 83 GPa
Strain rate sensitivity exponent m 0.02
Reference shear rate ˙γ(α)0 0.03 s-1
Initial resolved shear stress t0 500 MPa
Hardening law parameter h0 600 MPa
Saturation resolved shear stress ts 585 MPa
Hardening law parameter AA 1.3
Reference strain rate Ga0 300 MPa
表2  镍基单晶高温合金DD3力学参数[23]
图4  单晶和双晶压痕深度-载荷曲线
图5  不同取向单晶压痕面上分解切应力分布
图6  不同取向双晶压痕面上分解切应力分布
图7  不同取向双晶平面x=0上的分解切应力分布
图8  不同取向双晶晶界(y=0)分解切应力分布
[1] Cheng Y T, Cheng C M. Mater Sci Eng, 2004; R44: 91
[2] Diard O, Leclereq S, Rousselier G, Cailletaud G. Int J Plast, 2005; 21: 691
[3] Raabe D, Sachtleber M, Zhao Z, Roters F, Zaefferer S. Acta Mater, 2001; 49: 3433
[4] Wu X, Kalidindi S R, Necker C, Salem A A. Acta Mater, 2007; 55: 423
[5] Ma Q, Clarke D R. J Mater Res, 1995; 10: 853
[6] Nix W D, Gao H. J Mech Phys Solids, 1998; 46: 411
[7] Taylor G I. J Inst Met, 1938; 62: 307
[8] Hill R, Rice J R. J Mech Phys Solids, 1972; 20: 401
[9] Li H W, Feng L, Yang H. Trans Nonferrous Met Soc China, 2013; 23: 3729
[10] Wen Z X, Yue Z F. Comput Mater Sci, 2007; 40: 140
[11] Segurado J, LLorca J. Int J Plast, 2010; 26: 806
[12] Dong Z G, Huang H, Kang R. Mater Sci Eng, 2010; A527: 4177
[13] Huang H, Wu Y Q, Wang S L, He Y H, Zou J, Huang B Y, Liu C T. Mater Sci Eng, 2009; A523: 193
[14] Chicot D. Mater Sci Eng, 2009; A499: 454
[15] Kang S, Jung Y, Yoo B, Jang J, Lee Y. Mater Sci Eng, 2012; A532: 500
[16] Xu B X. Yonezu A, Yue Z F, Chen X. Comput Mater Sci, 2009; 46: 275
[17] Liu Y, Wang B, Yoshino M, Roy S, Lu H, Komanduri R. J Mech Phys Solids, 2005; 53: 2718
[18] Li L, Shen L M, Proust G, Moy C K S, Ranzi G. Mater Sci Eng, 2013; A579: 41
[19] Yan W Z, Wen S F, Liu J, Yue Z F. Mater Sci Eng, 2010; A527: 1850
[20] Peirce D, Asaro R J, Needleman A. Acta Metall, 1982; 30: 1087
[21] Anand L, Kothari M. J Mech Phys Solids, 1996; 44: 525
[22] Fang X, Yan W Z, Gao H S, Yue Z F, Liu J, Wang F S. Finite Elem Anal Des, 2012; 60: 64
[23] Wan J S, Yue Z F. Appl Math Mech, 2004; 25(1): 39
[23] (万建松, 岳珠峰. 应用数学和力学, 2004; 25(1): 39)
[1] 赵鹏, 谢光, 段慧超, 张健, 杜奎. 两种高代次镍基单晶高温合金热机械疲劳中的再结晶行为[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] 李嘉荣, 董建民, 韩梅, 刘世忠. 吹砂对DD6单晶高温合金表面完整性和高周疲劳强度的影响[J]. 金属学报, 2023, 59(9): 1201-1208.
[4] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[5] 徐永生, 张卫刚, 徐凌超, 但文蛟. 铁素体晶间变形协调与硬化行为模拟研究[J]. 金属学报, 2023, 59(8): 1042-1050.
[6] 张海峰, 闫海乐, 方烽, 贾楠. FeMnCoCrNi高熵合金双晶微柱变形机制的分子动力学模拟[J]. 金属学报, 2023, 59(8): 1051-1064.
[7] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[8] 王宗谱, 王卫国, Rohrer Gregory S, 陈松, 洪丽华, 林燕, 冯小铮, 任帅, 周邦新. 不同温度轧制Al-Zn-Mg-Cu合金再结晶后的{111}/{111}近奇异晶界[J]. 金属学报, 2023, 59(7): 947-960.
[9] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[10] 张禄, 余志伟, 张磊成, 江荣, 宋迎东. GH4169高温合金热机械疲劳循环损伤机理及数值模拟[J]. 金属学报, 2023, 59(7): 871-883.
[11] 王迪, 贺莉丽, 王栋, 王莉, 张思倩, 董加胜, 陈立佳, 张健. Pt-Al涂层对DD413合金高温拉伸性能的影响[J]. 金属学报, 2023, 59(3): 424-434.
[12] 李昕, 江河, 姚志浩, 董建新. O原子对高温合金基体NiCoNiCr晶界作用的理论计算分析[J]. 金属学报, 2023, 59(2): 309-318.
[13] 杨杜, 白琴, 胡悦, 张勇, 李志军, 蒋力, 夏爽, 周邦新. GH3535合金中晶界特征对碲致脆性开裂影响的分形分析[J]. 金属学报, 2023, 59(2): 248-256.
[14] 张子轩, 于金江, 刘金来. 镍基单晶高温合金DD432的持久性能各向异性[J]. 金属学报, 2023, 59(12): 1559-1567.
[15] 苏震奇, 张丛江, 袁笑坦, 胡兴金, 芦可可, 任维丽, 丁彪, 郑天祥, 沈喆, 钟云波, 王晖, 王秋良. 纵向静磁场下单晶高温合金定向凝固籽晶回熔界面杂晶的形成与演化[J]. 金属学报, 2023, 59(12): 1568-1580.