| 锻态TC18钛合金棒材中β相组织和织构特征研究* |
李凯1, 杨平1( ), 沙爱学2, 颜孟奇2 |
1 北京科技大学材料科学与工程学院, 北京 100083 2 中航工业北京航空材料研究院, 北京 100095 |
|
| INVESTIGATION OF MICROSTRUCTURE AND TEXTURE OF β PHASE IN A FORGED TC18 TITANIUM ALLOY BAR |
LI Kai1, YANG Ping1( ), SHA Aixue2, YAN Mengqi2 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 2 Beijing Institute of Aeronautical Materials, Aviation Industry Corporation of China, Beijing 100095 |
引用本文:
李凯, 杨平, 沙爱学, 颜孟奇. 锻态TC18钛合金棒材中β相组织和织构特征研究*[J]. 金属学报, 2014, 50(6): 707-714.
Kai LI,
Ping YANG,
Aixue SHA,
Mengqi YAN.
INVESTIGATION OF MICROSTRUCTURE AND TEXTURE OF β PHASE IN A FORGED TC18 TITANIUM ALLOY BAR[J]. Acta Metall Sin, 2014, 50(6): 707-714.
| [1] |
Zhang Y Q, Guo H Z, Sun H L, Yao Z K. Mater Heat Treatment, 2012; 41(6): 147
|
| [1] |
(张永强, 郭鸿镇, 孙红兰, 姚泽坤. 热加工工艺, 2012; 41(6): 147)
|
| [2] |
Huang X, Zhu Z S, Wang H H. Advanced Aeronautical Titanium Alloys and Applications. Beijing: National Defence Industry Press, 2012: 92
|
| [2] |
(黄 旭,朱知寿,王红红. 先进航空钛合金材料与应用. 北京: 国防工业出版社, 2012: 92)
|
| [3] |
Qiao E L, Feng Y Q, Li W Q, Xie R P, Zhang S B, Chen R J. Met World, 2013; (4): 72
|
| [3] |
(乔恩利, 冯永琦, 李渭清, 谢仁沛, 张少波, 陈瑞菁. 金属世界, 2013; (4): 72)
|
| [4] |
Glavicic M G, Goetz R L, Barker D R. Metall Mater Trans, 2008; 49A: 887
|
| [5] |
Lonardelli I, Gey N, Wenk H R. Acta Mater, 2007; 55: 5718
|
| [6] |
Gurao N P, Ali AA, Suwas S. Mater Sci Eng, 2009; A504: 24
|
| [7] |
Cayron C. Scr Mater, 2008; 59: 570
|
| [8] |
Salem A A, Glavicic M G, Semiatin S L. Mater Sci Eng, 2008; A494: 350
|
| [9] |
Obasi G C, Moat R J, Prakash D G L. Acta Mater, 2012; 60: 7169
|
| [10] |
Thomas M J, Wynne B P, Rainforth W M. Mater Charact, 2005; 55: 388
|
| [11] |
Markovsky P E, Matviychuk Y V, Bondarchuk V I. Mater Sci Eng,2013; A559: 782
|
| [12] |
Semiatin S L, Kinsel K T, Pilchak A L, Sargent G A. Metall Mater Trans, 2013; 44A: 3852
|
| [13] |
Sargent G A, Kinsel K T, Pilchak A L. Metall Mater Trans, 2012; 43A: 3570
|
| [14] |
Obasi G C, Birosca S, Quinta D F J. Acta Mater, 2012; 60: 1048
|
| [15] |
Obasi G C, Quinta D F J, Rugg D. Mater Sci Eng, 2013; A576: 272
|
| [16] |
Semiatin S L, Fagin P N, Glavicic M G, Ivasishin O M. Mater Sci Eng, 2001; A299: 225
|
| [17] |
Jackson M, Dashwood R, Christodoulou L. Metall Mater Trans, 2005; 36A: 1317
|
| [18] |
Karthikeyan T, Dasgupta A, Khatirkar R. Mater Sci Eng, 2010; A528: 549
|
| [19] |
He D, Zhu J C, Zaefferer S, Raabe D. Mater Sci Eng, 2012; A549: 20
|
| [20] |
Li C, Zhang X, Zhou K. Mater Sci Eng, 2012; A558: 668
|
| [21] |
Germain L, Gey N, Humbert M. Acta Mater, 2008; 56: 4298
|
| [22] |
Gey N, Bocher P, Uta E. Acta Mater, 2012; 60: 2647
|
| [23] |
Leo Prakash D G, Honniball P, Rugg D. Acta Mater, 2013; 61: 3200
|
| [24] |
Glavicic M G, Miller G D, Semiatin S L. Scr Mater, 2006; 54: 281
|
| [25] |
Gey N, Humbert M. Acta Mater, 2002; 50: 277
|
| [26] |
Shao H, Zhao Y Q, Ge P, Zeng W D. Mater Sci Eng, 2013; A586: 215
|
| [27] |
Lütjering G. Mater Sci Eng, 1998; A243: 32
|
| [28] |
Zhang Z,Wang Q J,Mo W. Titanium Metal Science and Heat Treatment. Beijing: Metallurgical Industry Press, 2009: 86
|
| [28] |
(张翥,王群骄,莫畏. 钛的金属学和热处理. 北京: 冶金工业出版社, 2009: 86)
|
| [29] |
Zhao D H, Wang L, Zhi M S, Xu F. Chin J Stere Image Analy, 2013; 18: 356
|
| [29] |
(赵登辉, 王琳, 智茂盛, 徐峰. 中国体视学与图像分析, 2013; 18: 356)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|