| 铁单元素基合金表面激光高熵合金化涂层的制备* |
张松( ), 吴臣亮, 王超, 伊俊振, 张春华 |
| 沈阳工业大学材料科学与工程学院, 沈阳 110870 |
|
| SYNTHESIS OF LASER HIGH ENTROPY ALLOYING COATING ON THE SURFACE OF SINGLE-ELEMENT Fe BASE ALLOY |
ZHANG Song( ), WU Chenliang, WANG Chao, YI Junzhen, ZHANG Chunhua |
| Institute of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870 |
引用本文:
张松, 吴臣亮, 王超, 伊俊振, 张春华. 铁单元素基合金表面激光高熵合金化涂层的制备*[J]. 金属学报, 2014, 50(5): 555-560.
Song ZHANG,
Chenliang WU,
Chao WANG,
Junzhen YI,
Chunhua ZHANG.
SYNTHESIS OF LASER HIGH ENTROPY ALLOYING COATING ON THE SURFACE OF SINGLE-ELEMENT Fe BASE ALLOY[J]. Acta Metall Sin, 2014, 50(5): 555-560.
| [1] |
Wang W R, Wang W L, Wang S C, Tsai Y C, Lai C H, Yeh J W. Intermetallics, 2012; 26: 44
|
| [2] |
Yeh J W, Chen S K, Lin S J, Gan J Y, Chin T S, Shun T T, Tsau C H, Chang S Y. Adv Eng Mater, 2004; 6: 299
|
| [3] |
Chuang M H, Tsai M H, Wang W R, Lin S U, Yeh J W. Acta Mater, 2011; 59: 6308
|
| [4] |
Zhang Y. Metallic Glasses and High Entropy Alloys. Beijing: Science Press, 2010: 69
|
| [4] |
(张 勇. 非晶和高熵合金. 北京: 科学出版社, 2010: 69)
|
| [5] |
Hsu C Y, Sheu T S, Yeh J W, Chen S K. Wear, 2010; 268: 653
|
| [6] |
Yeh J W, Chen Y L, Lin S J, Chen S K. Mater Sci Forum, 2007; 560: 1
|
| [7] |
Tang W Y, Chuang M H, Lin S J, Yeh J W. Metall Mater Trans, 2012; 43A: 2390
|
| [8] |
Chen M, Liu Y, Li Y X, Chen X. Acta Metall Sin, 2007; 43: 1020
|
| [8] |
(陈 敏, 刘 源, 李言祥, 陈 祥. 金属学报, 2007; 43: 1020)
|
| [9] |
Zhang H, Pan Y, He Y Z. Mater Des, 2011; 32: 1910
|
| [10] |
Wen L H, Kou H C, Li J S, Chang H, Xue X Y, Zhou L. Intermetallics, 2009; 17: 266
|
| [11] |
Zhang H, Pan Y, He Y Z. Acta Metall Sin, 2011; 47: 1075
|
| [11] |
(张 晖, 潘 冶, 何宜柱. 金属学报, 2011; 47: 1075)
|
| [12] |
Huang C, Zhang Y Z, Vilar R, Shen J Y. Mater Des, 2012; 41: 338
|
| [13] |
Zhang H, Pan Y, He Y Z, Jiao H S. Appl Surf Sci, 2011; 257: 2259
|
| [14] |
Tsau C H. Intermetallics, 2001; 9: 1085
|
| [15] |
Assadi H, Reutzel S, Herlach D M. Acta Mater, 2006; 54: 2793
|
| [16] |
Zhang S, Zhang C H, Man H C, Wu W T, Wang M C. Trans Nonferrous Met Soc, 2001; 11: 838
|
| [17] |
Zhang C H, Zhang S, Man H C, Liu C S, Cai Q K. Rare Met Mater Eng, 2005; 34: 701
|
| [17] |
(张春华, 张 松, 文效忠, 刘常升, 才庆魁. 稀有金属材料与工程, 2005; 34: 701)
|
| [18] |
Zhang S, Zhang C H, Wu W T, Wang M C. Acta Metall Sin, 2001; 37: 315
|
| [18] |
(张 松, 张春华, 吴维, 王茂才. 金属学报, 2001; 37: 315)
|
| [19] |
Qiu X W, Zhang Y P, He L, Liu C G. J Alloys Compd, 2013; 549: 195
|
| [20] |
Swalin R A. Thermodynamics of Solid. 2nd ed., New York: Wiley, 1991: 21
|
|